journal article·2018-11

Atmospheric chloride deposition in field concrete at coastal region

Jun Liu, Guangfeng Ou, Qiwen Qiu, Feng Xing, Kaifeng Tang, Jiaxin Zeng

Publisher page

Abstract

Abstract A field research is carried out at atmospheric marine zones for evaluating the chloride deposition behavior of concrete structures under multiple geographic and environmental factors. Geographic factors of offshore distance, elevation, concrete surface orientation and building barrier, and environmental factors of temperature variation and rainfall on chloride deposition of concrete surface layer are evaluated. Our investigation demonstrates that chloride deposition content is significantly affected by offshore distance, elevation, and building barrier. Effect of concrete surface orientation on chloride deposition depends on the presence of building barrier. Besides, the large temperature variation and rainfall facilitate the chloride deposition.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Concrete Corrosion and Durability · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Study on surface permeability of concrete under immersion10.3390/ma7020876 ↗
2. Assessment of the influence of concrete modification in the water uptake/evaporation kinetics by electrochemical impedance spectroscopy10.1016/j.electacta.2017.06.168 ↗
3. Electrochemical impedance interpretation of the carbonation behavior for fly ash–slag–cement materials10.1016/j.conbuildmat.2015.05.066 ↗
4. Characterization of carbonation behavior of fly ash blended cement materials by the electrochemical impedance spectroscopy method10.1016/j.cemconcomp.2015.10.006 ↗
5. Study on the carbonation behavior of cement mortar by electrochemical impedance spectroscopy10.3390/ma7010218 ↗
6. Electrochemical impedance measurement and modeling analysis of the carbonation behavior for cementititous materials10.1016/j.conbuildmat.2013.12.100 ↗
7. Influence of slag incorporation on electrochemical behavior of carbonated cement10.1016/j.conbuildmat.2017.05.008 ↗
8. Carbonation study of cement-based material by electrochemical impedance method
9. Sulfate attack of Portland cement concrete under dynamic flexural loading: a coupling function10.1016/j.conbuildmat.2016.02.052 ↗
10. Effects of sulfate attack and dry-wet circulation on creep of fly-ash slag concrete10.1016/j.conbuildmat.2016.08.023 ↗
11. Recent durability studies on concrete structure10.1016/j.cemconres.2015.05.021 ↗
12. Study of chloride penetration in concretes exposed to high-mountain weather conditions with presence of deicing salts10.1016/j.conbuildmat.2016.09.148 ↗
13. Corrosion of steel bars embedded in fibre reinforced concrete under chloride attack: state of the art10.1016/j.cemconres.2015.10.006 ↗
14. Understanding the interacted mechanism between carbonation and chloride aerosol attack in ordinary Portland cement concrete10.1016/j.cemconres.2017.02.032 ↗
15. Understanding the effect of curing age on the chloride resistance of fly ash blended concrete by rapid chloride migration test10.1016/j.matchemphys.2017.05.011 ↗
16. Long-term field study of chloride ingress in concretes containing pozzolans exposed to severe marine tidal zone10.1016/j.conbuildmat.2016.07.074 ↗
17. Aspects of the electrochemistry of steel in concrete10.1038/297109a0 ↗
18. Chloride-induced corrosion on reinforcing steel: from the fundamentals to the monitoring techniques10.1016/S0958-9465(02)00089-6 ↗
19. Surface chloride concentration of concrete under shallow immersion conditions10.3390/ma7096620 ↗
20. The importance of chloride content at the concrete surface in assessing the time to corrosion of steel in concrete structures10.1016/j.conbuildmat.2007.12.014 ↗
21. Formulation of an equation for surface chloride content of concrete due to permeation of chloride
22. Experimental investigation on pore structure characterization of concrete exposed to water and chlorides10.3390/ma7096646 ↗
23. Degradation of fly ash concrete under the coupled effect of carbonation and chloride aerosol ingress10.1016/j.corsci.2016.08.004 ↗
24. Permeation properties and pore structure of surface layer of fly ash concrete10.3390/ma7064282 ↗
25. Electrochemical feature for chloride ion transportation in fly ash blended cementitious materials10.1016/j.conbuildmat.2017.11.123 ↗
26. Chloride transport and microstructure of concrete with/without fly ash under atmospheric chloride condition10.1016/j.conbuildmat.2017.04.018 ↗
27. Marine aerosols: a review10.1016/0960-1686(91)90050-H ↗
28. Effect of distance from sea on chloride aggressiveness in concrete structures in Brazilian coastal site
29. Modelling of durability performance of Tasmanian bridges
30. Estimation of atmospheric sea salt dry deposition: wind speed and particle size dependence10.1029/JC087iC02p01246 ↗
31. Dry deposition and concentration of marine aerosols in a coastal area, sw Sweden10.1016/1352-2310(95)00355-X ↗
32. Effect of marine aerosol on atmospheric corrosion
33. The influence of airborne salinity on the atmospheric corrosion of steel10.1016/0010-938X(95)00058-R ↗
34. Corrosion of metals in the tropics10.1002/jctb.5010050901 ↗
35. Chloride penetration into concrete structures in the marine atmosphere zone – relationship between deposition of chlorides on the wet candle and chlorides accumulated into concrete10.1016/j.cemconcomp.2007.05.009 ↗
36. Durability of concrete structures in marine atmosphere zones-the use of chloride deposition rate on the wet candle as an environmental indicator10.1016/j.cemconcomp.2010.03.002 ↗
37. Chloride ingress profiles and binding capacity of mortar in cyclic drying-wetting salt fog environments10.1016/j.conbuildmat.2016.10.059 ↗
38. AASHTO T260–297 · 2009
39. Quantitative measurement of airborne sea-salt in the North Atlantic10.3402/tellusa.v30i4.10354 ↗
40. Salinity in marine atmospheric corrosion: its dependence on the wind regime existing in the site10.1016/S0010-938X(99)00048-7 ↗
41. Sea salt emission from the coastal zone
42. Tavwood Engineering Ltd · 1996
43. Chen · 2004
44. Ministerio de Fomento. Instrucción de hormigón estructural (EHE-08); 2008.
45. Decadal variation and trends in subsurface salinity from to 2012 in the northern South China Sea