Comprehensive resistance of fair-faced concrete suffering from sulfate attack under marine environments
Source abstract
Abstract
Abstract The fair-faced concrete structures serving in coastal areas may be harassed by sulfate ions carried by salt fog and rainwater. To explore the sulfate resistance performance of fair-faced concrete used in coastal subway station, specimens were subjected to simulated sulfate attack condition and actual marine environments in this study. The sulfate resistance properties of fair-faced concrete and the impact of sulfate on surface quality were investigated through compressive strength test, sulfate concentration distribution test, and the gray values of surface morphology characterization. The results show that the reminding residual strength of all specimens is still very high after exposed to simulated sulfate attack condition, demonstrating the superior sulfate resistance of fair-faced concrete used in coastal subway. Moreover, the sulfate corrosion can lead to the significantly coarsening of surface morphology, and the fair-faced concreted used in marine environments should pay special attention to sulfate corrosion. Besides, the coarse degree decreases with sulfate resistance coefficient, which means that fair-faced concrete with superior sulfate resistance can not only guarantee durability, but detain the degradation of surface morphology.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Corrosion and Durability · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Study and application of fair-faced concrete in large shield tunnel
2. Countermeasures to resolve the whole life cycle of fair-faced concrete buildings
3. Research on apparent quality control of fair-faced concrete of Nanjing South Station
4. Study on effects of air-entraining and anti-foaming on performance and apparent morphology of fair-faced concrete
5. Key points of quality control with its field verification for the fair-faced concrete of Hong Kong-Zhuhai-Macau Bridge
6. Inspection, diagnosis, and repair of architectural concrete surfaces10.1061/(ASCE)CF.1943-5509.0001034 ↗
7. Dark discoloration of fair-face concrete surfaces-transport and crystallization in hardening concrete10.3151/jact.6.409 ↗
8. A study on the application of the apc (architectural precast concrete) panel for the improvement of modern plasticity in youth training facilities
9. Influence of pore structure and moisture distribution on chloride “maximum phenomenon” in surface layer of specimens exposed to cyclic drying-wetting condition10.1016/j.conbuildmat.2016.11.071 ↗
10. A novel method for assessing C-S-H chloride adsorption in cement pastes10.1016/j.conbuildmat.2019.07.212 ↗
11. Chloride binding capacity of pastes influenced by carbonation under three conditions10.1016/j.cemconcomp.2017.08.011 ↗
12. Jin · 2020 · 1
13. Experimental study on durability of high performance fair faced concrete
14. Research on durability of bridge fair-faced concrete
15. Tao, Y.P., Gu, K.P., Zhong, S., 2018. The effect of fly ash on the durability of fair-faced concrete under seawater erosion environment. N. Build. Mater. 45(5),14-17+40.
16. Lv, D., Liu, D., 2010. Research on durability of architectural concrete based on experimental investigation and engineering application. R.E.I.T. 499-503.
17. Experimental study on corrosion resistance and microstructure hydration properties of High Performance Fair-faced Concrete
18. Experimental research on mechanical properties and mix proportion optimization of fair-faced concrete
19. Influence of SAP on the chloride penetration and corrosion behavior of steel bar in concrete10.1016/j.corsci.2020.108714 ↗
20. Mechanisms of cement hydration10.1016/j.cemconres.2010.09.011 ↗
21. Durability of copper slag contained concrete exposed to sulfate attack10.1016/j.conbuildmat.2010.11.067 ↗
22. Experimental and numerical study of the effects of solution concentration and temperature on concrete under external sulfate attack10.1016/j.cemconres.2020.106284 ↗
23. GB/T 50082-2009. Standard for test methods of long-term performance and durability of ordinary concrete. Beijing: China Construction Industry Press. 2009. 155-157.
24. Jin · 2006
25. GB/T 50081-2002. Standard for test method of mechanical properties on ordinary concrete. 2003. 53-67.
26. Durability and aesthetics of architectural concrete under chloride attack or carbonation10.3390/ma13040839 ↗
27. Kang · 2018
28. Durability and mechanism of high-salt resistance concrete exposed to sewage-contaminated seawater10.1016/j.conbuildmat.2020.119534 ↗
29. Effect of ion chelator on microstructure and properties of cement-based materials under sulfate dry-wet cycle attack10.1016/j.conbuildmat.2020.119527 ↗
30. Damage mechanism and interfacial transition zone characteristics of concrete under sulfate erosion and Dry-Wet cycles10.1016/j.conbuildmat.2020.119340 ↗
31. Compressive and direct tensile behavior of concrete containing Forta-Ferro fiber and calcium aluminate cement subjected to sulfuric acid attack with optimized design10.1016/j.conbuildmat.2020.118999 ↗
32. Interaction between sulfate and chloride solution attack of concretes with and without fly ash10.1016/j.cemconres.2007.02.016 ↗
33. Durability of concrete exposed to leaching and external sulphate attacks10.1016/j.cemconres.2009.07.021 ↗
34. Durability of metakaolin concrete to sulfate attack10.1016/j.cemconres.2006.03.026 ↗
35. Microstructural origins of cement paste degradation by external sulfate attack10.1016/j.conbuildmat.2015.07.186 ↗
36. Shui · 2014 · 269