Abstract
Abstract Although using polymeric waste as a substitution for stone aggregate in concrete can greatly contribute to diminishing environmental issues, it leads to the degradation of many mechanical features of concrete. To approach this issue, using upgraded waste granules can improve these degraded features. Therefore, for the first time in this work, through hot-compacting nylon waste, the compressive stress–strain performance of fiber-reinforced concrete incorporating upgraded nylon waste was assessed before and after heating. To do this, 81 concrete samples were made and subjected to the axial compressive test, with test variables of the volume of the upgraded nylon waste (0, 10, and 20%) substituting for sand, the volume fraction of steel fibers (0, 0.75, and 1.25%), and the heating temperature (20, 300, and 600 °C). Then, parameters contributing to the compressive behavior of concrete including the compressive strength, strain at peak stress, elastic modulus, ultimate strain, toughness index, and stress–strain graph were evaluated, the surface appearance and failure mode were examined, microstructural observations were conducted, and prediction models of the mechanical features were proposed. Moreover, the residual compressive strength values were assessed versus the estimations of the ACI 216, EN 1994–1-2, and ASCE codes. The results demonstrated that by raising the heat, notable degradation occurred in the mechanical features of the concretes, and the greatest drops occurred after 600 °C, such that compressive strength and elastic modulus on average dropped by 61 and 84%, respectively, and the ultimate strain increased by 2–9 folds. Further, adding nylon granules to the concrete mixtures lowered the mechanical features of the samples while introducing steel fibers improved them. Afterward, two stress–strain models were proposed to capture the post-heating compressive behavior of concrete. These models demonstrated proper agreement with the experimental results. Finally, the response surface method (RSM) was employed to present an optimum solution for the design parameters by maximizing the compressive strength and toughness index of concrete.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fire effects on concrete materials · Innovative concrete reinforcement materials · Structural Behavior of Reinforced Concrete
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (69)
Show source-provided references
1. Nematzadeh, M., Memarzadeh, A., & Karimi, A. (2020). Post-fire elastic modulus of rubberized fiber-reinforced concrete-filled steel tubular stub columns: Experimental and theoretical study. Journal of Constructional Steel Research, 175, 106310.10.1016/j.jcsr.2020.106310 ↗
2. Compressive stress strain behavior of crumb rubber concrete (CRC) and application in reinforced CRC slab10.1016/j.conbuildmat.2018.01.142 ↗
3. Pre-and post-heating behavior of concrete-filled steel tube stub columns containing steel fiber and tire rubber10.1016/j.istruc.2020.07.034 ↗
4. Material and structural performance evaluations of Hwangtoh admixtures and recycled PET fiber-added eco-friendly concrete for CO2 emission reduction10.3390/ma7085959 ↗
5. Combined effects of fly ash and waste ferrochromium on properties of concrete10.1016/j.conbuildmat.2011.11.026 ↗
6. Effects of waste PET as coarse aggregate on the fresh and harden properties of concrete10.1016/j.conbuildmat.2016.08.128 ↗
7. Assessment of mechanical and durability properties of concrete containing waste rubber tire as fine aggregate10.1016/j.conbuildmat.2014.09.102 ↗
8. Recycling of PET bottles as fine aggregate in concrete10.1016/j.wasman.2010.01.030 ↗
9. Predicting post-fire behavior of crumb rubber aggregate concrete10.1016/j.conbuildmat.2019.116834 ↗
10. Mechanical properties and abrasion behaviour of concrete containing shredded PET bottle waste as a partial substitution of natural aggregate10.1016/j.conbuildmat.2013.11.049 ↗
11. Rubber-tire particles as concrete aggregate10.1061/(ASCE)0899-1561(1993)5:4(478) ↗
12. Residual compressive stress-strain relationship for hybrid recycled PET–crumb rubber aggregate concrete after exposure to elevated temperatures10.1061/(ASCE)MT.1943-5533.0002749 ↗
13. Mechanical properties of concrete containing a high volume of tire–rubber particles10.1016/j.wasman.2008.01.015 ↗
14. Axial compressive performance of steel tube columns filled with steel fiber-reinforced high strength concrete containing tire aggregate after exposure to high temperatures10.1016/j.engstruct.2020.110608 ↗
15. ACI 544.1R-96,” State-of-the-Art Report on Fiber Reinforced Concrete”, 2002.
16. The effect of polypropylene fibers on the properties of fresh and hardened lightweight self-compacting concrete10.1016/j.conbuildmat.2010.06.018 ↗
17. Estimating properties of reactive powder concrete containing hybrid fibers using UPV
18. Quantifying curing and composition effects on compressive and tensile strength of 160–250 MPa RPC10.1016/j.conbuildmat.2019.117987 ↗
19. Prediction of shear behavior of steel fiber-reinforced rubberized concrete beams reinforced with glass fiber-reinforced polymer (GFRP) bars10.1016/j.compstruct.2020.113010 ↗
20. Fracture energy-based optimisation of steel fibre reinforced concretes10.1016/j.engfracmech.2013.04.018 ↗
21. Compressive and flexural behaviours of a new steel-fibre-reinforced recycled aggregate concrete with crumb rubber10.1016/j.conbuildmat.2015.01.036 ↗
22. Investigation on the mechanical properties of rubberized steel fiber concrete
23. Effect of elevated temperatures on mechanical properties of high-strength concrete containing varying proportions of hematite10.1002/fam.1102 ↗
24. Effect of fire insulation on fire resistance of hybrid-fiber reinforced reactive powder concrete beams10.1016/j.compstruct.2018.10.073 ↗
25. Compressive behaviour of concrete structures incorporating recycled concrete aggregates, rubber crumb and reinforced with steel fibre, subjected to elevated temperatures10.1016/j.jclepro.2014.02.036 ↗
26. Post-fire compressive strength of recycled PET aggregate concrete reinforced with steel fibers: Optimization and prediction via RSM and GEP10.1016/j.conbuildmat.2020.119057 ↗
27. Effect of elevated temperature and cooling regimes on mechanical and durability properties of concrete containing waste rubber fiber10.1016/j.conbuildmat.2017.01.065 ↗
28. Post-fire residual mechanical properties of concrete made with recycled rubber aggregate10.1016/j.firesaf.2013.02.002 ↗
29. ASTM C150. Annual Book of ASTM Standards. Philadelphia, PA: ASTM; 2012.
30. ASTM D2419-14: Standard test method for sand equivalent value of soils and fine aggregate.
31. ASTM C33. Standard specification for concrete aggregates. Annual Book of ASTM Standards; 2004.
32. ASTM C128: Standard Test Method for Density, Relative Density (Specific Gravity), and Absorption of Fine Aggregate
33. ACI 211.1-91 Standard Practice for Selecting Proportions for Normal, Heavyweight, and Mass Concrete ---Procedure for Mix Design
34. ASTM C 143/C 143M-98, (1998). Standard Test Method for Slump of Hydraulic Cement Concrete.
35. ASTM C192, C. (2006). Standard practice for making and curing concrete test specimens in the laboratory. ASTM International, West Conshohocken.
36. ISO. (1975). Fire resistance tests-elements of building construction. International Standard ISO 834, Geneva.
37. Evaluation of post-heating flexural behavior of steel fiber-reinforced high-strength concrete beams reinforced with FRP bars: Experimental and analytical results10.1016/j.engstruct.2020.111292 ↗
38. Compressive performance of steel fiber-reinforced rubberized concrete core detached from heated CFST10.1016/j.conbuildmat.2019.117832 ↗
39. Effect of rock wool waste on compressive behavior of pumice lightweight aggregate concrete after elevated temperature exposure
40. ACI (American Concrete Institute). (1989). Guide for determining the fire endurance of concrete elements. ACI 216R-89, Farmington Hills, MI.
41. Standard test method for compressive strength of cylindrical concrete specimens
42. Influence of waste rubber utilization on the fracture and steel–concrete bond strength properties of concrete10.1016/j.conbuildmat.2015.10.030 ↗
43. Concrete strength for fire safety design10.1680/macr.2005.57.8.445 ↗
44. Experimental investigations on residual bond performance in concrete subjected to elevated temperature10.1016/j.engstruct.2019.02.061 ↗
45. Thermal insulation enhancement in concretesby adding waste PET and rubber pieces10.1016/j.conbuildmat.2008.09.014 ↗
46. Eurocode 4, EN 1994-1-2:2004. Design of composite steel and concrete structures–Part 1-2: General rules for structural fire design.
47. Lie · 1992
48. The influence of aggregate type on the strength and elastic modulus of high strength concrete10.1016/j.conbuildmat.2014.08.055 ↗
49. The effect of forta-ferro and steel fibers on mechanical properties of high-strength concrete with and without silica fume and nano-silica10.1016/j.conbuildmat.2017.01.078 ↗
50. Microstructure of fire-damaged concrete. A case study10.1016/j.cemconcomp.2004.02.022 ↗
51. Experimental investigation on compression toughness of rubberized steel fibre concrete10.1016/j.conbuildmat.2016.04.022 ↗
52. Mechanical properties of steel fiber reinforced reactive powder concrete following exposure to high temperature reaching 800 C10.1016/j.nucengdes.2011.04.008 ↗
53. Post-fire mechanical performance of concrete made with selected plastic waste aggregates10.1016/j.cemconcomp.2014.07.004 ↗
54. Compressive behavior of steel fiber reinforced recycled aggregate concrete after exposure to elevated temperatures10.1016/j.conbuildmat.2014.08.012 ↗
55. The effect of elevated temperatures on the mechanical properties of concrete with fine recycled refractory brick aggregate and aluminate cement10.1016/j.conbuildmat.2017.04.138 ↗
56. Impact of elevated temperatures on the structural performance of recycled rubber concrete: Experimental and mathematical modeling
57. Residual properties of concrete containing recycled refractory brick aggregate at elevated temperatures10.1061/(ASCE)MT.1943-5533.0002125 ↗
58. Dougill, J. W. (1968). Some effects of thermal volume changes on the properties and behaviour of concrete.
59. Analytical model for concrete confinement in tied columns10.1061/JSDEAG.0006100 ↗
60. Tassios TP. Specific rules for concrete structures. In background document for Eurocode 8 -part1, Design rules, Commission of European communities, 1989.
61. Mansur, M. A., Chin, M. S., and Wee, T. H. (1999). Stress-strain relation-ship of high-strength fiber concrete in compression. J. Mater. Civil Eng., 10.1061/(ASCE)0899-1561(1999)11:1(21), 21–29.10.1061/(ASCE)0899-1561(1999)11:1(21) ↗
62. Residual stress–strain relationship for concrete after exposure to high temperatures10.1016/j.cemconres.2006.05.029 ↗
63. Stress-strain behavior of freshly compressed concrete under axial compression with a practical equation10.1016/j.conbuildmat.2016.04.045 ↗
64. Stress-strain relationship for plain concrete in compression
65. Erosion resistance of high-strength concrete containing forta-ferro fibers against sulfuric acid attack with an optimum design10.1016/j.conbuildmat.2017.07.180 ↗
66. Optimization of mechanical properties in concrete reinforced with fibers from solid urban wastes (PET bottles) for the production of ecological concrete10.1016/j.conbuildmat.2017.05.148 ↗
67. Wear minimisation in concrete with haematite10.1179/1433075X12Y.0000000034 ↗
68. Mechanical properties of GGBFS-based geopolymer concrete incorporating natural zeolite and silica fume with an optimum design using response surface method
69. Design-Expert (R) 8 software, Stat-Ease, Inc., Minneapolis, MN, USA 2012.