Low temperature process to create brick
Source abstract
Abstract
Abstract The making of durable alkali-activated aluminosilicate brick can be accomplished on a small or industrial scale according to the needs of the community. Brick made with this technology can be obtained in a few hours using a pressurized vessel and elevated curing temperatures (⩾100 °C) or after three to four weeks if the brick is cured under a tarp or in a solar heated enclosure in areas where energy is unavailable. The process is less expensive than conventional kiln firing of brick, because the development of strength vis a vis sintering is a result of a chemical reaction that takes place at a relatively low temperature. Starting materials available in Senegal consist of highly leached aluminosilicate soils (laterites) and tuffs that primarily contain kaolin, and/or or certain by-product materials now considered to be industrial waste (e.g. aluminum refining sludge). The dry ingredients are mixed with just enough concentrated caustic solution to form a thick paste, compacted in a mold, and allowed to cure. Caustic can consist of sodium hydroxide mixed with sodium silicate and water/seawater. The bricks produced in this fashion are durable and relatively inexpensive to make, thus the technology should appeal to those living in villages in less industrialized nations such as Senegal, because the technology uses locally available materials and solar heating that are available almost everywhere.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Recycling and utilization of industrial and municipal waste in materials production · Concrete and Cement Materials Research · Building materials and conservation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. N‘Diaye, Diop MMB, Ngom PM, Besson JC. Pouzolanic activity of acid and intermediary volcanic tuffs of Mako areas (Senegal). In: International Symposium on Industrial Minerals and Building Stones, International Association of Engineering Geology and the Environment (IAEGE), Proceedings; September 15–18 2003. p. 517–23.
2. Diop B, Jauberthie R, Melinge Y. Bouguerra. Influence of volcanic tuff fillers on the durability of mortar stored in sulfatic environment. In: Proceedings International symposium, Durability of concrete; Canmet/ACI congress, Montreal, Canada; June 2006.
3. Geopolymers and geopolymeric materials10.1007/BF01904446 ↗
4. Comparison of materials for making hydroceramic waste forms
5. Zeolites synthetized from Class F fly ash and sodium aluminate slurry10.1111/j.1151-2916.1997.tb03143.x ↗
6. Alkali-activated fly ashes A cement for the future10.1016/S0008-8846(98)00243-9 ↗
7. Chemical stability of cementious materials based on metakaolin10.1016/S0008-8846(99)00074-5 ↗
8. Breck · 1974
9. Dyer · 1988
10. Zeolite formation in alkali-activated cementitious systems10.1016/j.cemconres.2003.11.003 ↗
11. Binders for radioactive waste forms made from pretreated calcined sodium bearing waste (SBW)10.1023/B:JMSC.0000011502.85255.a8 ↗
12. Solidification of sodium bearing waste using hydroceramic and portland cement binders10.1002/9781118408438.ch24 ↗
13. Preparation and properties of hydroceramic waste forms made with simulated Hanford low-activity waste10.1111/j.1551-2916.2005.00775.x ↗
14. Bao Y, Grutzeck MW. General recipe and properties of a four inch hydroceramic waste form. In: Ceramic Transactions, vol. 176 (Environmental Issues and Waste Management Technologies in the Ceramic and Nuclear Industries XI), Am Ceram Soc, Westerville, OH; 2006. p. 63–74.10.1002/9781118407950.ch7 ↗
15. Reaction of kaolinite with caustic soda
16. Nature of the interaction of kaolinite with some bases
17. Richardson CK, Markuszewski R, Durham KS, Bluhm, DD. Effect of caustic and microwave treatment on clay minerals associated with coal. In: ACS Symposium Series, vol. 301, Mineral Matter Ash Coal; 1986. p. 513–23.10.1021/bk-1986-0301.ch038 ↗
18. Interaction of kaolinite with sodium hydroxide solutions
19. Influence of the degree of dehydroxylation of Kaolinite on the properties of aluminosilicate glasses10.1023/A:1010138130395 ↗
20. Characterization and quantification of the reactive fraction in volcanic pozzolans