Characterization of the degradation of self-compacting concretes in sodium sulfate environment: Influence of different mineral admixtures

H. Siad, S. Kamali-Bernard, H.A. Mesbah, G. Escadeillas, M. Mouli, H. Khelafi

Publisher page

Abstract

Abstract The effects of the type of mineral addition on the behavior of SCCs in sodium sulfate environments were studied. Three strength classes (30 MPa, 50 MPa and 70 MPa) and three different mineral additions were investigated: limestone filler, fly ash and natural pozzolan. The results were compared to those of vibrated concretes. Compressive strength, mass and dimensional changes dues to sodium sulfate attack were determined. The microstructure was studied using SEM–EDS and XRD analysis. For 720 days of immersion in 5% Na 2 SO 4 solution, the penetration depth of sulfate in different samples was quantified using SEM–EDS. The results were consistent with those of XRD analysis. This study shows the benefic effect of the incorporation of a natural pozzolan as a mineral admixture in SCC on the resistance of these concretes in sodium sulfate medium. SCCs with natural pozzolan present characteristics very comparable with those of SCC mixtures with fly ash. It appears that the use of vibrated concretes or SCC with limestone filler, especially with low compressive strength, in a rich sodium sulfate environment is not recommended.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Durability of self-consolidating concrete to sulfate attack under combined cyclic environments and flexural loading10.1016/j.cemconres.2008.12.003 ↗
2. Effect of mineral admixture on resistance to sulphuric and hydrochloric acid attacks in selfcompacting concrete10.1139/L09-157 ↗
3. Influence of cement type on ITZ porosity and chloride resistance of self-compacting concrete10.1016/j.cemconcomp.2009.11.007 ↗
4. Effect of mineral admixtures on properties of self-compacting concrete10.1016/j.cemconcomp.2011.04.005 ↗
5. The effect of mineral admixtures on mechanical properties, chloride ion permeability and impermeability of self-compacting concrete10.1016/j.conbuildmat.2011.07.049 ↗
6. Properties of self-compacting concretes made with binary, ternary, and quaternary cementitious blends of fly ash, blast furnace slag, and silica fume10.1016/j.conbuildmat.2008.09.015 ↗
7. Sulfate resistance of self-compacting concrete10.1016/S0008-8846(03)00184-4 ↗
8. Resistance of different types of concretes to cyclic sulfuric acid and sodium sulfate attack10.1016/j.cemconcomp.2010.07.002 ↗
9. American Concrete Institute. Building code requirements for structural concrete. ACI 318-99.
10. Roziere E. Etude de la durabilité des bétons par une approche performantielle. PhD Thèses, l’Ecole Centrale de Nantes; 2007.
11. GCI-714. Cours: Durabilité et Réparations du Béton. Université de Sherbrooke, Canada; 2009.
12. Microstructural study of the effect produced by magnesium sulfate on plain and silica fume-bearing Portland cement mortars10.1016/0008-8846(93)90004-S ↗
13. Durability of concrete exposed to leaching and external sulfate attacks10.1016/j.cemconres.2009.07.021 ↗
14. Sulfate attack on concrete with mineral admixtures10.1016/0008-8846(95)00195-6 ↗
15. The confused world of sulfate attack on concrete10.1016/j.cemconres.2004.04.004 ↗
16. Sulfate resistance of self-compacting concrete10.1016/S0008-8846(03)00184-4 ↗
17. Durability performance of self-consolidating concrete
18. Durability of self-consolidating concrete to combined effects of sulfate attack and frost action10.1617/s11527-008-9356-z ↗
19. Performance of self-compacting concrete containing different mineral admixtures10.1016/j.conbuildmat.2011.04.032 ↗
20. Association Française de Génie Civil (AFGC). Interim recommendations for use of self-compacting concrete; July 2002.
21. Backscattered electron imaging of cementitious microstructures: understanding and quantification10.1016/j.cemconcomp.2004.02.029 ↗
22. Sedran T, De Larrard F. BetonlabPro 2, ComputerAided MixDesign Software. Presses de l’Ecole Nationale des Ponts et Chaussées, 28 rue des Saints-Pères, 75007 Paris, France; 2000.
23. Dreux G, Festa J. Nouveau guide du béton. Eyrolles édition, France; 1995. RILEM TC 107-CSP. Measurement of time-dependent strains of concrete. Mater Struct 1998;31:507–12.10.1007/BF02481530 ↗
24. Consequences mecaniques de l’attaque sulfatique externe sur les betons autoplaçants
25. American Society for Testing and Materials. Standard test method for length change of hydraulic-cement mortars exposed to a sulfate solution. ASTM C1012-04; 2004.
26. Evaluation of sulfate resisting cements by a new test method
27. Material and environmental parameter effects on the leaching of cement pastes: experiments and modelling10.1016/j.cemconres.2007.10.009 ↗
28. Characterization of the mechanical damage of a chemically degraded cement paste10.1617/s11527-005-9011-x ↗
29. The confused world of sulfate attack on concrete, review10.1016/j.cemconres.2004.04.004 ↗
30. Predicting the durability of Portland cement systems in aggressive environments – laboratory validation10.1016/j.cemconres.2004.03.029 ↗
31. Some engineering properties of concrete containing natural pozzolana and silica fume10.3130/jaabe.5.349 ↗
32. Effect of limestone filler on the deterioration of mortars and pastes exposed to sulfate solutions at ambient temperature10.1016/j.cemconres.2007.08.003 ↗
33. Sustainable development and durability of self-compacting concretes
34. Siad H. Influence du type d’addition minérale sur le comportement physico-mécanique et sur la durabilité des bétons autoplaçants. PhD Thèses, INSA de RENNES (France); 2010.