journal article·2014-02

Alkali reactivity of crushed clay brick aggregate

Fatih Bektaş

Publisher page

Abstract

Abstract Use of recycled aggregate in concrete is a viable alternative when it is economically feasible. Recycled red clay brick either from construction rubble or from brick manufacturing rejects has been widely investigated as concrete aggregate. While engineering properties of clay brick aggregate has been the focus of numerous studies, research on the durability characteristics is limited. This paper presents the findings of a laboratory study that investigates the alkali reactivity of crushed red clay brick aggregate. Mortar mixes, in which crushed brick constitutes 10%, 25%, 50% and 100% of aggregate, and concrete mixes, which contained 0%, 50% and 100% crushed coarse brick aggregate, were produced. Expansion was determined by employing mortar bars and concrete prisms that were subjected to ASR-promoting conditions (e.g., elevated temperature, high humidity, enhanced alkaline environment). Effects of clay brick aggregate on engineering properties (i.e., compressive strength, flexural strength, and static elastic modulus) of concrete were also investigated using cylindrical and prismatic specimens conditioned as the other specimens for ASR testing. Additionally, microstructural investigation was carried out on samples using scanning electron microscope. The test results showed that the clay brick aggregate caused linear expansion proportional to its quantity. Based on a 0.05% expansion at 6 months criterion for the mortar bars stored at 38 °C over water none of the brick aggregate levels were deleteriously expansive. On the other hand, 10%, 25% and 50% brick aggregate mixtures, when tested in sodium hydroxide solution at 80 °C, produced significant expansions according to 0.10% expansion limit at 14 days. Microscope investigation confirmed the presence of alkali silica gel. Ettringite formation was also observed in the specimens examined. Compressive and flexural strengths of concrete were found to be negatively affected by the sodium hydroxide that was added to the mixing water. The clay brick aggregate concretes experienced expansion, however, no visual cracking was observed and there was no measured loss in engineering properties (i.e., compressive strength, flexural strength, and static elastic modulus) when compared to the control mix.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Recycled Aggregate Concrete Performance · Concrete and Cement Materials Research · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Recycling of demolished masonry rubble as coarse aggregate in concrete: review10.1061/(ASCE)0899-1561(2004)16:4(331) ↗
2. The use of recycled aggregate in concrete in Hong Kong10.1016/j.resconrec.2006.06.005 ↗
3. Properties of higher strength concrete made with crushed brick as coarse aggregate
4. Performance of overburnt distorted bricks as aggregates in pavement works10.1061/(ASCE)0899-1561(2006)18:6(777) ↗
5. Properties of concrete using crushed brick aggregate
6. Properties of concrete using crushed clinker brick as coarse aggregate
7. Performance and durability of concrete made with demolition waste and artificial fly ash-clay aggregates10.1016/S0956-053X(96)00038-4 ↗
8. Crushed brick as coarse aggregate for concrete
9. Using crushed clay brick as coarse aggregate in concrete10.1061/(ASCE)0899-1561(2006)18:4(518) ↗
10. The use of coarse and fine crushed brick as aggregate in concrete10.1016/j.conbuildmat.2006.12.013 ↗
11. Mechanical properties of brick aggregate concrete10.1016/j.conbuildmat.2008.07.023 ↗
12. Properties of concrete incorporating fine recycled aggregate10.1016/j.cemconres.2004.06.017 ↗
13. Effects of concrete durability of using recycled ceramic aggregates10.1617/s11527-005-9014-7 ↗
14. Structural concrete with incorporation of coarse recycled concrete and ceramic aggregates: durability performance10.1617/s11527-008-9411-9 ↗
15. Effects of crushed clay brick on mortar durability10.1016/j.conbuildmat.2008.09.006 ↗
16. Accelerated tests for assessing the potential exhibited by concrete aggregates for alkali-aggregate reaction10.1016/S0958-9465(97)00024-3 ↗
17. The ‘pessimum’ effect in an accelerated mortar bar test using 1M NaOH solution at 80°C10.1016/0958-9465(92)90023-O ↗
18. Alkali-aggregate reaction in concrete containing high-alkali cement and granite aggregate10.1016/S0008-8846(03)00189-3 ↗
19. The effect of delayed ettringite formation and alkali-silica reaction on concrete microstructure
20. Skalny · 2002
21. Delayed ettringite formation — processes and problems10.1016/0958-9465(96)00017-0 ↗
22. Implications of pre-formed microcracking in relation to the theories of DEF mechanism10.1016/j.cemconres.2006.10.014 ↗
23. Ettringite in hydration of Portland cement concrete and its occurrence in mature concrete
24. A state-of-the-art review on delayed ettringite attack on concrete10.1016/S0958-9465(02)00080-X ↗
25. Conclusions of the international RILEM TC 186-ISA workshop on internal sulfate attack and delayed ettringite formation (4–6 September 2002, Villars, Switzerland)10.1007/BF02481597 ↗
26. Sulfate attack on concrete: separating myths from reality
27. Effect of ettringite morphology on DEF-related expansion10.1016/j.cemconcomp.2010.01.002 ↗
28. Diagnosing delayed ettringite formation in concrete structures10.1016/j.cemconres.2008.01.003 ↗
29. Won M. Premature concrete deterioration due to ASR/DEF in Texas. In: Proceedings of international center for aggregates research 11th annual symposium: aggregates, asphalt concrete, Bases and Fines, Austin, Texas, US, 2003. [accessed online].
30. Delayed ettringite formation10.1016/S0008-8846(01)00466-5 ↗
31. Effect of alkalies on Portland cement hydration II. Alkalies present in form of sulphates10.1016/0008-8846(83)90078-9 ↗
32. Effects of alkali addition on the mechanical properties and durability of concrete10.1016/j.cemconres.2004.05.007 ↗
33. Engineering properties of concrete affected by alkali-silica reaction
34. Alkali-silica reactivity of some frequently used lightweight aggregates10.1016/j.cemconres.2004.01.017 ↗