journal article·2018-10

Influence of Barchip fiber on early-age cracking potential of high performance concrete under restrained condition

Dejian Shen, Wenting Wang, Jiwei Liu, Xiaoguang Zhao, Guoqing Jiang

Publisher page

Abstract

Abstract High performance concrete (HPC), which is a new-tech concrete, has been widely applied for its good workability, lasting durability, low permeability, and high strength. However, the high temperature rise and high autogenous shrinkage induced by the low water-to-cement (w/c) ratio would increase the early-age cracking potential in HPC. In order to reduce the cracking potential of HPC, Barchip fibers are applied to strengthen the early-age properties. Although the influence of Barchip fibers on the mechanical properties of concrete has been studied, investigations on the influence of Barchip fibers on the early-age cracking potential of HPC under adiabatic condition at uniaxial constant restraint degree are still lacking. The early-age cracking potential of HPC reinforced with different amounts of Barchip fibers (0, 4, 8, and 12 kg/m3) was tested by Temperature Stress Test Machine under adiabatic condition at full restraint degree in present study. Test results and corresponding analysis indicated that (1) the compressive strength and splitting tensile strength were enhanced by the addition of Barchip fibers in HPC; (2) Barchip fibers reduced autogenous shrinkage, restrained tensile stress rate and increased cracking age, specific tensile creep of early-age HPC; (3) the integrated criterion utilized to evaluate the cracking potential decreased first and then increased with increasing amount of Barchip fibers; (4) the optimal Barchip fiber amount of 8 kg/m3 was recommended for that poor dispersion and fiber clumping may occur in HPC with excessive addition of Barchip fibers.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete Properties and Behavior · Innovative concrete reinforcement materials · Fire effects on concrete materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (91)

Show source-provided references
1. The influence of longitudinal cracks on the corrosion protection afforded reinforcing steel in high performance concrete10.1016/j.cemconres.2008.03.018 ↗
2. Relationship between tensile Young’s modulus and strength of fly ash high strength concrete at early age10.1016/j.conbuildmat.2016.06.145 ↗
3. Tensile creep behavior of high strength concretes at early ages10.1007/BF02479631 ↗
4. Experimental study of early-age bond behavior between high strength concrete and steel bars using a pull-out test10.1016/j.conbuildmat.2016.03.094 ↗
5. T.J. Barrett, V.I. De la, W.J. Weiss, Reducing cracking in concrete structures by using internal curing with high volumes of fly ash, in: Structures Congress: Design of Concrete Bridges with Innovative Materials, 2012, 699–707.10.1061/9780784412367.063 ↗
6. Protected paste volume in concrete: extension to internal curing using saturated lightweight fine aggregate10.1016/S0008-8846(99)00178-7 ↗
7. An experimental approach for the analysis of early-age behaviour of high-performance concrete structures under restrained shrinkage10.1016/j.cemconres.2006.11.005 ↗
8. Early-age properties of cement-based materials: II. Influence of water-to-cement ratio10.1061/(ASCE)0899-1561(2009)21:9(512) ↗
9. Early age residual stress and stress relaxation of fly ash high-performance concrete10.1680/jmacr.16.00216 ↗
10. Self-desiccation and its importance in concrete technology10.1007/BF02486354 ↗
11. The effects of polypropylene fibers additions on compressive and tensile strengths of concrete
12. Unrestrained early age shrinkage of concrete with polypropylene, PVA, and carbon fibers10.1617/s11527-006-9106-z ↗
13. Developing crack resistant FRC overlay materials for repair Applications10.1139/l05-093 ↗
14. Tensile creep and cracking resistance of concrete with different water-to-cement ratios at early age10.1016/j.conbuildmat.2017.04.056 ↗
15. Controlling the coefficient of thermal expansion of cementitious materials-a new application for superabsorbent polymers10.1016/j.cemconcomp.2012.08.010 ↗
16. Effect of different fibers on the mechanical properties of concrete containing fly ash10.1016/j.conbuildmat.2006.06.026 ↗
17. Tensile creep and cracking potential of high performance concrete internally cured with super absorbent polymers at early age10.1016/j.conbuildmat.2017.12.136 ↗
18. Mechanical properties of high strength concrete reinforced with metallic and non-metallic fibres10.1016/j.cemconcomp.2007.03.006 ↗
19. Development of high strength flowable mortar with hybrid fibre10.1016/j.conbuildmat.2009.11.013 ↗
20. Workability of hybrid fibre reinforced self-compacting concrete10.1016/j.buildenv.2004.12.014 ↗
21. Shrinkage cracking-can it be prevented
22. Shrinkage cracking of fiber reinforced concrete
23. V. Ramakrishnan, W.V. Coyle, Steel fiber reinforced super-plasticized concretes for rehabilitation of bridge decks and highway pavements. Final Report to U.S. Department of Transportation, DOT/RSPA/DMA-50/84-2, 1983, 408.
24. Alternative reinforcing materials for developing countries
25. Fracture toughness of fiber reinforced concrete
26. Design of hybrid-fiber reinforcement for shrinkage cracking by crack width predictions
27. Creep, shrinkage, and cracking of restrained concrete at early age
28. K. Behfarnia, A. Behravan, An experimental study on mechanical properties of HPP fiber reinforced concrete (Barchip fibers). International Conference on Concrete and Development, 2013.
29. Mechanical behaviors of concrete combined with steel and synthetic macro-fibers10.12989/cac.2007.4.3.207 ↗
30. Application of high performance polypropylene fibers in concrete lining of water tunnels10.1016/j.matdes.2013.09.075 ↗
31. Tensile basic creep: measurements and behavior at early age
32. Parametric assessment of stress development and cracking in internally cured restrained mortars experiencing autogenous deformations and thermal loading
33. Quantifying stress development and remaining stress capacity in restrained, internally cured mortars
34. Effect of internal curing with super absorbent polymers on residual stress development and stress relaxation in restrained concrete ring specimens10.1016/j.conbuildmat.2016.05.048 ↗
35. Testing system for determining the mechanical behavior of early age concrete under restrained and free uniaxial shrinkage10.1007/BF02473424 ↗
36. Tensile creep behavior of concrete subject to constant restraint at very early ages10.1061/(ASCE)MT.1943-5533.0000671 ↗
37. Internal curing of high-performance concrete with pre-soaked fine lightweight aggregate for prevention of autogenous shrinkage cracking10.1016/j.cemconres.2008.02.001 ↗
38. Influence of prewetted lightweight aggregates on the behavior and cracking potential of internally cured concrete at an early age10.1016/j.conbuildmat.2015.08.093 ↗
39. Influence of curing temperature on autogenous shrinkage and cracking resistance of high-performance concrete at an early age10.1016/j.conbuildmat.2015.11.039 ↗
40. ACI Committee 207, Effect of restraint, volume change and reinforcement on cracking of mass concrete (207.2R-95), Farmington Hills, Mich, 1995.
41. Early-age tensile creep and cracking potential of concrete internally cured with pre-wetted lightweight aggregate10.1016/j.conbuildmat.2016.12.187 ↗
42. Effect of fiber types on creep behavior of concrete10.1016/j.conbuildmat.2015.12.149 ↗
43. Effect of different fiber orientations on compressive creep behavior of SiC fiber-reinforced mullite matrix composites10.1016/S0955-2219(99)00022-9 ↗
44. Short-term tensile creep and shrinkage of ultra-high performance concrete10.1016/j.cemconcomp.2009.01.002 ↗
45. Tensile basic creep versus compressive basic creep at early ages: comparison between normal strength concrete and a very high strength fiber reinforced concrete10.1617/s11527-013-0150-1 ↗
46. Application of non-corrosive Barchip fibres for high strength concrete enhancements in aggressive environments10.1016/j.compositesb.2013.04.012 ↗
47. Fibrous ferrocement composite with PVC-coated weld mesh and bar-chip polyolefin fibers
48. R. Springenschmid, R. Breitenbucher, Influence of constituents, mix proportions and temperature on cracking sensitivity of concrete, in: Springenschmid, R., (Ed.), Proc. Int. RILEM Symp., Prevention of Thermal Cracking in Concrete at Early Stages, E & FN Spon, London, UK, 1998, pp. 40–50.
49. CS (Chinese Standard) GB 175-2007/XG1-2009. Common Portland Cement, Quality Supervision Inspection and Quarantine of the People’s Republic of China and Standardization Administration of the People’s Republic China, China, 2009 (in Chinese).
50. ASTM C150 (2012) Standard Specification for Portland cement.
51. Shrinkage of polypropylene fiber-reinforced high-performance concrete10.1061/(ASCE)MT.1943-5533.0000258 ↗
52. R. Springenschmid, E. Gierlinger, W. Kiernozicky, Thermal stresses in mass concrete: a new testing method and he influence of different cements, in: Proceedings of the 15th International Conference on Large Dams (ICOLD), Lausanne, 1985, 57–72.
53. Tensile creep due to restraining stresses in high-strength concrete at early ages10.1016/j.cemconres.2005.11.017 ↗
54. S.J. Lokhorst, Deformational behavior of concrete influenced by hydration related changes of the microstructure, Research Report, Delft University of Technology, Delft, The Netherlands, 1998.
55. Early-age cracking in reconstructed concrete bridge barrier walls
56. CS (Chinese Standard) GB/T 50081-2002, Standard for Test Method of Mechanical Properties on Ordinary Concrete, Ministry of Construction of the People’s Republic of China and Quality Supervision Inspection and Quarantine of the People’s Republic of China, China, 2002 (in Chinese).
57. W. Liu, Z.Q. Zhu, Research on performance of polypropylene fiber concrete. Low Temperature Architecture Technology, 2009, (in Chinese).
58. On the origin of eigenstresses in lightweight aggregate concrete10.1016/S0958-9465(03)00072-6 ↗
59. Research on early cracking sensitivity of polypropylene fiber reinforced concrete
60. Å.L. Døssland, Fibre reinforcement in load carrying concrete structures: laboratory and field investigations compared with theory and finite element analysis, Fakultet for Naturvitenskap Og Teknologi, 2008.
61. High-performance fiber-reinforced concrete: a review10.1007/s10853-016-9917-4 ↗
62. Fibre reinforced cement-based (FRC) composites after over 40 years of development in building and civil engineering10.1016/j.compstruct.2008.03.006 ↗
63. Effect of workability characteristics on the hardened performance of FRSCCMs10.1016/j.conbuildmat.2012.11.051 ↗
64. Investigation on mechanical properties and microstructure of high performance polypropylene fiber reinforced lightweight aggregate concrete10.1016/j.conbuildmat.2016.04.116 ↗
65. Effect of curing temperature and type of cement on early-age shrinkage of high-performance concrete10.1016/S0008-8846(01)00601-9 ↗
66. Early ages shrinkage and cracking in cementitious systems
67. Effect of autogenous deformation on the cracking risk of slag cement concretes10.1016/j.cemconcomp.2010.12.003 ↗
68. Predicting relative humidity of early-age concrete under sealed and unsealed conditions
69. Separation of thermal and autogenous deformation at varying temperatures using optical fiber sensors10.1016/j.cemconcomp.2007.01.005 ↗
70. Estimation of temperature effects on autogenous shrinkage of concrete by a new prediction model10.1016/j.conbuildmat.2012.03.005 ↗
71. Plastic shrinkage cracking in concrete materials-influence of fly ash and fibers
72. Carbon and steel microfiber-reinforced cement-based composites for thin repairs10.1061/(ASCE)0899-1561(1994)6:1(88) ↗
73. Leemann · 2014 · 73
74. Mehta · 2006
75. Influences of fibers on drying shrinkage of fiber-reinforced cementitious composite10.1061/(ASCE)0733-9399(2001)127:1(37) ↗
76. Effect of polypropylene fibers on shrinkage and cracking of concretes10.1617/s11527-008-9361-2 ↗
77. S. Hagihara, Y. Masuda, S. Nakamura, Creep Behaviour of High-Strength Concrete in Early Age. 6th International Symposium on High Strength/High Performance 2002.
78. Influence of ring size on the restrained shrinkage behavior of ultra high performance fiber reinforced concrete10.1617/s11527-013-0119-0 ↗
79. Properties of cracking resistance of cemfiber reinforced concrete
80. Mechanical properties of young concrete: Part II: determination of model parameters and test program proposals10.1007/BF02479615 ↗
81. M. Krauß, F.S. Rostasy, A.W. Gutsch, Modelling of degree of hydration on basis of adiabatic heat release. IPACS REPORT BE96-3843, 2001, 13.
82. Maturity computer for controlled curing and hardening of concrete
83. Autogenous shrinkage and induced restraining stresses in high-strength concretes10.1016/S0008-8846(00)00399-9 ↗
84. The character of early-age plastic cracking of polypropylene fiber reinforced concrete and fractal evaluation
85. Zhu · 1999
86. Visco-elastic response
87. Modeling of the influence of fibers on creep of fiber reinforced cementitious composite10.1016/S0266-3538(03)00160-X ↗
88. ASTM, Standard test method for determining age at cracking and induced tensile stress characteristics of mortar and concrete under restrained shrinkage. Standard C 1581–04, ASTM Int, West Conshohocken (PA), 2013.
89. Cracking sensitivity of normal- and high-strength concretes
90. Influences of short discrete fibers in high strength concrete with very coarse sand10.3844/ajassp.2010.1572.1578 ↗
91. Optimized workability and mechanical properties of FRCM by using fiber factor approach: theoretical and experimental study10.1617/s11527-013-0221-3 ↗