journal article·2018-11

Effect of very high limestone content and quality on the sulfate resistance of blended cements

Andre Baldermann, Moien Rezvani, Tilo Proske, Cyrill Grengg, Florian Steindl, Marlene Sakoparnig, Claudia Baldermann, Isabel Galan, Florian Emmerich, Florian Mittermayr

Publisher page

Abstract

Abstract Sulfate attack was investigated on blended ordinary Portland cement (OPC) based mortars with limestone replacements up to 65 wt-% in 30 g·L−1 Na2SO4 solutions at 20 °C and 8 °C for 200 days. Although CEM I 52.5R with ∼12 wt-% C3A was used, some blended mortars with a water/powder ratio of 0.35 and ≤50 wt-% limestone replacement passed the test requirements (Δ-expansion ≤0.5 mm/m after 91 days) and exhibited a better performance than pure OPC reference mixes with water/powder ratios of 0.5 and 0.6. Under accelerated test conditions, the deterioration level of blended mortars arising from sulfate attack can be approximated by the reaction of portlandite with aqueous sulfate to secondary expansive gypsum, ettringite and thaumasite. The pore structure and the reactivity of carbonates and cement hydrates originally present in blended cements should be considered for predicting the long-term stability of concrete in sulfate-loaded environments.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Building materials and conservation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (79)

Show source-provided references
1. Eco-friendly concretes with reduced water and cement contents — mix design principles and laboratory tests10.1016/j.cemconres.2013.04.011 ↗
2. Sulfate resistance of cement-reduced eco-friendly concretes10.1016/j.cemconcomp.2014.09.020 ↗
3. Cements with a high limestone content – mechanical properties, durability and ecological characteristics of the concrete10.1016/j.conbuildmat.2016.05.009 ↗
4. Eco-friendly concretes with reduced water and cement content – mix design principles and application in practice10.1016/j.conbuildmat.2013.12.066 ↗
5. J. Juhart, G.A. David, C. Nickel, F. Mittermayr, Ökologische Optimierung von Beton mit inerten Mikro- und Eco-Füllern, in: Proceedings 19th ibausil, 2015, pp. 1073–1084.
6. Monitoring and modelling the early age and hardening behaviour of eco-concrete through continuous non-destructive measurements: Part II. Mechanical behaviour10.1016/j.cemconcomp.2016.07.003 ↗
7. Chapter 4 – eco-friendly concretes with reduced water and cement content: mix design principles and experimental tests A2 – Nazari, Ali
8. A huge number of artificial waste material can be supplementary cementitious material (SCM) for concrete production – a review part II10.1016/j.jclepro.2015.12.115 ↗
9. Sustainable cement production—present and future10.1016/j.cemconres.2011.03.019 ↗
10. A review of alternative approaches to the reduction of CO2 emissions associated with the manufacture of the binder phase in concrete10.1016/j.cemconres.2015.04.012 ↗
11. The Anthropocene is functionally and stratigraphically distinct from the Holocene10.1126/science.aad2622 ↗
12. Limestone filler cement in low w/c concrete rational use of energy10.1016/S0008-8846(02)01087-6 ↗
13. Recent advances in the field of cement hydration and microstructure analysis10.1016/j.cemconres.2011.03.028 ↗
14. Supplementary cementitious materials10.1016/j.cemconres.2010.12.001 ↗
15. Cement substitution by a combination of metakaolin and limestone10.1016/j.cemconres.2012.09.006 ↗
16. Assessment of the sustainability potential of concrete and concrete structures considering their environmental impact, performance and lifetime10.1016/j.conbuildmat.2014.01.039 ↗
17. Limestone addition effects on concrete porosity10.1016/j.cemconcomp.2016.06.006 ↗
18. Sulfate attack on cementitious materials containing limestone filler – a review10.1016/j.cemconres.2008.11.007 ↗
19. Evaporation — a key mechanism for the thaumasite form of sulfate attack10.1016/j.cemconres.2013.03.003 ↗
20. Durability of concrete — degradation phenomena involving detrimental chemical reactions10.1016/j.cemconres.2007.09.015 ↗
21. Mechanism of sulfate attack on Portland cement concrete — another look10.1016/0008-8846(83)90040-6 ↗
22. Swiss tunnel structures: concrete damage by formation of thaumasite10.1016/S0958-9465(03)00141-0 ↗
23. Effects of gypsum formation on the performance of cement mortars during external sulfate attack10.1016/S0008-8846(02)00955-9 ↗
24. The formation and role of ettringite in Iowa highway concrete deterioration10.1016/j.cemconres.2004.05.029 ↗
25. Effect of limestone filler on the deterioration of mortars and pastes exposed to sulfate solutions at ambien temperature10.1016/j.cemconres.2007.08.003 ↗
26. Analysis of concrete in a vertical ventilation shaft exposed to sulfate-containing groundwater for 45 years10.1016/j.cemconcomp.2010.09.012 ↗
27. Influence of the Ca/Si ratio of the C-S–H phase on the interaction with sulfate ions and its impact on the ettringite crystallization pressure10.1016/j.cemconres.2014.12.002 ↗
28. Physical and microstructural aspects of sulfate attack on ordinary and limestone blended Portland cements10.1016/j.cemconres.2009.08.005 ↗
29. Microstructural study of sulfate attack on ordinary and limestone Portland cements at ambient temperature10.1016/S0008-8846(02)00914-6 ↗
30. Environmental controls and reaction pathways of coupled de-dolomitization and thaumasite formation10.1016/j.cemconres.2017.02.011 ↗
31. Rapid ikaite (CaCO3·6H2O) crystallization in a man-made river bed: hydrogeochemical monitoring of a rarely documented mineral formation10.1016/j.apgeochem.2015.10.003 ↗
32. The decisive role of acidophilic bacteria in concrete sewer networks: a new model for fast progressing microbial concrete corrosion10.1016/j.cemconres.2017.08.020 ↗
33. Microbiologically induced concrete corrosion: a case study from a combined sewer network10.1016/j.cemconres.2015.06.011 ↗
34. An accelerated sulfate resistance test for concrete10.1617/s11527-015-0731-2 ↗
35. “Sulfate attack,” or is it?10.1016/S0008-8846(99)00068-X ↗
36. Does gypsum formation during sulfate attack on concrete lead to expansion?10.1016/S0008-8846(99)00211-2 ↗
37. The confused world of sulfate attack on concrete10.1016/j.cemconres.2004.04.004 ↗
38. Chemo-mechanical modelling of the external sulfate attack in concrete10.1016/j.cemconres.2016.12.003 ↗
39. Ettringite solubility and geochemistry of the Ca(OH)2-Al2(SO4), 3–H2O system at 1 atm pressure and 298 K10.1016/S0009-2541(97)00128-9 ↗
40. Solubility of Fe-ettringite (Ca6[Fe(OH)6]2(SO4)3·26H2O)10.1016/j.gca.2007.09.035 ↗
41. Sulfate attack expansion mechanisms10.1016/j.cemconres.2013.07.005 ↗
42. On the relevance of volume increase for the length changes of mortar bars in sulfate solutions10.1016/j.cemconres.2013.01.002 ↗
43. A thermodynamic and experimental study of the conditions of thaumasite formation10.1016/j.cemconres.2007.11.003 ↗
44. Thaumasite formation in a tunnel of bapanxia dam in Western China10.1016/j.cemconres.2005.10.011 ↗
45. The effect of the secondary component on the hydration of Portland cement: Part 1. A fine non-hydraulic filler10.1016/0008-8846(90)90011-L ↗
46. The role of calcium carbonate in cement hydration10.1016/j.cemconres.2006.10.013 ↗
47. Influence of various amounts of limestone powder on performance of Portland limestone cement concretes10.1016/j.cemconcomp.2009.08.003 ↗
48. Portland-limestone cements. Their properties and hydration compared to those of other composite cements10.1016/j.cemconcomp.2004.02.006 ↗
49. The effects of limestone addition, clinker type and fineness on properties of Portland cement10.1016/S0008-8846(00)00427-0 ↗
50. The filler effect: the influence of filler content and surface area on cementitious reaction rates10.1111/jace.12264 ↗
51. Assessing understanding and unlocking supplementary cementitious materials10.21809/rilemtechlett.2016.12 ↗
52. Thaumasite formation in Portland-limestone cement pastes10.1016/S0008-8846(99)00100-3 ↗
53. Thaumasite formed by sulfate attack on mortar with limestone filler10.1016/S0958-9465(03)00120-3 ↗
54. Concrete under sulphate attack: an isotope study on sulphur sources10.1080/10256016.2012.641964 ↗
55. The occurrence of thaumasite in modern construction – a review10.1016/S0958-9465(01)00092-0 ↗
56. The thaumasite form of sulfate attack in the UK10.1016/S0958-9465(03)00106-9 ↗
57. Thaumasite Sulfate Attack, Popcorn Calcite Deposition and acid attack in concrete stored at the “Blindtarmen” test site Oslo, from 1952 to 198210.1016/j.matchar.2009.01.007 ↗
58. C, O and S isotopic signatures in concrete which have suffered thaumasite formation and limited thaumasite form of sulfate attack10.1016/S0958-9465(03)00110-0 ↗
59. Changes in the phase assemblage of concrete exposed to sea water10.1016/j.cemconcomp.2013.09.015 ↗
60. Mineralogical and chemical assessment of concrete damaged by the oxidation of sulfide-bearing aggregates: Importance of thaumasite formation on reaction mechanisms10.1016/j.cemconres.2012.06.008 ↗
61. Breitenbücher · 2006
62. Impact of drying on pore structures in ettringite-rich cements10.1016/j.cemconres.2016.03.003 ↗
63. Geochemistry and mineralogy of the Oligo-Miocene sediments of the Valley of Lakes, Mongolia10.1007/s12549-016-0268-6 ↗
64. Effect of aqueous Si/Mg ratio and pH on the nucleation and growth of sepiolite at 25°C10.1016/j.gca.2018.02.027 ↗
65. Aragonite–calcite veins of the ‘Erzberg’ iron ore deposit (Austria): environmental implications from young fractures
66. Substantial iron sequestration during green-clay authigenesis in modern deep-sea sediments10.1038/ngeo2542 ↗
67. Influence of porosity on compressive and tensile strength of cement mortar10.1016/j.conbuildmat.2012.11.072 ↗
68. Mercury porosimetry of cement-based materials and associated correction factors
69. Mercury porosimetry – an inappropriate method for the measurement of pore size distributions in cement-based materials10.1016/S0008-8846(00)00370-7 ↗
70. Influence of clay in limestone fillers for self-compacting cement based composites10.1016/j.conbuildmat.2010.09.009 ↗
71. Crystallization in pores10.1016/S0008-8846(99)00002-2 ↗
72. Use of mineral admixtures to prevent thaumasite formation in limestone cement mortar10.1016/S0958-9465(03)00153-7 ↗
73. Experimental study on physical sulfate salt attack10.1617/s11527-016-0936-z ↗
74. The role of calcium hydroxide in the formation of thaumasite10.1016/j.cemconres.2008.04.005 ↗
75. Calcium silicate hydrate (C-S-H) gel solubility data and a discrete solid phase model at 25 degrees C based on two binary non-ideal solid solutions10.1016/j.cemconres.2015.07.006 ↗
76. Solubility behavior of Ca-, S-, Al-, and Si-bearing solid phases in Portland cement pore solutions as a function of hydration time10.1016/S0008-8846(02)00855-4 ↗
77. The density of cement phases10.1016/j.cemconres.2009.06.005 ↗
78. Sulfate ingress in Portland cement10.1016/j.cemconres.2010.04.004 ↗
79. Sulfate transfer through concrete: migration and diffusion results10.1016/j.cemconcomp.2011.05.001 ↗