journal article·2020-07

Effect of Barchip fiber on stress relaxation and cracking potential of concrete internally cured with super absorbent polymers

Dejian Shen, Zhizhuo Feng, Jiacheng Kang, Chuyuan Wen, Huafeng Shi

Publisher page

Abstract

Abstract High-strength concrete (HSC) that has shown the outstanding performance is extensively utilized in construction. HSC usually suffers the high autogenous shrinkage when the water-to-cement (w/c) ratio is low. Internal curing (IC) is developed as reservoir in concrete to reduce HSC shrinkage at early age by introducing additional water. Meanwhile, Barchip fibers have been already utilized to improve material properties of HSC. Investigations on the effect of the proportion of Barchip fibers (0%, 0.3%, 0.6%, and 0.9% by volume fraction of concrete) on early-age stress relaxation of concrete internally cured with super absorbent polymers (SAPs) were conducted by restrained ring test. Results obtained from the test were as follows: (1) the free shrinkage in concrete deceased with the increase of the proportion of Barchip fibers; (2) the strain in steel ring decreased when the proportion of Barchip fibers increased; (3) the residual stress in concrete decreased with the increase of the proportion of Barchip fibers; (4) increasing the proportion of Barchip fibers caused the decrease of stress rate; (5) the relaxed stress increased with increase of Barchip fibers proportion; (6) when the proportion of Barchip fibers increased, the time to cracking of concrete was delayed, and the cracking potential of concrete decreased significantly; (7) SAPs utilized in IC improved the performance of concrete reinforced with Barchip fibers significantly.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete Properties and Behavior · Innovative concrete reinforcement materials · Fire effects on concrete materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Reducing cracking in concrete structures by using internal curing with high volumes of fly ash
2. Influence of ground granulated blast furnace slag on cracking potential of high performance concrete at early age10.1016/j.conbuildmat.2019.117839 ↗
3. Quantifying stress development and remaining stress capacity in restrained, internally cured mortars
4. Early-age cracking resistance of ground granulated blast furnace slag concrete10.1016/j.conbuildmat.2019.06.028 ↗
5. Internally-cured high-performance concrete under restrained shrinkage and creep. Concreep 7 workshop on creep, shrinkage and durability of concrete and concrete structures
6. Effect of internal curing with super absorbent polymers on autogenous shrinkage of concrete at early age10.1016/j.conbuildmat.2015.12.115 ↗
7. Influence of polypropylene fiber geometry on plastic shrinkage cracking in concrete10.1016/j.cemconres.2006.01.010 ↗
8. Early-age behavior and cracking resistance of high-strength concrete reinforced with Dramix 3D steel fiber10.1016/j.conbuildmat.2018.10.125 ↗
9. Effect of internal curing with super absorbent polymers on residual stress development and stress relaxation in restrained concrete ring specimens10.1016/j.conbuildmat.2016.05.048 ↗
10. Influence of initial cracks on the frequency of a 60-year-old reinforced concrete box beam
11. Behavior of reinforced concrete box beam with initial cracks repaired with basalt fiber-reinforced polymer sheet10.1177/0731684415595469 ↗
12. Effects of admixtures and SRA on early age shrinkage of concrete
13. Plastic shrinkage cracking of polypropylene fiber reinforced concrete
14. Bentur · 1990
15. Early-age behavior and cracking potential of fly ash concrete under restrained condition10.1680/jmacr.18.00106 ↗
16. Effect of polypropylene plastic fibers length on cracking resistance of high performance concrete at early age10.1016/j.conbuildmat.2019.117874 ↗
17. Effect of internally stored water on creep of high-performance concrete
18. D.P. Bentz, W.J. Weiss, Internal curing: a 2010 state-of-the-art review. NISTIR 7765, National Institute of Standards and Technology, 2011.10.6028/NIST.IR.7765 ↗
19. Benefits of internal curing on service life and life-cycle cost of high-performance concrete bridge decks – a case study10.1016/j.cemconcomp.2010.02.007 ↗
20. Relaxation of stress in concrete and its relation to creep
21. Prevention of autogenous shrinkage in high-strength concrete by internal curing using wet lightweight aggregates10.1016/S0008-8846(01)00608-1 ↗
22. Efficiency of lightweight aggregates for internal curing of high strength concrete to eliminate autogenous shrinkage10.1007/BF02482108 ↗
23. Application of internal curing for mixtures containing high volumes of fly ash10.1016/j.cemconcomp.2012.06.008 ↗
24. Effect of pre-soaked superabsorbent polymer on shrinkage of high-strength concrete10.1617/s11527-014-0351-2 ↗
25. Super absorbing polymers as an internal curing agent for mitigation of early-age cracking of high-performance concrete bridge decks10.1016/j.conbuildmat.2010.06.063 ↗
26. Water-entrained cement-based materials: I. Principles and theoretical background10.1016/S0008-8846(01)00463-X ↗
27. Effect of internally stored water on creep of high performance concrete
28. Early age creep and stress relaxation of concrete containing blended cements10.1007/BF02482107 ↗
29. Efficiency of polypropylene and metallic fibres on control of shrinkage and cracking of recycled aggregate mortars10.1016/S0950-0618(99)00047-1 ↗
30. Tensile creep behavior of high strength concretes at early ages10.1007/BF02479631 ↗
31. P. Lura, G. Ye, V. Cnudde, P. Jacobs, Preliminary results about 3D distribution of superabsorbent polymers in mortars, in: International Conference on Microstructure Related Durability of Cementitious Composites 2008 Nanjing, China.
32. Free and restrained shrinkage for normal and high strength concretes
33. Effect of double hooked-end steel fiber on early-age cracking potential of high strength concrete in restrained ring specimens10.1016/j.conbuildmat.2019.07.319 ↗
34. Shrinkage cracking of restrained concrete slabs10.1061/(ASCE)0733-9399(1998)124:7(765) ↗
35. Influence of ground granulated blast furnace slag on early-age cracking potential of internally cured high performance concrete10.1016/j.conbuildmat.2019.117083 ↗
36. Influence of specimen size and geometry on shrinkage cracking10.1061/(ASCE)0733-9399(2000)126:1(93) ↗
37. Standard practice for estimating the cracking tendency of concrete
38. ASTM C1581M-18, Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage, ASTM International, West Conshohocken, PA, 2018, pp. 1–7.
39. Potential for restrained shrinkage cracking of concrete and mortar
40. Tensile creep and cracking potential of high performance concrete internally cured with super absorbent polymers at early age10.1016/j.conbuildmat.2017.12.136 ↗
41. Cracking behavior of concrete with shrinkage reducing admixtures and PVA fiber10.1016/j.cemconcomp.2009.08.004 ↗
42. Toughness enhancement in steel fiber reinforced concrete through fiber hybridization10.1016/j.cemconres.2007.05.005 ↗
43. CS (Chinese Standard) GB 175-2007/XG3-2018. Common Portland Cement, Quality Supervision Inspection and Quarantine of the People’s Republic of China and Standardization Administration of the People’s Republic China, China, 2018 (in Chinese).
44. CS (Chinese Standard) GB/T 50080-2016. Standard for test method of performance on ordinary fresh concrete, Ministry of Construction of the People’s Republic of China and Quality Supervision Inspection and Quarantine of the People’s Republic of China, China, 2016 (in Chinese).
45. Protected paste volume in concrete: extension to internal curing using saturated lightweight fine aggregate10.1016/S0008-8846(99)00178-7 ↗
46. Mixture proportioning for internal curing
47. ASTM. Standard Specification for Lightweight Aggregate for Internal Curing of Concrete, Standard C 1761/C 1761M-13b. ASTM International, West Conshohocken, PA, 2013.
48. Influence of Barchip fiber length on early-age behavior and cracking resistance of concrete internally cured with super absorbent polymers10.1016/j.conbuildmat.2019.03.209 ↗
49. CS (Chinese Standard) GB/T 50081-2019, Standard for Test Methods of Concrete Physical and Mechanical Properties, Ministry of Construction of the People’s Republic of China and State Administration for Market Regulation, China, 2019 (in Chinese).
50. Lura · 2003
51. Predicting relative humidity of early-age concrete under sealed and unsealed conditions10.1680/jmacr.18.00068 ↗
52. ASTM C1761/C1761M-17 · 2017
53. Assessing residual stress development and stress relaxation in restrained concrete ring specimens10.1016/S0958-9465(03)00069-6 ↗
54. Shrinkage cracking characteristics of concrete using ring specimens
55. A dual concentric ring test for evaluating residual stress development due to restrained volume change10.1520/JAI103118 ↗
56. Plastic shrinkage cracking in concrete materials – influence of fly ash and fibers
57. Cracking behavior of concrete with shrinkage reducing admixtures and PVA fibers
58. Quantifying shrinkage cracking in fiber reinforced concrete using the ring test10.1617/s11527-006-9089-9 ↗
59. Internal curing by superabsorbent polymers in ultra-high performance concrete10.1016/j.cemconres.2015.05.005 ↗
60. A dual concentric ring test for evaluating residual stress development due to restrained volume change10.1520/JAI103118 ↗
61. Restrained shrinkage testing: the impact of specimen geometry on quality control testing for material performance assessment
62. H.R. Shah, A.B. Hossain, W.J. Weiss, Using the restrained ring test in conjunction with passive acoustic emission to quantify the tole of steel fiber reinforcement in shrinkage cracking mitigation, in: Proceedings of ICFRC International Conference on Fiber Composites, High Performance Concretes and Smart Materials. Chennai, India, Jan 8-10,2004, pp. 99–111.
63. Early age residual stress and stress relaxation of fly ash high-performance concrete10.1680/jmacr.16.00216 ↗
64. Effect of fiber types on creep behavior of concrete10.1016/j.conbuildmat.2015.12.149 ↗
65. Modeling of the influence of fibers on creep of fiber reinforced cementitious composite10.1016/S0266-3538(03)00160-X ↗
66. CEB-FIP (Comite Euro-International du Beton – Federation International de la Precontrainte). Model Code 90. Model Code for concrete Structures, Paris, 1990.
67. Creep, shrinkage and cracking of restrained concrete at early age
68. Analysis of cable networks by dynamic relaxation
69. Influence of age of loading, water-cement ratio and rate of loading on fracture energy of concrete10.1007/BF02472745 ↗
70. Comparative study natural and fibers to reduce plastic shrinkage cracking in cement-based composite
71. Effect of shrinkage-reducing admixture and expansive agent on mechanical properties and drying shrinkage of Engineered Cementitious Composite (ECC)10.1016/j.conbuildmat.2018.05.203 ↗
72. Secondary reinforced-adding cellulose fiber
73. Tensile strength of concrete affected by uniformly distribution and closely spread short lengths of wire reinforcement