Influence of Barchip fiber on early-age autogenous shrinkage of high strength concrete
Source abstract
Abstract
Abstract High strength concrete (HSC) is vulnerable to early-age cracking owing to a low water-to-cement (w/c) ratio. Barchip fibers have been utilized to reduce the autogenous shrinkage of concrete. The relationship between autogenous shrinkage and ultrasonic velocity of HSC reinforced with Barchip fibers was studied utilizing the non-contact shrinkage test. Results indicated that the autogenous shrinkage and ultrasonic velocity of concrete decreased with the volume percentage of Barchip fibers increasing. Besides, models for predicting early-age autogenous shrinkage strain were proposed considering the fiber volume percentage and age based on the results of ultrasonic velocity.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete Properties and Behavior · Innovative concrete reinforcement materials · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (80)
Show source-provided references
1. Properties of high strength polypropylene fiber concrete containing recycled aggregate10.1016/j.conbuildmat.2020.118010 ↗
2. Efficiency of lightweight aggregates for internal curing of high strength concrete to eliminate autogenous shrinkage10.1007/BF02482108 ↗
3. The influence of longitudinal cracks on the corrosion protection afforded reinforcing steel in high performance concrete10.1016/j.cemconres.2008.03.018 ↗
4. Effect of Barchip fiber on stress relaxation and cracking potential of concrete internally cured with super absorbent polymers10.1016/j.conbuildmat.2020.118392 ↗
5. Tensile creep behavior of high strength concretes at early ages10.1007/BF02479631 ↗
6. Early-age cracking resistance of ground granulated blast furnace slag concrete10.1016/j.conbuildmat.2019.06.028 ↗
7. Early-age properties of cement-based materials: II. Influence of water-to-cement ratio10.1061/(ASCE)0899-1561(2009)21:9(512) ↗
8. Effect of polypropylene plastic fibers length on cracking resistance of high performance concrete at early age10.1016/j.conbuildmat.2019.117874 ↗
9. Self-desiccation and its importance in concrete technology10.1007/BF02486354 ↗
10. Early-age behavior and cracking resistance of high-strength concrete reinforced with Dramix 3D steel fiber10.1016/j.conbuildmat.2018.10.125 ↗
11. An experimental approach for the analysis of early-age behaviour of high-performance concrete structures under restrained shrinkage10.1016/j.cemconres.2006.11.005 ↗
12. The effects of polypropylene fibers additions on compressive and tensile strengths of concrete
13. Developing crack resistant FRC overlay materials for repair applications10.1139/l05-093 ↗
14. Unrestrained early age shrinkage of concrete with polypropylene, PVA, and carbon fibers10.1617/s11527-006-9106-z ↗
15. Prevention of autogenous shrinkage in high-strength concrete by internal curing using wet lightweight aggregates10.1016/S0008-8846(01)00608-1 ↗
16. Volume change and cracking in internally cured mixtures made with saturated lightweight aggregate under sealed and unsealed conditions10.1016/j.cemconcomp.2009.04.003 ↗
17. High strength concrete: strength, permeability, and cracking
18. The influence of mix composition, w/b ratio and curing on restrained shrinkage cracking of cementitious mortars10.1016/j.conbuildmat.2018.04.099 ↗
19. Influence of ground granulated blast furnace slag on early-age cracking potential of internally cured high performance concrete10.1016/j.conbuildmat.2019.117083 ↗
20. Early-age behaviour and cracking potential of fly ash concrete under restrained condition10.1680/jmacr.18.00106 ↗
21. Influence of barchip fibers on early-age cracking potential of high performance concrete under restrained condition10.1016/j.conbuildmat.2018.07.121 ↗
22. Influence of ground granulated blast furnace slag on cracking potential of high performance concrete at early age10.1016/j.conbuildmat.2019.117839 ↗
23. Mechanical properties of high strength concrete reinforced with metallic and non-metallic fibres10.1016/j.cemconcomp.2007.03.006 ↗
24. Development of high strength flowable mortar with hybrid fibre10.1016/j.conbuildmat.2009.11.013 ↗
25. Workability of hybrid fibre reinforced self-compacting concrete10.1016/j.buildenv.2004.12.014 ↗
26. An experimental study on mechanical properties of hpp fiber reinforced concrete (barchip fibers)
27. Influence of fibers on drying shrinkage in restrained concrete10.1016/j.conbuildmat.2017.05.093 ↗
28. Shrinkage of polypropylene fiber-reinforced high-performance concrete10.1061/(ASCE)MT.1943-5533.0000258 ↗
29. Shrinkage cracking of fiber reinforced concrete
30. Steel fiber reinforced super-plasticized concretes for rehabilitation of bridge decks and highway pavements
31. Alternative reinforcing materials for developing countries
32. Fracture toughness of fiber reinforced concrete
33. Design of hybrid-fiber reinforcement for shrinkage cracking by crack width predictions
34. Creep, shrinkage, and cracking of restrained concrete at early age
35. Mechanical properties of high strength flowing concrete with hybrid fibers10.1016/j.conbuildmat.2011.08.057 ↗
36. Durability investigation of barchip fiber-reinforced concrete lining of water supply tunnels
37. Fibrous ferrocement composite with PVC-coated weld mesh and bar-chip polyolefin fibers
38. Mechanical behaviors of concrete combined with steel and synthetic macro-fibers10.12989/cac.2007.4.3.207 ↗
39. Application of high performance polypropylene fibers in concrete lining of water tunnels10.1016/j.matdes.2013.09.075 ↗
40. Influence of Barchip fiber length on early-age behavior and cracking resistance of concrete internally cured with super absorbent polymers10.1016/j.conbuildmat.2019.03.209 ↗
41. Combined Non-Destructive Testing (NDT) method for the evaluation of the mechanical characteristics of Ultra High Performance Fibre Reinforced Concrete (UHPFRC)10.1016/j.conbuildmat.2016.11.068 ↗
42. Prediction model for Ultrasonic Pulse Velocity (UPV) in polypropylene fiber reinforced concrete containing slag
43. Post-crack (or post-peak) flexural response and toughness of fiber reinforced concrete after exposure to high temperature10.1016/j.conbuildmat.2010.04.003 ↗
44. Enhancement of mechanical properties in polypropylene– and nylon–fibre reinforced oil palm shell concrete10.1016/j.matdes.2013.02.070 ↗
45. Laboratory study on the effect of polypropylene fiber on durability, and physical and mechanical characteristic of concrete for application in sleepers10.1016/j.conbuildmat.2013.02.076 ↗
46. Estimation of compressive strength of self-compacted concrete with fibers consisting nano-SiO2 using ultrasonic pulse velocity10.1016/j.conbuildmat.2013.03.082 ↗
47. Characterization of natural fibre-reinforced composites with advanced ultrasonic techniques
48. Mechanical behavior of self-compacting concrete pavements incorporating recycled tire rubber crumb and reinforced with polypropylene fiber10.1016/j.jclepro.2016.04.079 ↗
49. Evaluating mechanical properties of macro-synthetic fiber-reinforced concrete with various types and contents10.1007/s11223-017-9907-z ↗
50. Durability of high strength flowing concrete with hybrid fibres10.1016/j.conbuildmat.2012.04.085 ↗
51. Investigation on mechanical properties and microstructure of high performance polypropylene fiber reinforced lightweight aggregate concrete10.1016/j.conbuildmat.2016.04.116 ↗
52. Flexural toughness characteristics of steel–polypropylene hybrid fibre-reinforced oil palm shell concrete10.1016/j.matdes.2014.01.004 ↗
53. Autogenous shrinkage of concrete containing granulated blast-furnace slag10.1016/j.cemconres.2006.01.005 ↗
54. The influence of chemical admixtures on the autogenous shrinkage ultra-high performance concrete10.4028/www.scientific.net/KEM.452-453.725 ↗
55. Early age setting, shrinkage and tensile characteristics of ultra high performance fiber reinforced concrete10.1016/j.conbuildmat.2012.12.015 ↗
56. Application of non-corrosive Barchip fibres for high strength concrete enhancements in aggressive environments10.1016/j.compositesb.2013.04.012 ↗
57. ASTM/C150M–19a, Standard Specification for Portland Cement, ASTM International, West Conshohocken, PA, 2019.
58. CS (Chinese Standard) GB 175-2007/XG3-2018. Common Portland Cement, Quality Supervision Inspection and Quarantine of the People’s Republic of China and Standardization Administration of the People’s Republic China, China, 2018 (in Chinese).
59. CS (Chinese Standard) GB/T 50082-2009. Test Methods of Long-Term Performance and Durability of Ordinary Concrete, Ministry of Construction, China, 2009 (in Chinese).
60. Improving test method to measure early age autogenous shrinkage in concrete based on air cooling
61. Autogenous shrinkage of high performance concrete containing mineral admixtures under different curing temperatures10.1016/j.conbuildmat.2014.03.023 ↗
62. Assessment of early-age autogenous shrinkage strains in concrete using bentonite clay as internal curing technique10.1016/j.conbuildmat.2014.05.051 ↗
63. Effect of internal curing with super absorbent polymers on autogenous shrinkage of concrete at early age10.1016/j.conbuildmat.2015.12.115 ↗
64. Monitoring of concrete structures using the ultrasonic pulse velocity method10.1088/0964-1726/24/11/113001 ↗
65. CS (Chinese Standard) GB/T 50081-2019, Standard for Test Methods of Concrete Physical and Mechanical Properties, Ministry of Construction of the People’s Republic of China and State Administration for Market Regulation, China, 2019 (in Chinese).
66. Properties of cracking resistance of cemfiber reinforced concrete10.4028/www.scientific.net/KEM.280-283.1765 ↗
67. Effect of polypropylene fibers on shrinkage and cracking of concretes10.1617/s11527-008-9361-2 ↗
68. Autogenous shrinkage of ground-granulated blast-furnace slag concrete
69. Influence of ground granulated blast furnace slag on the early-age anti-cracking property of internally cured concrete10.1016/j.conbuildmat.2019.06.149 ↗
70. Simulation analysis on hydration kinetics and microstructure development of tricalcium silicate considering dissolution mechanisms10.1016/j.conbuildmat.2020.118535 ↗
71. Effect of autogenous deformation on the cracking risk of slag cement concretes10.1016/j.cemconcomp.2010.12.003 ↗
72. Effect of temperature rising inhibitor on autogenous shrinkage of cement pastes10.1016/j.conbuildmat.2019.06.044 ↗
73. Shrinkage cracking-can it be prevented
74. Influence of polypropylene fiber geometry on plastic shrinkage cracking in concrete10.1016/j.cemconres.2006.01.010 ↗
75. Prediction model for shrinkage of concrete including autogenous shrinkage. Creep, shrinkage and durability mechanics of concrete and other quasi-brittle materials
76. Carbon and steel microfiber-reinforced cement-based composites for thin repairs10.1061/(ASCE)0899-1561(1994)6:1(88) ↗
77. Addition of pre-wetted lightweight aggregate and steel/polypropylene fibers in high-performance concrete to mitigate autogenous shrinkage
78. Analyses and models of the autogenous shrinkage of hardening cement paste10.1016/0008-8846(95)00140-8 ↗
79. Comité Euro-International Du Béton (CEB), CEB-FIP Model Code For Concrete Structures, Lausanne, Switzerland, 2013.
80. CEN. Eurocode 2: Design of concrete structures: Part 1-1: General rules and rules for buildings. CEN. 2001, 230p, Brussels.