Abstract
Abstract In order to obtain the drying control condition with no or minimal effect on concrete strength, various drying temperatures conditions are used as 150 °C, 120 °C, 105 °C, 85 °C and 60 °C, and the drying procedure of continuous and intermittent cyclic are presented independently in this study. The change of specimen mass is recorded in the drying process, and the compressive strength and splitting tensile strength are measured after the natural cooling. The results show that the concrete compressive strength initially decreases and then increases with the increase in drying temperature, while the splitting tensile strength always decreases. The relative compressive and splitting tensile strength of concrete in dry state are 1 and 0.99 respectively after 115.5 h of continuous drying at 105 °C, which denotes the optimal drying control condition has minimal effect on the strength, and efficiency is suitable. Finally, the change in components and defects structure of the concrete after minimal damage drying is analyzed through the thermo-gravimetric analysis, electron microscope scanning and industrial CT scanning.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fire effects on concrete materials · Concrete and Cement Materials Research · Concrete Properties and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Strain-rate effect on the tensile behavior of concrete at different relative humidity levels10.1007/BF02482196 ↗
2. Effect of moisture condition on concrete core strengths
3. Influence of cracking in presence of free water on the mechanical behavior of concrete10.1680/macr.1991.43.154.53 ↗
4. Influence of free water in concrete on the cracking process10.1680/macr.1990.42.152.143 ↗
5. Moisture and strain rate effects on concrete strength
6. Experimental study on fracture toughness of concrete with different moisture contents
7. Influence of free water on dynamic behavior of dam concrete under biaxial compression10.1016/j.conbuildmat.2016.02.090 ↗
8. Experiments of the compressive properties of dry and saturated concrete under different loading rates
9. Experiments on saturated concrete under different splitting tensile rate and mechanism on strength change
10. Effect of moisture content on static compressive elasticity modulus of concrete
11. Moisture effect on compressive behavior of concrete under dynamic loading10.1007/s11771-014-2481-7 ↗
12. Influence of free water content on the compressive mechanical behaviour of cement mortar under high strain rate10.1007/s12046-011-0024-6 ↗
13. Integrity of CFRP-concrete bond subjected to long-term cyclic temperature and mechanical stress10.1016/j.compstruct.2016.04.040 ↗
14. Mechanical properties of high performance self-compacting concretes at room and high temperature10.1016/j.conbuildmat.2016.02.132 ↗
15. Effects of high temperature on the residual compressive strength of high-strength siliceous concretes
16. Recycled concrete made with different natural coarse aggregates exposed to high temperature10.1016/j.conbuildmat.2008.08.017 ↗
17. Influence of temperature, cement type and level of concrete consolidation on chloride ingress in conventional and high-strength concretes10.1016/S0950-0618(97)00004-4 ↗
18. The people’s republic of China industry standard SL 352-2006, Test Code for Hydraulic Concrete.
19. Calcium silicate hydrate from dry to saturated state: structure dynamics and mechanical properties10.1016/j.actamat.2013.12.016 ↗
20. A model for the microstructure of calcium silicate hydrate in cement paste10.1016/S0008-8846(99)00209-4 ↗
21. Thermodynamics of water confined in porous calcium-silicate-hydrates10.1021/la301738p ↗
22. Reactive molecular simulation on water confined in the nanopores of the calcium silicate hydrate gel: structure, reactivity, and mechanical properties10.1021/jp509292q ↗
23. Effects of elevated temperature on the structure and properties of calcium–silicate–hydrate gels: the role of confined water10.1039/c3sm50975c ↗
24. Confined water dissociation in disordered silicates nanometer-channels at elevated temperatures: mechanism, dynamics and impact on the substrates10.1021/acs.langmuir.6b00444 ↗
25. Dynamical behaviors of structural, constrained and free water in calcium- and magnesium-silicate-hydrate gels10.1016/j.jcis.2016.01.071 ↗
26. About microcracking due to leaching in cementitious composites: X-ray microtomography description and numerical approach10.1016/j.cemconres.2009.09.021 ↗
27. 3D experimental investigation of the microstructure of cement pastes using synchrotron X-ray microtomography (μCT)10.1016/j.cemconres.2006.10.012 ↗
28. Concrete at high temperatures — a general review10.1016/0379-7112(88)90033-1 ↗
29. Mechanical properties of geopolymer concrete containing polyvinyl alcohol fiber exposed to high temperature10.1016/j.conbuildmat.2016.09.001 ↗
30. Evaluation of microstructural and microchemical aspects of high density concrete exposed to sustained elevated temperature10.1016/j.conbuildmat.2016.09.053 ↗