Investigation of the acid and sulfate resistance performances of hydrogen-rich water based mortars
Source abstract
Abstract
Abstract The present article illustrates the acid and sulfate resistance performance of control (CM) and the hydrogen-rich water-based mortar (HM) samples. The 28 days cured CM and HM samples were exposed to 5% HCl, 5% HNO3, and 5% sodium sulfate solutions for 30, 60, 90, 120, 150, and 180 days to evaluate their acid and sulfate resistance performances. The impact of acid and sulfate attack was evaluated measuring the weight and compressive strength loss of mortar samples in the different exposure regimes. Additionally, water absorption, porosity, and sorptivity tests were performed to evaluate the transport properties of the mortars. Analyzing the result, a lesser extent of compressive strength loss (47.63% in HCl, 39.47% in HNO3, and 3% in Na2SO4) was observed for the hydrogen-rich water-based mortar as compared to that of the control mortar (57.33% in HCl, 55.4% in HNO3, and 14% in Na2SO4) after 180 days exposure. Based on the X-ray diffraction, Fourier transform infrared spectroscopy, and scanning electron microscopy analysis, a plausible mechanism has been proposed to explain the beneficial effect of the hydrogen-rich water-based mortars against acid and sulfate attacks.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Mehta · 2006
2. 2013
3. Influence of various acids on the physico-mechanical properties of pozzolanic cement mortars10.1007/s12046-007-0048-0 ↗
4. Microstructural study of sulfate attack on ordinary and limestone Portland cements at ambient temperature10.1016/S0008-8846(02)00914-6 ↗
5. Use of barium carbonate to inhibit sulfate attack in cements10.1016/j.cemconres.2014.12.006 ↗
6. Durability of the hydrated limestone-silica fume Portland10.1016/S0008-8846(99)00049-6 ↗
7. High durability cementitious material with mineral admixtures and carbonation curing10.1016/j.wasman.2006.01.030 ↗
8. Chemical admixtures — chemistry, applications and their impact on concrete microstructure and durability10.1016/j.cemconres.2015.05.016 ↗
9. Aïtcin · 2016
10. Mechanical and durability properties of cement mortar with Algerian pozzolana10.1007/s10853-006-0227-0 ↗
11. Cement mixtures containing copper tailings as an additive: durability properties10.1590/S1516-14392012005000129 ↗
12. Studies on blended cements containing a high volume ofnatural pozzolans10.1016/S0008-8846(03)00173-X ↗
13. Durability of mortars modified with metakaolin10.1016/S0008-8846(03)00090-5 ↗
14. Use of waste brick as a partial replacement of cement in mortar10.1016/j.wasman.2009.03.026 ↗
15. The sulphate resistance of cements containing red brick dust and ground basaltic pumice with sub-microscopic evidence of intra-pore gypsum and ettringite as strengtheners10.1016/j.cemconcomp.2011.10.001 ↗
16. Durability characteristics of steel fibre reinforced geopolymer concrete10.1016/j.conbuildmat.2015.06.014 ↗
17. Compressive strength and durability properties of high volume fly ash (HVFA) concretes containing ultrafine fly ash (UFFA)10.1016/j.conbuildmat.2015.02.068 ↗
18. Mailvaganam · 1999
19. Multi-functional organic corrosion inhibitor10.1016/S0958-9465(03)00039-8 ↗
20. Kerkhoff · 2007
21. Hydrogen-rich water revealed benefits in controlling the physical and mechanical performances of cement mortar10.1016/j.conbuildmat.2015.09.014 ↗
22. ASTM C150/C150M-16 · 2016
23. ASTM C305-14 · 2014
24. ASTM C642-13 · 2013
25. ASTM C267-01 · 2001
26. ASTM C109/C109M-16a · 2016
27. Acidic attack of cement based materials: a review. Part 1. Principle of acidic attack10.1016/S0950-0618(01)00012-5 ↗
28. M. Alexander, A. Bertron, N. De Belie, Performance of cement-based materials in aggressive aqueous environments, Springer 2013, pp. 102–104.10.1007/978-94-007-5413-3 ↗
29. An X-ray diffraction, fourier- transform infrared spectroscopy and scanning electron microscopy/ energy-dispersive spectroscopic investigation of the effect of sodium lignosulfonate superplasticizer on the hydration of portland cement type V10.1080/03602559909351619 ↗
30. P.E. Stutzman, Guide for X-ray powder diffraction analysis of Portland cement and clinker, US Department of Commerce, Technology Administration, National Institute of Standards and Technology, Office of Applied Economics, Building and Fire Research Laboratory, 1996.
31. Pozzolana and pozzolanic cement
32. Dry-grinded ultrafine cements hydration: physicochemical and microstructural characterization10.1590/S1516-14392013005000014 ↗
33. Effect of some chemical admixtures on physico-chemical and rheological properties of oil well cement pastes10.1016/j.conbuildmat.2016.05.044 ↗
34. Comparative study of the characteristics of nano silica, silica fume– and fly ash–incorporated cement mortars10.1590/S1516-14392014005000054 ↗
35. Cement mixtures containing copper tailings as an additive: durability properties10.1590/S1516-14392012005000129 ↗
36. Study physico-chemical properties of blended cements containing fixed amount of silica fume, blast furnace slag, basalt and limestone, a comparative study10.1016/j.conbuildmat.2014.08.071 ↗
37. A.S. Benosman, M. Mouli, H. Taibi, M. Belbachir, Y. Senhadji, I. Bahlouli, D. Houivet, Studies on chemical resistance of PET-mortar composites: microstructure and phase composition changes, (2013).10.4236/eng.2013.54049 ↗
38. Infrared spectra and characteristic frequencies of inorganic ions10.1021/ac60068a007 ↗
39. Durability assessment of high-performance concrete with SRAs and FLWAs10.1016/j.cemconcomp.2014.12.004 ↗
40. Acidic attack of cement based materials under the common action of high, ambient temperature and pressure10.1016/j.conbuildmat.2012.04.025 ↗
41. Hydration mechanism of the hydrogen-rich water based cement paste10.1021/acs.jpcc.6b01444 ↗
42. Effect of pH on the hydration of tricalcium silicate10.1111/j.1151-2916.1993.tb03691.x ↗
43. On the hydration of Portland cement