Performance and microstructure of bricks with protective coatings subjected to salt weathering
Source abstract
Abstract
Abstract Salt crystallization is the crucial damaging mechanism which affects the durability of porous masonry units like bricks. Improper selection of protective treatments and replacement strategies often degrade the situation further and result in frequent future interventions. In this paper, the role of pore size distribution of the bricks in resisting salt crystallization and its effect on the performance of protective coatings has been discussed. Bricks with different microstructural properties were treated with common water repellent coatings - silicone-based and acrylic siloxane-based and were subjected to accelerated salt weathering tests. The performance of the coatings was studied using standard methods, and the coatings were then evaluated for their compatibility with various bricks with varying microporosity, when exposed to sodium sulphate. Bricks highly prone to salt crystallization have been found to be more sensitive to the properties of treatments over them, as breathability assumes a greater significance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Building materials and conservation · Concrete and Cement Materials Research · Hygrothermal properties of building materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. A polydimethylsiloxane coating to minimize weathering effects on granite10.1016/j.conbuildmat.2016.08.146 ↗
2. The pore system of sedimentary rocks as a key factor in the durability of building materials10.1016/j.enggeo.2011.01.008 ↗
3. Salt damage in porous materials: how high supersaturations are generated10.1016/S0022-0248(02)01429-X ↗
4. Predicting salt damage in practice: a theoretical insight into laboratory tests
5. Chemo-mechanics of salt damage in stone10.1038/ncomms5823 ↗
6. Crystal growth in porous materials - II: influence of crystal size on the crystallization pressure10.1016/j.jcrysgro.2005.05.008 ↗
7. Crystal growth in porous materials - I: the crystallization pressure of large crystals10.1016/j.jcrysgro.2005.05.007 ↗
8. Factors affecting crystallization pressure10.1617/2912143802.009 ↗
9. Experimente zur Messung und erklarung der sogenannten Kristallisationskraft
10. Neugebauer · Geol. Palaontologie Abh. · 1973 · 143 · 22310.1127/njgpa/143/1973/223 ↗
11. Xie · Cement Concr. Res. · 1992 · 22 · 63110.1016/0008-8846(92)90015-N ↗
12. The thermodynamics of frost damages to porous solids10.1039/tf9615701541 ↗
13. S.A. Russell, Stone preservation committee report. Appendix 1. H.M. Stationary Office, London, 1927.
14. Crystallization damage by sodium sulfate10.1016/S1296-2074(03)00022-0 ↗
15. A critical discussion of salt weathering laboratory tests for assessment of petrological features susceptibility10.1016/j.proeps.2016.12.082 ↗
16. How does sodium sulfate crystallize? Implications for the decay and testing of building materials10.1016/S0008-8846(00)00381-1 ↗
17. Salt weathering: influence of evaporation rate, supersaturation and crystallization pattern10.1002/(SICI)1096-9837(199903)24:3<191::AID-ESP942>3.0.CO;2-G ↗
18. Role of pore structure in salt crystallisation in unsaturated porous stone10.1016/j.jcrysgro.2003.09.004 ↗
19. Coatings on brick masonry: are they protective or can they enhance deterioration?10.1179/019713607806112387 ↗
20. Testing the effectiveness of protective coatings on traditional bricks10.1016/j.conbuildmat.2016.02.114 ↗
21. RILEM · 1980 · 175
22. Modification of the porous network by salt crystallization in experimentally weathered sedimentary stones10.1617/s11527-007-9308-z ↗
23. S.D. Rani, M. Deb, M. Santhanam, R. Gettu, Evaluation of repair mortar materials for old monuments in southern India, 2016, pp. 631–635.
24. Indian Standard, Common Burnt Clay Building Bricks- Specification, 1992, 1997.
25. Durability Index Testing Procedure Manual, 2018, 2018.
26. Use of TEOS for fired-clay bricks consolidation10.1617/s11527-013-0120-7 ↗
27. Experimental study on the salt weathering resistance of fired clay bricks consolidated by ethyl silicate10.1617/s11527-015-0665-8 ↗
28. Influence of mineralogy and firing temperature on the porosity of bricks10.1016/S0955-2219(03)00249-8 ↗
29. China’s brick history and conservation: laboratory results of Shanghai samples from 19th to 20th century10.1016/j.conbuildmat.2017.06.094 ↗
30. Bricks in historical buildings of Toledo City: characterisation and restoration10.1016/S1044-5803(03)00101-3 ↗
31. Mineralogical changes during firing of calcium-rich brick clays
32. Influence of firing temperature and mineralogical composition on bending strength and porosity of ceramic tile bodies10.1016/j.clay.2008.01.005 ↗
33. Stress from crystallization of salt10.1016/j.cemconres.2003.12.034 ↗
34. Towards a more effective and reliable salt crystallization test for porous building materials: state of the art10.1617/s11527-018-1180-5 ↗
35. K. Scrivener, R. Snellings, B. Lothenbach, A Practical Guide to Microstructural Analysis of Cementitious Materials, First Spon Press, BocaRaton, 2016, https://doi.org/10.7693/wl20150205.