journal article·2017-07Open access

Artificial ageing of glass with sand abrasion

Kyriaki Corinna Datsiou, Mauro Overend

Abstract

The strength of glass is governed by the condition of its surface which deteriorates progressively as surface flaws accumulate on exposure to weathering action during its service life. Therefore, knowledge of the strength of naturally aged glass is crucial in order to ensure its safe use in load-bearing applications. Artificial ageing tests can be very useful in this regard, but they have traditionally focused on degradation in light transmittance properties rather than the strength of glass. Experimental testing has been undertaken in this study to investigate the effectiveness of a falling abrasive method for the artificial ageing of glass. Abrasive medium is allowed to fall freely on monolithic glass and induce a random surface flaw population. 390 annealed glass specimens grouped in 26 series were artificially aged using different combinations of ageing parameters. The specimens were subsequently subjected to destructive and non-destructive testing to determine the influence of each ageing parameter and to establish a combination that produces strength characteristics similar to those of naturally aged glass. Existing artificial ageing recommendations were found to significantly overestimate design strengths by up to 253% at low probabilities of failure, Pf = 0.008 and are therefore, deemed unsafe. However, it was found that the falling abrasive method using a different combination of ageing parameters provides good correlation to the strength of naturally aged glass.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Structural Analysis of Composite Materials · Building materials and conservation · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Haldimann · 2008
2. K. Zammit, M. Overend, Increasing the design strength of glass - fractography and stress testing, in: International Association for Shell and Spatial Structures (IASS) Symposium, 2009.
3. The effectiveness of resin-based repairs on the inert strength recovery of glass10.1016/j.conbuildmat.2015.03.072 ↗
4. Strength of weathered window glass
5. Fink · 2000
6. Abiassi · 1981
7. Glass Failure Prediction Model10.1061/(ASCE)0733-9445(1984)110:2(197) ↗
8. Experimental study of weathered tempered glass plates from the Northeastern United States10.1061/(ASCE)AE.1943-5568.0000220 ↗
9. Durability of SG-laminated reinforced glass beams: effects of temperature, thermal cycling, humidity and load-duration10.1016/j.conbuildmat.2011.07.046 ↗
10. Weathering action on thermo-viscoelastic properties of polymer interlayers for laminated glass10.1016/j.conbuildmat.2015.08.010 ↗
11. Time-dependent behavior of laminated glass10.1061/(ASCE)MT.1943-5533.0000032 ↗
12. Time and temperature dependent mechanical behaviour and durability of laminated safety glass
13. Postbreakage behavior of heat strengthened laminated glass under wind effect10.1061/(ASCE)0733-9445(1993)119:2(454) ↗
14. C. Völker, D. Philipp, M. Masche, and T. Kaltenbach, “Development of a test method for the investigation of the abrasive effect of sand particles on components of solar energy systems”, in 29th European PV Solar Energy Conference and Exhibition, 2014, pp. 22–26.
15. Mechanical strength of soda-lime glass sandblasted by gravitation10.1007/s40544-015-0075-5 ↗
16. S. Benbahouche, F. Roumili, R. Zegadi, Mechanical strength of tempered soda – lime – silica glass damaged by sand gravitation determined by bending with circular supports, in: XIX International Congress on Glass, 2001, pp. 286–289.
17. N. Protopopescu, Sand Trickling Abrasion Testing of Float Glass. Some Methodological and Experimental Considerations, in: Glass Processing Days, 2001, pp. 261–265.
18. K. C. Datsiou and M. Overend, Evaluation of Artificial Ageing Methods for Glass, in: Proc. Challenging Glass 5, 2016, pp. 581–591.
19. Study of light scattering on a soda lime glass eroded by sandblasting10.1016/j.jeurceramsoc.2007.01.011 ↗
20. Effect of impact angle on glass surfaces eroded by sand blasting10.1016/S0955-2219(99)00140-5 ↗
21. Effect of annealing and chemical strengthening on soda lime glass erosion wear by sand blasting10.1016/S0955-2219(02)00169-3 ↗
22. Transitions in the erosive wear behaviour of a glass ceramic10.1016/0043-1648(91)90367-4 ↗
23. Characterisation of the scratch resistance of annealed and tempered architectural glass10.1016/j.tsf.2011.04.104 ↗
24. J. Schneider, H. Techen, and R. Stengler, “Determination of the scratch resistance of annealed and tempered glasses by using UST (Universal Surface Tester)”, 53rd Int. Wissenschaftliches Kolloquium, no. Technische Universität Ilmenau, 2008.
25. Y. Rodichev, Y. Yevplov, H. Soroka, F. Veer, Surface Cracked Layer and Damage Resistance of Glass under Contact Loading, in: Proc. Challenging Glass 3, 2012.10.3233/978-1-61499-061-1-523 ↗
26. Surface damage of soda – lime – silica glasses : indentation scratch behavior10.1016/S0022-3093(02)01937-3 ↗
27. Schula · 2014
28. DIN 52348; Deutsches Institut Fur Normung, Standard for Testing of Glass and Plastics; Abrasion Test; Sand Trickling Method., www.din.de, 1985.
29. ASTM D968–05, Standard Test Methods for Abrasion Resistance of Organic Coatings by Falling Abrasive, ASTM Int. West Conshohocken; PA; 2010; DOI 10.1520/D0968-05R10; www.astm.org.
30. GlasStress Ltd, Scattered Light Polariscope SCALP Instruction Manual, ver. 5.5.
31. Biaxial flexure strength and dynamic fatigue of soda – lime – silica float glass10.1111/j.1151-2916.2002.tb00352.x ↗
32. ASTM C1499–03, Standard Test Method for Monotonic Equibiaxial Flexural Strength of Advanced Ceramics at Ambient Temperature, ASTM Int. West Conshohocken; PA; 2010; 2009, DOI 10.1520/C1499-09; www.astm.org.
33. Quinn · 2007
34. Abaqus 6.12 Documentation, Analysis User’s Manual. SIMULIA, 2012.
35. Reliability analysis of window glass failure pressure data10.1016/0167-4730(91)90026-6 ↗
36. B. Bergman, Estimation of Weibull Parameters By Using a Weight Function, 1986, vol. 5, pp. 611–614.10.1007/BF01731525 ↗
37. On the determination of Weibull parameters10.1007/BF00722337 ↗
38. Liu · 1997
39. Weibull statistics for glass strength
40. EN 12603, Glass in building — Procedures for goodness of fit and confidence intervals for Weibull distributed glass strength data, CEN Eur. Comm. Stand., 2002.
41. ASTM E1300–12a, Standard Practice for Determining Load Resistance of Glass in Buildings, ASTM Int. West Conshohocken; PA; 2010; 2012, DOI 10.1520/E1300-12A; www.astm.org, pp. 1–59.
42. Mil-Prf-13830B, Optical components for fire control instruments; General specification governing the manufacture, assembly and inspection of, U.S. Mil. Perform. Specif., 1997.
43. Fatigue limit and crack arrest in alkali-containing silicate glasses10.1007/BF02403942 ↗
44. Quantification of residual stress from photonic signatures of fused silica10.1063/1.4865025 ↗
45. F. Veer and Y. Rodichev, Corrosion effects on soda lime glass, in: Proc. Challenging Glass 2, 2010.
46. Abernethy · 2006