Abstract This study investigated the effects of mixture proportion and curing condition on the mechanical and shrinkage behaviors of high-performance fiber-reinforced cementitious composites (HPFRCCs). Different water-to-binder (W/B) ratios and amounts of mineral admixtures, such as zirconium silica fume (Zr SF) and blast furnace slag were evaluated. The test results indicate that initial steam-heat curing accelerated the strength development and was sufficient to develop its full strength. The ultimate autogenous shrinkage was insignificantly affected by the curing conditions, but the heat curing accelerated the development of autogenous shrinkage. HPFRCC with a lower W/B ratio and greater amount of Zr SF exhibited higher autogenous shrinkage but lower drying shrinkage. In addition, the amount of total shrinkage of HPFRCC was more effectively reduced by providing heat curing when a higher W/B ratio and a smaller amount of Zr SF were used. There were no increases in the autogenous and drying shrinkage for HPFRCC immediately after finishing the initial heat curing, meaning that there is no possibility of shrinkage cracks forming in HPFRCC elements after the heat curing process. Finally, the autogenous shrinkage behaviors of HPFRCC were simulated with several prediction models from literature and an optimized model, considering equivalent age, was suggested.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Innovative concrete reinforcement materials · Concrete and Cement Materials Research · Concrete Properties and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Composition of reactive powder concretes10.1016/0008-8846(95)00144-2 ↗
2. Tensile strain-hardening FRC composites: Historical evolution since the
3. Slurry infiltrated fiber concrete (SIFCON): Properties and applications
4. Conditions for pseudo strain-hardening in fiber reinforced brittle matrix composites10.1115/1.3119767 ↗
5. Slurry infiltrated mat concrete (SIMCON)
6. Tensile strain-hardening behavior of polyvinyl alcohol engineered cementitious composite (PVA-ECC)
7. Engineered steel fibers with optimal properties for reinforcement of cement composites10.3151/jact.1.241 ↗
8. Shrinkage and cracking of restrained ultra-high-performance fiber-reinforced concrete slabs at early age10.1016/j.conbuildmat.2014.09.097 ↗
9. Shrinkage properties of ultra-high performance concrete (UHPC)10.1166/asl.2011.1505 ↗
10. Effect of drying conditions on autogenous shrinkage in ultra-high performance concrete at early-age10.1617/s11527-010-9670-0 ↗
11. Comparative shrinkage behavior of ultra-high-performance fiber-reinforced concrete under ambient and heat curing conditions10.1016/j.conbuildmat.2017.12.029 ↗
12. Early age compressive stress-strain properties of low-, medium, and high-strength concretes
13. Compressive behavior of ultra-high-performance fiber-reinforced concrete
14. ASTM C1611/C1611M · 2014
15. Effectiveness of shrinkage-reducing admixture in reducing autogenous shrinkage stress of ultra-high-performance fiber-reinforced concrete10.1016/j.cemconcomp.2015.09.005 ↗
16. Mechanical behavior of UHPC (Ultra High Performance Concrete) according to hybrid use of steel fibers10.4028/www.scientific.net/AMR.287-290.453 ↗
17. Demystifying autogenous shrinkage
18. ASTM C157 · 2014
19. ASTM C39 · 2014
20. Material and bond properties of ultra high performance fiber reinforced concrete with micro steel fibers10.1016/j.compositesb.2013.10.081 ↗
21. RILEM TC162-TDF: test and design methods for steel fibre reinforced concrete: design of steel fibre reinforced concrete using the σ-w method: principles and applications10.1617/13837 ↗
22. Flexural response of steel-fiber-reinforced concrete beams: effects of strength, fiber content, and strain-rate10.1016/j.cemconcomp.2015.10.001 ↗
23. NMR, XRD, IR and synchrotron NEXAFS spectroscopic studies of OPC and OPC/slag cement paste hydrates10.1617/s11527-011-9737-6 ↗
24. Mechanisms of delayed ettringite formation in Portland cement systems
25. Influence of curing regime and steel fibres on the mechanical properties of UHPC10.1680/macr.14.00333 ↗
26. S. Granger, A. Loukili, G. Pijaudier-Cabot, G. Chanvillard, Mechanical characterization of the self-healing effect of cracks in Ultra High Performance Concrete (UHPC), in: Proceedings Third International Conference on Construction Materials, Performance, Innovations and Structural Implications, 2005, pp. 22–24.
27. Japan Concrete Institute, Committee report, Autogenous shrinkage of concrete, E. Tazawa (Eds.), E&FN Spon, 1999.
28. Influence of reinforcing bar type on autogenous shrinkage stress and bond behavior of ultra high performance fiber reinforced concrete10.1016/j.cemconcomp.2013.11.014 ↗
29. Autogenous shrinkage and induced restraining stresses in high-strength concretes10.1016/S0008-8846(00)00399-9 ↗
30. Influence of cement and admixture on autogenous shrinkage of cement paste10.1016/0008-8846(95)00010-0 ↗
31. Self-desiccation and its importance in concrete technology10.1007/BF02486354 ↗
32. Analyses and models of the autogenous shrinkage of hardening cement paste: I. Modelling at macroscopic scale10.1016/0008-8846(95)00140-8 ↗
33. The relationship between autogenous shrinkage and pore structure of cement paste with mineral admixtures10.1016/j.conbuildmat.2010.04.018 ↗
34. Hydration and microstructure of ultra high performance concrete incorporating rice husk ash10.1016/j.cemconres.2011.06.009 ↗
35. Pore structure of concrete with mineral admixtures and its effect on self-desiccation shrinkage
36. Mehta · 2006
37. Assessing drying shrinkage and water permeability of reactive powder concrete produced in Hong Kong10.1016/j.conbuildmat.2011.05.006 ↗
38. Effect of water-to-cementitious materials ratio and silica fume on the autogenous shrinkage of concrete10.1016/S0008-8846(03)00149-2 ↗
39. Strength development and drying shrinkage of high-strength concretes10.1016/0958-9465(96)00024-8 ↗
40. ASTM C1074 · 2011
41. NRMCA, CIP 39–Maturity Methods to Estimate Concrete Strength. National Ready Mix Concrete Association, 2006.
42. CEB-FIP · Structural Concrete: Textbook on Behavior, Design and Performance · 1999 · vol. 1 · 43
43. EN-1992, Eurocode 2: Design of Concrete Structures: Part 1–1: General Rules and Rules for Buildings, Brussels, 2001, pp. 230.
44. J. Jonasson, H. Hedlund, An engineering model for creep and shrinkage in high performance concrete, in: Proceedings of the International RILEM Workshop on Shrinkage of Concrete, Shrinkage, RILEM, Paris, Bagneux, France, 2000, pp.173–178.
45. E. Tazawa, S. Miyazawa, Effect of constituents and curing condition on autogenous shrinkage of concrete. in: E. Tazawa (Ed.), Proceedings of International Workshop, Autogenous Shrinkage of Concrete, Hiroshima, Japan, E & FN Spon, 1998, pp. 269–280.10.1201/9781482272123 ↗
46. Creep and shrinkage of high-performance concrete
47. Autogenous shrinkage of concrete containing granulated blast-furnace slag10.1016/j.cemconres.2006.01.005 ↗
48. B.A. Graybeal, Material Property Characterization of Ultra-High Performance Concrete (No. FHWA-HRT-06-103), 2006.
49. Role of lightweight synthetic particles on the restrained shrinkage cracking behavior of mortar10.1061/(ASCE)MT.1943-5533.0000213 ↗