Pull-out creep mechanism of synthetic macro fibres under a sustained load
Source abstract
Abstract
Abstract The creep of cracked fibre reinforced concrete is still being investigated for incorporation into design guidelines. While the mechanism responsible for the time-dependent crack opening of steel fibre reinforced concrete has been associated with the fibre pull-out, a combination of pull-out creep and fibre creep have been reported for macro-synthetic fibre reinforced concrete. However, these phenomena are yet to be fully understood. In macro-synthetic fibre reinforced concrete, two possibilities exist: simultaneous occurrence of pull-out creep and fibre lengthening occurring within the matrix under sustained loading, or pull-out creep followed by fibre lengthening due to creep. This study investigates these phenomena. Single synthetic macro fibres were embedded into 50 mm cube cement-mortar samples and subjected to 50% of the average maximum pull-out load obtained from the single fibre pull-out tests. All tests were conducted in a controlled climate room. X-ray computed tomography (CT) images of samples were taken at different time intervals to assess the phenomena responsible for the increased crack widening in macro-synthetic fibre reinforced concrete. The results obtained have shown that the phenomena associated with the increased crack widening of cracked macro-synthetic fibre reinforced concrete are a simultaneous interplay of fibre pull-out and lengthening within the matrix. It is significant to note that fibre lengthening is a prominent mechanism.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Innovative concrete reinforcement materials · Concrete and Cement Materials Research · Concrete Properties and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Fibre reinforced cement-based (FRC) composites after over 40 years of development in building and civil engineering10.1016/j.compstruct.2008.03.006 ↗
2. Time-dependent pull-out behaviour of hooked-end steel fibres in concrete10.1016/j.cemconcomp.2017.02.006 ↗
3. Failure of fibre-reinforced composites by pull-out fracture10.1007/BF01117378 ↗
4. Post-cracking behaviour of steel fibre reinforced concrete10.1007/BF02480574 ↗
5. Pull-out behaviour of hooked steel fibres10.1007/BF02483148 ↗
6. Pullout behavior of steel fibers in self-compacting concrete10.1061/(ASCE)MT.1943-5533.0000001 ↗
7. Pullout behavior of steel fibers from cement-based composites10.1016/S0008-8846(97)00061-6 ↗
8. Experimental, analytical and numerical analysis of the pullout behaviour of steel fibres considering different fibre types, inclinations and concrete strengths10.1002/suco.201300058 ↗
9. Time-dependent behaviour of fibre pull-out in self-compacting concrete10.1016/j.cemconcomp.2016.12.004 ↗
10. Effect of the fiber geometry on the pullout response of mechanically deformed steel fibers10.1016/j.cemconres.2012.10.014 ↗
11. Pull-out behavior of steel fiber embedded in flowable RPC and ordinary mortar10.1016/j.conbuildmat.2014.11.037 ↗
12. Fiber-matrix bond characteristics of alkali-activated slag cement-based composites10.1061/(ASCE)MT.1943-5533.0001642 ↗
13. Performance evaluation of corrugated steel fiber in cementitious matrix10.1016/j.conbuildmat.2016.10.094 ↗
14. Predicting the pullout response of inclined hooked steel fibers10.1016/j.cemconres.2010.05.005 ↗
15. Pull-out response of macro synthetic fibre from concrete matrix: effect of loading rate and embedment length10.1016/j.conbuildmat.2016.12.160 ↗
16. Characterising the time-dependant behaviour on the single fibre level of SHCC: Part 2: the rate effects on fibre pull-out tests10.1016/j.cemconres.2009.06.006 ↗
17. Post-crack creep behavior of steel and synthetic FRC under flexural loading
18. Fracture behavior of concrete members reinforced with structural synthetic fibers10.1016/j.engfracmech.2006.01.032 ↗
19. Post-cracking behaviour of steel and macro-synthetic fibre-reinforced concretes10.1016/j.conbuildmat.2010.12.022 ↗
20. Flexural performance of fibre reinforced concrete made with steel and synthetic fibres10.1016/j.conbuildmat.2012.06.042 ↗
21. Mechanical properties of a large-scale synthetic fibre reinforced concrete ground slab10.1016/j.conbuildmat.2012.11.043 ↗
22. Fibre distribution in macro-plastic fibre reinforced concrete slab-panels10.1016/j.conbuildmat.2014.04.067 ↗
23. Effect of inclining angle, bundling and surface treatment on synthetic fibre pull-out from a cement matrix10.1016/0010-4361(90)90005-H ↗
24. Predicting the flexural postcracking performance of steel fiber reinforced concrete from the pullout of single fibers
25. Pullout behavior of polypropylene fibers from cementitious matrix10.1016/j.cemconres.2004.02.014 ↗
26. Bond characteristics of structural polypropylene fibres in concrete with regards to post-crack strength and durable design10.1108/02630800510610143 ↗
27. Bond behaviour and flexural performance of structural synthetic fibre-reinforced concrete10.1680/macr.2006.58.6.401 ↗
28. Polymeric fibers pullout behavior and microstructure as cementitious composites reinforcement10.1080/00405000.2013.773124 ↗
29. Pullout behavior of polypropylene macro-synthetic fibers treated with nano-silica10.1016/j.conbuildmat.2015.02.047 ↗
30. Tensile creep of macro-synthetic fibre reinforced concrete (MSFRC) under uni-axial tensile loading10.1016/j.cemconcomp.2014.08.002 ↗
31. Characterising the time-dependant behaviour on the single fibre level of SHCC: Part 1: mechanism of fibre pull-out creep10.1016/j.cemconres.2009.06.007 ↗
32. Short-term and creep pull-out behavior of polypropylene macrofibers at varying embedded lengths and angles from a concrete matrix10.1016/j.conbuildmat.2017.05.005 ↗
33. Quantitative X-ray tomography10.1179/1743280413Y.0000000023 ↗
34. Simple and fast porosity analysis of concrete using X-ray computed tomography10.1617/s11527-014-0519-9 ↗
35. EN12350-2 · 2000
36. EN 14889-2 · 2006
37. The effect of mixing on the performance of macro synthetic fibre reinforced concrete10.1016/j.cemconres.2017.10.010 ↗
38. EN12390-3 · 2002
39. The CT Scanner Facility at Stellenbosch University: an open access X-ray computed tomography laboratory10.1016/j.nimb.2016.08.005 ↗
40. Pull-out behaviour of polypropylene fibres from cementitious matrix10.1016/j.cemconres.2004.02.014 ↗
41. Creep of Cracked fibre reinforced shotcrete panels