Abstract
Abstract This study deals with the results of sulphate attack on concrete containing fine bone china ceramic aggregate (BCFA). Natural river sand in concrete was substituted by 0%, 20%, 40%, 60%, 80% and 100% fine bone china aggregate. The concrete specimens were submerged in 3% MgSO4 solution for 7, 28, 90 and 180 days. The influence of sulphate solution was evaluated by change in mass and change in compressive strength. Studies related to microstructure like FT-IR and XPS were carried out to monitor the influence of BCFA in sulphate resistance of concrete.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Innovative concrete reinforcement materials · Recycled Aggregate Concrete Performance · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Assessment of mechanical and durability properties of concrete containing waste rubber tire as fine aggregate10.1016/j.conbuildmat.2014.09.102 ↗
2. Properties of recycled aggregate concrete made with recycled aggregates with different amounts of old adhered mortars10.1016/j.matdes.2014.01.044 ↗
3. A comparative study on the properties of the mortar with the cathode ray tube funnel glass sand at different treatment methods10.1016/j.conbuildmat.2017.05.019 ↗
4. Mechanical properties of glass fiber reinforced ceramic concrete10.1016/j.conbuildmat.2013.10.046 ↗
5. Performance of concrete made with steel slag and waste glass10.1016/j.conbuildmat.2016.03.217 ↗
6. Effect of supplementary cementitious materials on autogenous shrinkage of ultra-high performance concrete10.1016/j.conbuildmat.2016.09.123 ↗
7. Existence of dividing strength in concrete containing recycled coarse aggregate10.1061/(ASCE)MT.1943-5533.0000864 ↗
8. Self-compacting concretes with supplementary cementitious materials: shrinkage and cracking tendency10.1061/(ASCE)MT.1943-5533.0001852 ↗
9. Characterization of concrete made with recycled aggregate from ceramic sanitary ware10.3989/mc.2011.59710 ↗
10. Using ceramic sanitary ware waste as concrete aggregate10.1016/j.conbuildmat.2013.06.063 ↗
11. Mechanical properties of structural concrete with fine recycled ceramic aggregates10.1016/j.conbuildmat.2014.04.037 ↗
12. Properties of high performance concrete made with recycled fine ceramic and coarse mixed aggregates10.1016/j.conbuildmat.2014.07.016 ↗
13. Test research on effects of ceramic polishing powder on carbonation and sulphate-corrosion resistance of concrete10.1016/j.conbuildmat.2014.01.023 ↗
14. Concrete made from ceramic industry waste: durability properties10.1016/j.conbuildmat.2010.11.049 ↗
15. Microstructure and properties of recycled concretes using ceramic sanitary ware industry waste as coarse aggregate10.1016/j.conbuildmat.2011.12.075 ↗
16. Durability of recycled concrete made with recycled ceramic sanitary ware aggregate inter-indicator relationships10.1016/j.conbuildmat.2015.12.176 ↗
17. Durability-related performance of concrete containing fine recycled aggregates from crushed bricks and sanitary ware10.1016/j.matdes.2015.11.023 ↗
18. BIS10262 · 2009
19. Reuse of sanitary ceramic wastes as coarse aggregate in eco-efficient concretes10.1016/j.cemconcomp.2011.08.015 ↗
20. Utilisation of crushed floor and wall tile wastes as aggregate in concrete production10.1016/j.jclepro.2015.07.003 ↗
21. Compressive strength and resistance to chloride penetration of mortars using ceramic waste as fine aggregate10.1016/j.conbuildmat.2011.05.008 ↗
22. Measurement methods of carbonation profiles in concrete: thermogravimetry, chemical analysis and gamma densimetry10.1016/j.cemconres.2007.04.015 ↗
23. Effect of alkalis on fresh C-S-H gels. FTIR analysis10.1016/j.cemconres.2009.01.003 ↗
24. Characterization of ceramic roof tile wastes as pozzolanic admixture10.1016/j.wasman.2008.10.019 ↗
25. A DSC study of the drying process of TEOS derived wet silica gels10.1016/S0040-6031(97)00309-2 ↗
26. Determining cement composition by Fourier transform infrared spectroscopy10.1016/1065-7355(94)00031-X ↗
27. Early hydration and setting of Portland cement monitored by IR, SEM and Vicat techniques10.1016/j.cemconres.2009.01.017 ↗
28. Application of Fourier transform infrared spectroscopy to study concrete degradation induced by biogenic sulfuric acid10.1617/s11527-015-0631-5 ↗
29. A Fourier transform infrared spectroscopic investigation of the early hydration of Portland cement and the influence of sodium lignosulfonate10.1016/S0008-8846(99)00243-4 ↗
30. Analyses of the surfaces of concrete by Raman and FT-IR spectroscopies: comparative study of hardened samples after demoulding and after organic post-treatment10.1002/sia.3548 ↗
31. The confused world of sulfate attack on concrete10.1016/j.cemconres.2004.04.004 ↗
32. Maslehuddin, Magnesium-sodium sulfate attack in plain and blended cements10.1061/(ASCE)0899-1561(1994)6:2(201) ↗
33. Means of increasing the acid resistance of porcelain and earthenware10.1007/BF01159918 ↗
34. Lateral force microscopic examination of interfacial transition zone in ceramic concrete10.1016/j.conbuildmat.2017.08.080 ↗
35. Strength and impact resistance properties of concrete containing fine bone China ceramic aggregate10.1016/j.conbuildmat.2018.02.213 ↗
36. Stability of calcium carbonate and magnesium carbonate in rainwater and nitric acid solutions10.1016/j.enconman.2006.03.021 ↗