Characteristics of volume change and heavy metal leaching in mortar specimens recycled heavyweight waste glass as fine aggregate
Source abstract
Abstract
Abstract Industrial waste, such as heavyweight waste glass, has become a global concern in terms of environmental safety and resource recycling. The reuse and recycling of heavyweight waste glass are necessary from the viewpoint of environmental protection. At the same time, concrete, three-quarters of which consists of aggregate, is one of the most widely used infrastructure materials, and it is being exhausted. The heavyweight waste glass being is considered as the most suitable substitute for aggregate due to its physical characteristics and chemical composition. In this study, to evaluate whether heavyweight waste glass could be as a concrete material, we carried out drying shrinkage, expansion by alkali-silica reaction (ASR) and heavy metal leaching of mortar. We found that when the heavyweight waste glass substitution ratio increased, the drying shrinkage decreased. Furthermore, the existing models predicted the experimental results, inversely. However, the expansion of ASR mortar gradually increased with an increase in the substitution ratio of heavyweight waste glass. When fly ash 20% or blast furnace slag 50% was mixed in mortar specimens, the ASR expansion could be controlled within the permitted limit of 0.1% at 14 days by the ASTM 1260 criteria. Moreover, the leached concentration of As, Cd, Cu and Hg from the mortar were detected below the criteria specified in drinking water regulatory levels, however, further investigation is needed to determine the leaching characteristics of Pb and Cr according to heavyweight waste glass substitution ratio in mortar specimens. Conclusively, the overall test results of this study have demonstrated that it may be feasible to utilize heavyweight waste glass as fine aggregate in mortar specimens.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Recycled Aggregate Concrete Performance · Recycling and utilization of industrial and municipal waste in materials production · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Concrete: microstructure, properties, and materials
2. Improvement of mechanical properties of recycled aggregate concrete basing on a new combination method between recycled aggregate and natural aggregate10.1016/j.conbuildmat.2017.05.084 ↗
3. Effect of cement and admixture on the utilization of recycled aggregates in concrete10.1016/j.conbuildmat.2017.04.152 ↗
4. Performance of coconut shell as coarse aggregate in concrete10.1016/j.conbuildmat.2017.02.066 ↗
5. Use of waste glass as sand in mortar: Part i – Fresh, mechanical and durability properties10.1016/j.cemconcomp.2012.08.028 ↗
6. A review on the use of waste glasses in the production of cement and concrete10.1016/j.resconrec.2007.01.013 ↗
7. A study of the effects of LCD glass sand on the properties of concrete10.1016/j.wasman.2008.03.005 ↗
8. Effects of heavy weight waste glass recycled as fine aggregate on the mechanical properties of mortar specimens10.1016/j.anucene.2016.09.035 ↗
9. Evaluation of the durability of concrete made with crushed glass aggregates10.1016/j.jclepro.2012.09.021 ↗
10. Use of recycled CRT funnel glass as fine aggregate in dry-mixed concrete paving blocks10.1016/j.jclepro.2013.12.084 ↗
11. Effect of aggregate on shrinkage of concrete and a hypothesis concerning shrinkage
12. Studies on concrete containing ground waste glass10.1016/S0008-8846(99)00213-6 ↗
13. Mechanical properties and ASR evaluation of concrete tiles with waste glass aggregate10.1016/j.scs.2015.02.005 ↗
14. The effects of lithium hydroxide solution on alkali silica reaction gels created with opal10.1016/j.cemconres.2003.10.011 ↗
15. Using lithium nitrate and pozzolanic glass powder in concrete as ASR suppressors10.1016/j.cemconcomp.2007.08.010 ↗
16. Alkali–silica reactions of mortars produced by using waste glass as fine aggregate and admixtures such as fly ash and Li2CO310.1016/j.wasman.2007.04.005 ↗
17. Production of alumino-borosilicate foamed glass body from waste LCD glass10.1016/j.jiec.2013.02.038 ↗
18. Development of a method for recycling of CRT funnel glass
19. Evaluation on the applicability of heavy weight waste glass as fine aggregate of shielding concrete
20. ASTM C 157 · 2003
21. Evaluation of accelerated test methods for determining alkali-silica reactivity of concrete aggregates10.1016/j.cemconcomp.2006.03.001 ↗
22. An accelerated method for testing the potential alkali reactivity of siliceous aggregates10.1016/0008-8846(86)90134-1 ↗
23. Evaluation of modified ASTM C 1260 accelerated mortar bar test for alkali-silica reactivity10.1016/S0008-8846(02)00903-1 ↗
24. ASTM C 1260 · 2007 · 1
25. Properties of self-compacting concrete prepared with recycled glass aggregate10.1016/j.cemconcomp.2008.12.002 ↗
26. Utilization of recycled glass derived from cathode ray tube glass as fine aggregate in cement mortar10.1016/j.jhazmat.2011.05.019 ↗
27. A study on creep and drying shrinkage of high performance concrete10.1016/S0008-8846(01)00539-7 ↗
28. Prediction of the shrinkage behavior of recycled aggregate concrete: a review10.1016/j.conbuildmat.2014.12.102 ↗
29. Eurocode 2: design of concrete structures – Part 1–1: general rules and rules for buildings
30. ACI Committee · 2008
31. CEB-FIP, C · 1991 · 51
32. Powers · Rev. Mater. Constr. · 1961 · 545 · 79
33. Studies on expansion properties in mortar containing waste glass and fibers10.1016/j.cemconres.2003.12.005 ↗
34. ASR expansion behavior of recycled glass fine aggregates in concrete10.1016/j.cemconres.2009.09.003 ↗
35. Alkali-aggregate expansion inhibiting admixtures10.1016/S0958-9465(97)00072-3 ↗
36. Use of the NBRI accelerated test to evaluate the effectiveness of mineral admixtures in preventing the alkali-silica reaction10.1016/0008-8846(87)90064-0 ↗
37. Mechanism of mineral admixture suppressing alkali-silica reaction: Part II. Retardation of the transport of Na, K and OH ions on pore structure caused by acidic action of mineral admixture particles in matrix10.1016/0008-8846(94)90118-X ↗
38. Heavy metal speciation and leaching behaviors in cement based solidified/stabilized waste materials10.1016/S0304-3894(00)00360-5 ↗
39. Effect of PbII and CrVI ions on the hydration of slag alkaline cement and the immobilization of these heavy metal ions10.1680/adcr.1999.11.3.111 ↗
40. Immobilization of cesium in alkaline activated fly ash matrix10.1016/j.jnucmat.2005.06.006 ↗
41. Morrison · 2004