Study on the durability of eco-friendly recycled aggregate concrete with supplementary cementitious materials: The combined action of compound salt solution of MgSO4, Na2SO4, and NaCl and dry-wet cycles
Source abstract
Abstract
Focusing on eco-friendliness and sustainability, recycled aggregate concrete (RAC) has been recently substituted for natural aggregate concrete (NAC) in new constructions. In Northwest China, high-concentration corrosive ions of magnesium, sulfate, and chloride exist in soil and groundwater, which have a severe adverse effect of exposing RAC’s durability. To improve the efficient utilization of RAC in the environment of the aggressive ion, the durability experiment of eco-friendly RAC with supplementary cementitious materials (SCMs) under the combined action of 7.5 %Na 2SO 4 + 7.5 %MgSO 4 + 5 %NaCl and dry-wet cycles was investigated. Results show that RAC with the ternary blend of cement-fly ash-granulated blast furnace slag had the best durability among all the RAC mixtures. The 10 % fly ash + 20 % silica fume and 10 % fly ash + 20 % metakaolin negatively affected the durability improvement of RAC. At the same D&W cycles, the relative content of hydration and corrosive products of RAC with SCMs was lower than that of RAC without SCMs, and Friedel’s salt and Mg 10(OH) 18Cl 2·5H 2O were not found. The mineral phase composition of RAC exposed to the compound salt solution was related to the relative content of portlandite. Furthermore, grain volume increasing from brucite and gypsum, salt crystallization pressure from blödite and MgCl 2, and solid volume changing from thenardite to mirabilite mainly degraded RAC’s durability.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Recycled Aggregate Concrete Performance · Concrete and Cement Materials Research · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Effects of mix design and functional unit on life cycle assessment of recycled aggregate concrete: Evidence from CO2 concrete10.1016/j.conbuildmat.2022.128712 ↗
2. Effects of recycled aggregate combinations and recycled powder contents on fracture behavior of fully recycled aggregate concrete10.1016/j.jclepro.2022.132895 ↗
3. Recycled aggregates from construction and demolition waste towards an application on structural concrete: A review
4. An evaluation of the recycled aggregate characteristics and the recycled aggregate concrete mechanical properties10.1016/j.conbuildmat.2019.117978 ↗
5. Flexural behaviour and efficiency of CFRP-liminate reinforced recycled concrete beams: Optimization using linear weighted sum method10.1016/j.compstruct.2020.113259 ↗
6. Effective utilization and recycling of mixed recycled aggregates for a greener environment10.1016/j.jclepro.2019.07.075 ↗
7. Performance evolution of the interfacial transition zone (ITZ) in recycled aggregate concrete under external sulfate attacks and dry-wet cycling10.1016/j.conbuildmat.2019.116938 ↗
8. Durable performance of recycled aggregate concrete in aggressive environment10.1061/(ASCE)MT.1943-5533.0003253 ↗
9. Toward the development of sustainable concretes with recycled concrete aggregates: Comprehensive review of studies on mechanical properties10.1061/(ASCE)MT.1943-5533.0002304 ↗
10. Durability performance of brine-exposed shotcrete in salt lake environment10.1016/j.conbuildmat.2018.08.139 ↗
11. Deterioration of marine concrete exposed to wetting-drying action10.1016/j.jclepro.2020.123383 ↗
12. Chemical and mineralogical alterations of concrete subjected to chemical attacks in complex underground tunnel environments during 20–36 years10.1016/j.cemconcomp.2017.11.007 ↗
13. Damage behavior of the multiple ITZs in recycled aggregate concrete subjected to aggressive ion environment10.1016/j.conbuildmat.2020.118419 ↗
14. Performance evolution of recycled aggregate concrete (RAC) exposed to external sulfate attacks under full-soaking and dry-wet cycling conditions10.1016/j.conbuildmat.2020.118675 ↗
15. Performance of self-compacting concrete incorporating recycled concrete fines and aggregate exposed to sulphate attack10.1016/j.conbuildmat.2016.06.058 ↗
16. Experiment study on performance of cast-in-situ recycled aggregate concrete under different sulfate attack exposures10.1016/j.conbuildmat.2020.119144 ↗
17. Effect of MgSO4 solution on recycled aggregate concrete
18. Influence of recycled fine aggregates on the resistance of mortar to magnesium sulfate stack10.1016/j.wasman.2009.04.002 ↗
19. Evaluation of sulfate resistance of concrete with recycled and natural aggregates10.1016/j.conbuildmat.2017.06.161 ↗
20. Resistance of recycled aggregate concrete containing low- and high-volume fly ash against the combined action of freeze-thaw cycles and sulfate attack10.1016/j.conbuildmat.2018.01.084 ↗
21. Damage of recycled concrete with different aggregate substitution rates from the coupled action of freeze-thaw cycles and sulfate attack10.1016/j.conbuildmat.2019.06.060 ↗
22. Supplementary cementitious materials10.1016/j.cemconres.2010.12.001 ↗
23. A.O. Sojobi, T.F. Awolusi, G.B. Aina, O.L. Oke, M. Oladokun, D.O. Oguntayo, Ternary and quaternary blends as partial replacement of cement to produce hollow sandcrete blocks, Heliyon, 2021, 7: e07227. DOI: 10.1016/j.heliyon.2021.e07227.10.1016/j.heliyon.2021.e07227 ↗
24. Study on the mechanical properties and microstructure of fiber reinforced metakaolin-based recycled aggregate concrete10.1016/j.conbuildmat.2021.123554 ↗
25. Comparisons of natural and recycled aggregate concretes prepared with the addition of different mineral admixtures10.1016/j.cemconcomp.2011.05.009 ↗
26. Mechanical and durability properties of sustainable self-compacting concrete with recycled concrete aggregate and fly ash, slag, and silica fume10.1016/j.conbuildmat.2019.117115 ↗
27. Durability assessment of recycled aggregate HVFA concrete10.3390/app10186454 ↗
28. Corrosion resistance of recycled aggregate concrete incorporating slag
29. Berndt · Properties of sustainable concrete containing fly ash, slag and recycled concrete aggregate · 2009 · 23 · 2606
30. Evaluation of the damage process of recycled aggregate concrete under sulfate attack and wetting-drying cycles10.1016/j.conbuildmat.2017.02.022 ↗
31. Effect of fly ash, GGBS, and metakaolin on mechanical and durability properties of self-compacting concrete made with 100% coarse recycled aggregate, Journal of Hazardous10.1061/(ASCE)HZ.2153-5515.0000595 ↗
32. Performance assessment of concrete incorporating recycled coarse aggregates and metakaolin: A systematic approach10.1016/j.conbuildmat.2019.117223 ↗
33. Bond, durability and microstructural characteristics of ground granulated blast furnace slag based recycled aggregate concrete10.1016/j.conbuildmat.2019.04.017 ↗
34. Combined effects of supplementary cementitious materials (silica fume, GGBS, fly ash and rice husk ash) and steel fiber on the hardened properties of recycled aggregate concrete10.1016/j.conbuildmat.2020.120636 ↗
35. GB 175-2007, Common portland cement, National Standard of the People’s Republic of China.
36. GB/T 1596-2017, Fly ash used for cement and concrete, National Standard of the People’s Republic of China.
37. GB/T 18046-2017, Ground granulated blast furnace slag used for cement, mortar and concrete, National Standard of the People’s Republic of China.
38. GB/T 27690-2011, Silica fume for cement mortar and concrete, National Standard of the People’s Republic of China.
39. GB/T 25177-2010, Recycled coarse aggregate for concrete, National Standard of the People’s Republic of China.
40. Frost durability and stress-strain relationship of lining shotcrete in cold environment10.1016/j.conbuildmat.2018.11.264 ↗
41. GB/T 50081-2019, Standard for test methods of concrete physical and mechanical properties, National Standard of the People’s Republic of China.
42. Damage layer thickness and formation mechanism of shotcrete with and without steel fiber under sulfate corrosion of cry-wet cycles by ultrasound plane testing method10.1016/j.conbuildmat.2016.06.146 ↗
43. Comparison of fly ash, silica fume and metakaolin from mechanical properties and durability performance of mortar mixtures view point10.1016/j.conbuildmat.2014.07.089 ↗
44. Enhancing concrete sulfate resistance by adding NaCl10.1016/j.conbuildmat.2022.126370 ↗
45. The distributions of bound sulfates and chlorides in concrete subjected to mixed NaCl, MgSO4, Na2SO4 attack10.1016/S0008-8846(00)00386-0 ↗
46. Hydration kinetics and microstructure evolution of NaCl-mixed tricalcium silicate pastes10.1016/j.cemconres.2022.106934 ↗
47. New insights into how MgCl2 deteriorates Portlandite cement concrete10.1016/j.cemconres.2019.03.026 ↗
48. Improving the sulfate attack resistance of concrete by using supplementary cementitious materials (SCMs): A review10.1016/j.conbuildmat.2021.122628 ↗
49. Chloride ion permeability improvement of recycled aggregate concrete using pretreated recycled aggregates by silica fume slurry10.1016/j.conbuildmat.2020.121498 ↗
50. Mechanism of blended steel slag mortar with CO2 curing exposed to sulfate attack10.1016/j.conbuildmat.2020.118880 ↗
51. Attack of limestone cement-based material exposed to magnesium sulfate solution at low temperature, Journal of Wuhan University of Technology – Mater
52. Properties of magnesium silicate hydrates (M-S-H)10.1016/j.cemconres.2015.10.003 ↗
53. Characterization of magnesium silicate hydrate (M-S-H)10.1016/j.cemconres.2018.09.007 ↗
54. Effect of multiple ions on the degradation in concrete subjected to sulfate attack10.1016/j.conbuildmat.2020.119846 ↗
55. Study of deterioration of concrete exposed to different types of sulfate solution under drying-wetting cycles10.1016/j.conbuildmat.2016.04.094 ↗
56. Durability degradation of lining shotcrete exposed to Mg2+–SO42-–Cl-
57. The influence of sodium sulfate and magnesium sulfate on the stability of bound chlorides in cement paste10.1016/j.conbuildmat.2019.116775 ↗
58. Durability and microstructural analyses of concrete produced with treated demolition waste aggregates10.1016/j.conbuildmat.2022.128597 ↗
59. The mechanical and interfacial properties of concrete prepared by recycled aggregate with chloride corrosion media10.1016/j.conbuildmat.2021.122653 ↗
60. Performance of recycled concretes exposed to sulphate soil for 10 years10.1016/j.conbuildmat.2015.11.025 ↗
61. The effect of recycled fine aggregate treated as washed, less washed and unwashed on the mechanical and durability characteristics of concrete under MgSO4 and freeze-thaw cycles10.1016/j.jobe.2021.103924 ↗
62. Response of concrete to accelerated physical salt attack exposure10.1016/j.cemconres.2015.02.006 ↗
63. Mechanism of concrete deterioration due to salt crystallization10.1016/j.matchar.2004.08.013 ↗