journal article·2020-08Open access

Railway ballast stabilising agents: Comparison of mechanical properties

Diego Maria Barbieri, Marius Tangerås, Elias Kassa, Inge Hoff, Zhuangzhuang Liu, Fusong Wang

Abstract

Expensive and time-consuming maintenance operations are routinely performed to preserve the ballast mechanical properties in railway lines. Binding agents are used for ballast stabilisation. Four different additives based on bitumen, organosilane, lignosulphonate and polyurethane are investigated in the laboratory by means of repeated load triaxial tests. The parameters that are directly relevant for use in railway structures are assessed. Each binder type significantly influences both the resilient modulus and the resistance to permanent deformation of the treated specimens. The ballast mechanical properties can be conveniently modified, thus being beneficial to track stability and railway maintenance programme.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Railway Engineering and Dynamics · Geotechnical Engineering and Underground Structures · Civil and Geotechnical Engineering Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (69)

Show source-provided references
1. Selig · 1994
2. Norwegian National Rail Administration - Bane NOR SF, Overbygning – teknisk regelverk, https://trv.banenor.no/wiki/Overbygning, 2019 (accessed October 8, 2019).
3. Effect of particle size distribution and subgrade condition on degradation of railway ballast under impact loads10.1007/s10035-017-0747-0 ↗
4. Characterization of the fouled ballast layer in the substructure of a 19th century railway track under renewal10.3208/sandf.50.55 ↗
5. Effect of grading on degradation of crushed-rock railway ballast and on permanent axial deformation10.3141/2154-15 ↗
6. A review of loading conditions for railway track structures due to train and track vertical interaction
7. Track transitions in railways: a review10.1016/j.conbuildmat.2016.02.084 ↗
8. S. Lakušic, M. Ahac, I. Haladin, Track stability using ballast bonding method, in: 10th Slov. Road Transp. Congr., Portoroz, 2010.
9. High speed and track deterioration: the role of vertical stiffness of the track10.1243/095440904322804411 ↗
10. Transition of railroad bridge approaches10.1061/(ASCE)1090-0241(2005)131:11(1392) ↗
11. Automated and cost effective maintenance for railway (ACEM–Rail)10.1016/j.sbspro.2012.06.1082 ↗
12. V. Fontserè, A.L. Pita, N. Manzo, A. Ausilio, NEOBALLAST: New High-performance and Long-lasting Ballast for Sustainable Railway Infrastructures, in: Transp. Res. Procedia, Elsevier, 2016, pp. 1847–1854. doi:10.1016/j.trpro.2016.05.151.10.1016/j.trpro.2016.05.151 ↗
13. Polyurethane-based stabilization of railroad ballast – a critical review, Nternational10.1080/23248378.2019.1570477 ↗
14. Bitumen stabilized ballast: a potential solution for railway track-bed10.1016/j.conbuildmat.2016.07.067 ↗
15. Bitumen stabilized ballast: a full-scale investigation on its use for existing and newly constructed railway trackbeds
16. Novel performance-based technique for predicting maintenance strategy of bitumen stabilised ballast10.1016/j.conbuildmat.2017.11.115 ↗
17. Polyurethane reinforced ballasted track: review, innovation and challenge10.1016/j.conbuildmat.2019.03.031 ↗
18. Innovative stabilization techniques for weak crushed rocks used in road unbound layers: a laboratory investigation10.1016/j.trgeo.2018.12.002 ↗
19. Organosilane and lignosulfonate as innovative stabilization techniques for crushed rocks used in road unbound layers10.1016/j.trgeo.2019.100308 ↗
20. Characterizing temperature performance of bio-modified binders containing RAP binder10.1061/(ASCE)MT.1943-5533.0002373 ↗
21. Mechanical characterisation of the fouled ballast in ancient railway track substructure by large-scale triaxial tests10.1016/j.sandf.2012.05.009 ↗
22. W.F. Anderson, P. Fair, Behavior of railroad ballast under monotonic and cyclic loading, 134 (2008) 316–327. doi:10.1061/(ASCE)1090-0241(2008)134.10.1061/(ASCE)1090-0241(2008)134:3(316) ↗
23. Cyclic loading of railway ballast under triaxial conditions and in a railway test facility10.1007/s10035-009-0144-4 ↗
24. Shear behaviour of railway ballast based on large-scale triaxial tests10.1061/(ASCE)1090-0241(1998)124:5(439) ↗
25. Analysis of asphalt concrete track based on service line test results10.1016/j.conbuildmat.2019.01.131 ↗
26. Evaluation of asphalt concrete mixtures for railway track10.1016/j.conbuildmat.2014.09.053 ↗
27. Investigation of asphalt track behavior under cyclic loading: full-scale testing and numerical simulation10.1520/JTE20160554 ↗
28. N. Thom, Principles of pavement engineering, second, ICE, Lon, 2014.
29. Broader societal issues of nanotechnology10.1023/A:1025548512438 ↗
30. K. Sobolev, S.P. Shah, Nanotechnology in construction, in: K. Sobolev, S.P. Shah (Eds.), Proc. NICOM5, Springer, 2015, p. 509. doi:10.1007/978-3-319-17088-6.10.1007/978-3-319-17088-6 ↗
31. Modern developments related to nanotechnology and nanoengineering of concrete10.1007/s11709-016-0343-0 ↗
32. J. Daniels, M.S. Hourani, Soil improvement with organo-silane, in: U.S.-China Work. Gr. Improv. Technol. 2009, Orlando, 2009. doi:doi.org/10.1061/41025(338)23.10.1061/41025(338)23 ↗
33. Nanotechnology as a preventive engineering solution to highway infrastructure failures10.1061/(ASCE)CO.1943-7862.0000670 ↗
34. V. Padmavathi, E.C. Nirmala Peter, P.N. Rao, M. Padmavathi, Stabilization of soil using Terrasil, Zycobond and cement as admixtures, in: H. Poulos (Ed.), Latest Thoughts Gr. Improv. Tech. GeoMEast 2018, Springer, 2018, pp. 163–170.10.1007/978-3-030-01917-4_13 ↗
35. Stiffness-based quality control evaluation of modified subgrade soil using lightweight deflectometer10.1061/(ASCE)MT.1943-5533.0001958 ↗
36. BS EN, Characterisation of waste. Leaching. Compliance test for leaching of granular waste materials and sludges. Part 2: one stage batch test at a liquid to solid ratio of 10 l/kg for materials with particle size below 4 mm (without or with size reduction), 2003.
37. DD CEN/TS, Characterization of waste. Leaching behaviour tests. Up-flow percolation test (under specified conditions), 2006.
38. Mechanisms of stabilization of expansive soil with lignosulfonate admixture10.1016/j.trgeo.2017.11.001 ↗
39. Stabilization of silty sand with nontraditional additives
40. A theoretical and experimental study on the behaviour of lignosulfonate-treated sandy silt10.1016/j.compgeo.2014.06.010 ↗
41. B. Ta’negonbadi, R. Noorzad, Physical and geotechnical long-term properties of lignosulfonate-stabilized clay: an experimental investigation, Transp. Geotech. 17 (2018) 41–50. doi:10.1016/j.trgeo.2018.09.001.10.1016/j.trgeo.2018.09.001 ↗
42. Application of lignin-stabilized silty soil in highway subgrade: a macroscale laboratory study
43. I. Hoff, L.J. Bakløkk, J. Aurstad, Influence of laboratory compaction method on unbound granular materials, in: 6th Int. Symp. Pavements Unbound, 2003.
44. NPRA, Stabilisering av bærelag med DUSTEX, oppfølging av FOU rapport nr. 2008003393-1, 2017.
45. Application of lignin-based by-product stabilized silty soil in highway subgrade: a field investigation10.1016/j.jclepro.2016.12.002 ↗
46. F.S. Rostler, R.M. White, K. Nair, R.G. Hucks, J.W. Newton, Study of methods of stabilizing conventional ballast using polymers, Oakland, 1966.
47. Application of polyurethane geocomposites to help maintain track geometry for high-speed ballasted railway tracks10.1631/jzus.A12ISGT3 ↗
48. Track stiffness management using the XiTRACK GeoComposite
49. M.S. Dersch, E. Tutumluer, A.P. Mareno, C.T. Peeler, D.K. Bower, Characterization of polyurethane coated railroad ballast behavior, Transp. Res. Rec. (2011).
50. Polyurethane coating of railroad ballast aggregate for improved performance
51. A. Keene, T. Edil, J. Tinjum, Mitigating ballast fouling and enhancing rail freight capacity, Madison, 2012.
52. Elastomeric revetments – an innovative solution for coastal protection and erosion control
53. CEN, ISO 13286-7 Cyclic load triaxial test for unbound mixtures, Belgium, 2004.
54. The effects of grading scale on repeated load triaxial test results10.1080/10298430108901719 ↗
55. CEN, ISO 13286-4 Test methods for laboratory reference density and water content - Vibrating hammer, Belgium, 2003.
56. B. Dongmo-Engeland, GARAP, Influence of sample’s height on the development of permanent deformation, Trondheim, 2005.
57. State of the art. I: resilient response of unbound aggregates10.1061/(ASCE)0733-947X(2000)126:1(66) ↗
58. State of the art. II: permanent strain response of unbound aggregates10.1061/(ASCE)0733-947X(2000)126:1(76) ↗
59. Deformational behavior of fouled railway ballast10.1139/cgj-2013-0271 ↗
60. I. Hoff, R.S. Nordal, A study to improve equipment and procedures for triaxial testing of coarse grained granular materials, in: R.S. Nordal, G. Refsdal (Eds.), 5th Int. Conf. Bear. Capacit. Roads Airfields, Tapir, Trondheim, 1998, pp. 1351–1360.
61. Deformation and degradation mechanisms of railway ballast under high frequency cyclic loading10.1061/(ASCE)GT.1943-5606.0001375 ↗
62. R.G. Hicks, C.L. Monismith, Factors influencing the resilient properties of granular materials, in: Highw. Res. Rec., 1971, pp. 15–31.
63. Characterization of granular material
64. A.F.L. Hyde, Repeated load triaxial testing of soils, University of Nottingham, 1974.
65. An experimental study on the characteristics of polyurethane-mixed coarse aggregates by large-scale triaxial test10.1016/j.conbuildmat.2017.03.107 ↗
66. Study of railway track stiffness modification by polyurethane reinforcement of the ballast10.1016/j.trgeo.2014.06.005 ↗
67. Full-scale study of Neoballast section for its application in railway tracks: optimization of track design10.1617/s11527-018-1167-2 ↗
68. Permanent deformation behavior of granular materials and the shakedown concept10.3141/1757-09 ↗
69. Reducing railway track settlement using three-dimensional polyurethane polymer reinforcement of the ballast10.1016/j.conbuildmat.2013.03.002 ↗