Nanolime, ethyl silicate and sodium silicate: Advantages and inconveniences in consolidating ancient bricks (XII-XIII century)
Source abstract
Abstract
This paper aims to study the strengths and drawbacks of nanolime, ethyl silicate and sodium silicate coatings in consolidating heritage bricks. Initial X-ray diffraction (XRD), X-ray fluorescence (XRF), and thermogravimetric analyses (TG-MS) showed the bricks are particularly rich in carbonates, although they also contain quartz and minor proportions of halite and gypsum. The consolidants were examined by Transmission Electron Microscopy (TEM); Optical Microscopy (OM) and Scanning Electron Microscopy (SEM); and their effectiveness was tested by non-destructive methods based on colour variation or minimally destructive ones as peeling tests, Shore-A hardness and water permeability tests. The colorimetric properties of bricks were dissimilarly affected by the treatments being ethyl silicate the one that induced the lowest change. It was found that sodium silicate formed hard coatings that were prone to cracks and efflorescence formation after few days of curing. Nanolime and ethyl silicate provided similar consolidation performance, although water permeability was visibly reduced by the latter coating. In contrast, the initial XRD, XRF and TG-MS characterisation of heritage bricks confirmed they are more similar (compatible) to nanolime than the rest of treatments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Building materials and conservation · Cultural Heritage Materials Analysis · Conservation Techniques and Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Practical Building Conservation, Earth, Brick & Terracotta, Ashgate, London, 2015s.
2. E. Sebastián, G. Cultrone, Technology of Rammed-Earth Constructions (“Tapial”) in Andalusia (Spain): Their Restoration and Conservation, In: M.B. Dan, R. Přikryl, Á. Török - (Eds) Materials, Technologies and Practice in Historic Heritage Structures, Springer, Dordrecht, 2010, pp. 11-28. DOI:10.1007/978-90-481-2684-2_2.10.1007/978-90-481-2684-2_2 ↗
3. Characterisation of earthen walls in the Generalife (Alhambra): microstructural and physical changes induced by deposition of Ca(OH)2 nanoparticles in original and reconstructed samples10.1016/j.conbuildmat.2019.117202 ↗
4. ICOMOS 2nd International charter for the conservation and restoration of monuments and sites; the Venice charter, 1964.
5. Doehne · 2010
6. A further appraisal of the ‘lime technique’ for limestone consolidation, using a radioactive tracer
7. The nanolimes in Cultural Heritage conservation: characterisation and analysis of the carbonatation process10.1016/j.culher.2007.10.007 ↗
8. Nanotechnology in cultural heritage conservation: nanometric slaked lime saves architectonic and artistic surfaces from decay10.1016/j.culher.2006.02.001 ↗
9. Influence of substrate pore structure and nanolime particle size on the effectiveness of nanolime treatments10.1016/j.conbuildmat.2019.03.130 ↗
10. Use of diluted Ca(OH)2 suspensions and their transformation into nanostructured CaCO3 coatings: a case study in strengthening heritage materials (stucco, adobe and stone)10.1016/j.apsusc.2017.02.248 ↗
11. Use of image analysis to evaluate surface dispersion and covering performance of nanolime coatings sprayed on heritage material substrates10.1016/j.apsusc.2019.03.066 ↗
12. D. R. Lide, ed., CRC Handbook of Chemistry and Physics, Internet Version, , CRC Press, Boca Raton, FL, 2005.
13. Commercial Ca(OH)2 nanoparticles for the consolidation of immovable works of art10.1007/s00339-013-7942-6 ↗
14. A new method for consolidating wall paintings based on dispersions of lime in alcohol10.1179/sic.2000.45.3.154 ↗
15. An overview of nanolime as a consolidation method for calcareous substrates10.37558/gec.v11i0.455 ↗
16. Lime mortar consolidation with nanostructured calcium hydroxide dispersions: the efficacy of different consolidating products for heritage conservation10.1127/ejm/2015/0027-2437 ↗
17. Nanolime suspensions applied on natural lithotypes: the influence of concentration and residual water content on carbonatation process and on treatment effectiveness10.1016/j.culher.2009.04.001 ↗
18. Effect of solvent on nanolime transport within limestone: how to improve in-depth deposition10.1016/j.colsurfa.2016.03.007 ↗
19. Optimization of nanolime solvent for the consolidation of coarse porous limestone10.1007/s00339-016-0382-3 ↗
20. Influence of porosity and relative humidity on consolidation of dolostone with calcium hydroxide nanoparticles: effectiveness assessment with non-destructive techniques10.1016/j.matchar.2009.11.007 ↗
21. Durability of traditional and new nanoparticle based consolidating products for the treatment of archaeological stone tools: Chert artifacts from Atapuerca sites (Burgos, Spain)10.1016/j.culher.2016.10.019 ↗
22. Solvent-based ethyl silicate for stone consolidation: influence of the application technique on penetration depth, efficacy and pore occlusion10.1617/s11527-014-0417-1 ↗
23. A. Sierra-Fernández, L.S. Gómez-Villalba, M.E. Rabanal, R. Fort, New nanomaterials for applications in conservation and restoration of stony materials: A review, Mater Constr 67 (2017) 107. DOI:10.3989/mc.2017.07616.10.3989/mc.2017.07616 ↗
24. Characterization and reactivity of silicatic consolidants10.1016/j.conbuildmat.2006.01.006 ↗
25. Recent advance in alkoxysilane-based consolidants for stone10.1016/j.porgcoat.2018.11.003 ↗
26. Impacts of consolidation procedures on colour and absorption kinetics of carbonate stone10.1179/2047058412Y.0000000075 ↗
27. Consolidation with ethyl silicate: how the amount of product alters the physical properties of the bricks and affects their durability10.3989/mc.2018.12817 ↗
28. Effect of sodium silicate on Portland cement/calcium aluminate cement/gypsum rich-water system: strength and microstructure10.1039/C8RA09901D ↗
29. Influence of sodium silicate addition on the adsorption of oleic acid by fluorite, calcite and barite10.1016/0301-7516(85)90002-X ↗
30. Silicate species of water glass and insights for alkali-activated green cement
31. Synthesis and morphological examination of high-purity Ca(OH)2 nanoparticles suitable to consolidate porous surfaces10.1016/j.apsusc.2017.03.210 ↗
32. ASTM, D 3359-02. Standard Test Methods for Measuring Adhesion by Tape Test, (2004).
33. Standardization of peeling tests for assessing the cohesion and consolidation characteristics of historic stone surfaces10.1617/s11527-011-9778-x ↗
34. The effectiveness of ethyl silicate as consolidating and protective coating to extend the durability of earthen plasters10.1016/j.conbuildmat.2019.117445 ↗
35. RILEM COMMISSION 25 PEM, Test No I.1 – Porosity accessible to water, Mater. Constr. RILEM 13. (1980) 177–179.
36. D. Vandevoorde, V. Cnudde, J. Dewanckele, L. Brabant, M. de Bouw, V. Meynen, E. Verhaeven, Validation of in situ applicable measuring techniques for analysis of the water absorption by stone, Proc. Chem. (2013) 317–327.10.1016/j.proche.2013.03.039 ↗
37. A. Lyons, Materials for architects and builders: Fourth edition, Taylor & Francis, London, 2010. DOI:10.4324/9780080949598.10.4324/9780080949598 ↗
38. EN 771-16:2011, Methods of test for masonry units - Part 16: Determination of dimensions, European Committee for Standardization (CEN); 2011.
39. Földvári · 2011
40. J.W. Anthony, R.A. Bideaux, K.W. Bladh, M.C. Nichols (Eds.), Handbook of Mineralogy, Mineralogical Society of America, Chantilly, VA 20151-1110, USA. http://www.handbookofmineralogy.org/.
41. Weathering traces in ancient bricks from historic buildings10.1016/j.buildenv.2004.08.027 ↗
42. Bricks in historical buildings of Toledo City: characterisation and restoration10.1016/S1044-5803(03)00101-3 ↗
43. Thermal analysis – including evolved gas analysis – of clay raw materials10.1016/0169-1317(93)90029-Z ↗
44. Cracking of organosilicone stone consolidants in gel form10.2307/1506552 ↗
45. Monitoring Wall Paintings Affectedby Soluble Salts – The Conservation of Wall Paintings
46. Sodium metasilicate (Na2SiO3): a thermo-kinetic analysis of its CO2 chemical sorption10.1016/j.tca.2008.04.022 ↗
47. Pierre · 2020
48. Use of TEOS for fired-clay bricks consolidation10.1617/s11527-013-0120-7 ↗
49. Calcium hydroxide nanoparticles coatings applied on cultural heritage materials: their influence on physical characteristics of earthen plasters10.1016/j.apsusc.2019.144195 ↗
50. Ethyl silicate for surface protection of concrete: performance in comparison with other inorganic surface treatments10.1016/j.cemconcomp.2013.05.008 ↗