Mechanism and erosion resistance of internally cured concrete including super absorbent polymers against coupled effects of acid rain and fatigue load

Wenzhen Wang, Aiqin Shen, Ziming He, Yinchuan Guo, Desheng Li

Publisher page

Abstract

Abstract This study explored a novel method for inhibiting the effects of acid rain erosion and fatigue loading in concrete by incorporating super absorbent polymers (SAP). Three different dosages and four particle sizes of SAP were considered to evaluate the erosion resistance to a simulated acid rain solution (pH = 3.0) for eight test cycles. The mass loss, compressive strength, flexural strength, and erosion depth as well as the results of X-ray diffraction (XRD) and the mercury intrusion porosimetry (MIP) testing were employed to explore the erosion behavior and mechanism of the internally cured concrete with SAPs. The results show that the coupled effects of acid rain and fatigue loading has a remarkable influence on the performance degradation of concrete. The erosion of concrete by acid rain was delayed and weakened with the addition of SAP, particularly when 0.10% SAP was added with a particle size of 100–120 mesh. Moreover, the SAP promoted hydration, which lessened the deterioration caused by pore deformation and improved the internal pore structure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete Properties and Behavior · Concrete and Cement Materials Research · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. R. Ragoug, O.O. Metalssi, F. Barberon, J.M. Torrenti, J.B.D.E.D. Lacaillerie, Durability of cement pastes exposed to external sulfate attack and leaching: Physical and chemical aspects, Cem. Concr. Res. 116(2019) 134-145, https://doi.org/10.1016/j.cemconres.2018.11.006.10.1016/j.cemconres.2018.11.006 ↗
2. Influence of accelerator type and dosage on the durability of wet-mixed sprayed concrete against external sulfate attack10.1016/j.conbuildmat.2019.117883 ↗
3. Durability of Steel Fibre Reinforced Concrete (SFRC) exposed to acid attack-A literature review
4. Simulated sulfuric and nitric acid rain inhibits leaf breakdown in streams: A microcosm study with artificial reconstituted fresh water10.1016/j.ecoenv.2020.110535 ↗
5. Investigation on effect of aggregate on three non-destructive testing properties of concrete subjected to sulfuric acid attack10.1016/j.conbuildmat.2016.04.017 ↗
6. An experimental investigation on the erosion resistance of concrete containing various PET particles percentages against sulfuric acid attack10.1016/j.conbuildmat.2014.12.037 ↗
7. Steel and synthetic types of fibre reinforced concrete exposed to chemical erosion10.1016/j.conbuildmat.2015.06.023 ↗
8. Acid attack on geopolymer cement mortar based on waste-glass powder and calcium aluminate cement at mild concentration10.1016/j.conbuildmat.2018.10.203 ↗
9. Understanding of the deterioration characteristic of concrete exposed to external sulfate attack: Insight into mesoscopic pore structures10.1016/j.conbuildmat.2020.119932 ↗
10. M. Lanzon, E. Martinez, M. Mestre, J. Antonio Madrid, Use of zinc stearate to produce highly-hydrophobic adobe materials with extended durability to water and acid-rain, Constr. Build. Mater. 139(2017) 114-122, https://doi.org/10.1016/j.conbuildmat.2017.02.055.10.1016/j.conbuildmat.2017.02.055 ↗
11. Physical-chemical study, characterisation and use of image analysis to assess the durability of earthen plasters exposed to rain water and acid rain10.1016/j.conbuildmat.2018.07.235 ↗
12. Durability of self-compacting concrete containing pumice and zeolite against acid attack, carbonation and marine environment10.1016/j.conbuildmat.2017.12.235 ↗
13. Compressive and direct tensile behavior of concrete containing Forta-Ferro fiber and calcium aluminate cement subjected to sulfuric acid attack with optimized design10.1016/j.conbuildmat.2020.118999 ↗
14. Erosion resistance of high-strength concrete containing forta-ferro fibers against sulfuric acid attack with an optimum design10.1016/j.conbuildmat.2017.07.180 ↗
15. Performance optimization of hybrid fiber concretes against acid and sulfate attack10.1016/j.jobe.2020.101443 ↗
16. Using EDTA-2Na to inhibit sulfate attack in slag cement mortar under steam curing10.1016/j.conbuildmat.2020.120324 ↗
17. Sulphuric acid resistance of plain, polymer modified, and fly ash cement concretes10.1016/j.conbuildmat.2009.08.001 ↗
18. The degradation mechanisms of alkali-activated fly ash/slag blend cements exposed to sulphuric acid10.1016/j.conbuildmat.2018.08.050 ↗
19. Effect of acid rain erosion on steel fiber reinforced concrete10.1007/s11595-017-1569-y ↗
20. R. Preetham, R. Hari Krishna, M.N. Chandraprabha, T. Thomas, Vehicular soot for improvement of chemical stability of cement composites towards acid rain and sewage like atmospheres, Constr. Build. Mater. 248(2020) 118604, https://doi.org/10.1016/j.conbuildmat.2020.118604.10.1016/j.conbuildmat.2020.118604 ↗
21. Feasibility study of waste Poly Ethylene Terephthalate (PET) particles as aggregate replacement for acid erosion of sustainable structural normal and lightweight concrete10.1016/j.jclepro.2016.02.143 ↗
22. Sustainable approach for recycling waste tire rubber and polyethylene terephthalate (PET) to produce green concrete with resistance against sulfuric acid attack10.1016/j.jclepro.2016.03.074 ↗
23. Mechanical properties and durability of concrete specimens containing nano silica in sulfuric acid rain condition10.1016/j.conbuildmat.2018.01.137 ↗
24. Comparison of corrosion resistance mechanism between ordinary Portland concrete and alkali-activated concrete subjected to biogenic sulfuric acid attack10.1016/j.conbuildmat.2019.117071 ↗
25. Influence of superabsorbent polymers (SAPs) type and particle size on the performance of surrounding cement-based materials10.1016/j.conbuildmat.2020.121442 ↗
26. Early-state water migration characteristics of superabsorbent polymers in cement pastes10.1016/j.cemconres.2019.02.010 ↗
27. Cement-based materials modified with superabsorbent polymers: A review10.1016/j.conbuildmat.2019.07.139 ↗
28. Absorption kinetics of superabsorbent polymers (SAP) in various cement-based solutions10.1016/j.cemconres.2017.03.009 ↗
29. Self-healing of modified sulfur composites with calcium sulfoaluminate cement and superabsorbent polymer10.1016/j.compositesb.2019.01.003 ↗
30. Life-cycle crack resistance and micro characteristics of internally cured concrete with superabsorbent polymers10.1016/j.conbuildmat.2020.119794 ↗
31. Research on shrinkage development and fracture properties of internal curing pavement concrete based on humidity compensation10.1016/j.conbuildmat.2019.01.115 ↗
32. The influence of superabsorbent polymers on strength and durability properties of blended cement mortars10.1016/j.cemconcomp.2014.03.008 ↗
33. Effect of superabsorbent polymer on the properties of concrete10.3390/polym9120672 ↗
34. Influence of SAP on the chloride penetration and corrosion behavior of steel bar in concrete10.1016/j.corsci.2020.108714 ↗
35. Effects of SAP on the properties and pore structure of high performance cement-based materials10.1016/j.conbuildmat.2016.11.090 ↗
36. Effect of superabsorbent polymers (SAP) on the freeze-thaw resistance of concrete: results of a RILEM interlaboratory study10.1617/s11527-016-0868-7 ↗
37. An experimental study on absorptivity measurement of superabsorbent polymers (SAP) and effect of SAP on freeze-thaw resistance in mortar specimen10.1016/j.conbuildmat.2020.120974 ↗
38. Chemical durability of superabsorbent polymer (SAP) based geopolymer mortars (GPMs)10.1016/j.conbuildmat.2019.05.101 ↗
39. Investigation on the mechanical properties and environmental impacts of pervious concrete containing fly ash based on the cement-aggregate ratio10.1016/j.conbuildmat.2019.01.044 ↗
40. Effect of controlled environmental conditions on mechanical, microstructural and durability properties of cement mortar10.1016/j.conbuildmat.2017.12.206 ↗
41. Deterioration of mode II fracture toughness, compressive strength and elastic modulus of concrete under the environment of acid rain and cyclic wetting-drying10.1016/j.conbuildmat.2019.116809 ↗
42. Freeze-thaw resistance of recycled aggregate concrete damaged by simulated acid rain10.1016/j.jclepro.2020.124396 ↗
43. Deterioration of concrete due to acid rain attack in north China
44. Deterioration mechanism of interface transition zone of concrete pavement under fatigue load and freeze-thaw coupling in cold climatic areas10.1016/j.conbuildmat.2017.11.031 ↗
45. Evolution mechanism of microscopic pores in pavement concrete under multi-field coupling10.1016/j.conbuildmat.2018.04.022 ↗
46. Investigations of chloride ions permeability of pavement concrete under coupled effect of fatigue loading and hydrodynamic pressure
47. Deflection determination method for BFRP prestressed concrete beams under fatigue loading10.1016/j.compstruct.2019.111182 ↗
48. Model of time-dependent and stress-dependent chloride penetration of concrete under sustained axial pressure in the marine environment10.1016/j.conbuildmat.2018.03.077 ↗
49. Numerical simulation of internal stress in pavement concrete under rolling fatigue load
50. Ministry of Transport of the People’s Republic of China (Mot) · 2005
51. Shape feature parameters and distribution rule of coarse aggregate based on image analysis
52. Durability of concrete exposed to leaching and external sulphate attacks10.1016/j.cemconres.2009.07.021 ↗
53. Long-term behaviors of concrete under low-concentration sulfate attack subjected to natural variation of environmental climate conditions10.1016/j.cemconres.2018.11.017 ↗
54. Investigation of carbonation resistance and mechanism of SAP internal curing concrete in humid and hot environment