Corrosion behaviors of basalt fiber exposed to the acids
Source abstract
Abstract
Abstract In this work, Taguchi method was employed to elaborate the effects of temperature, concentration and immersion time of typical acids (HCl, H2SO4, HNO3) on the morphology and tensile strength of basalt fiber (BF). The results showed that the corrosion behavior of BF was controlled by the ion-exchange process with presence of H+ ions, and irregular and spiral cracks were formed during this process, which led to the severe degradation on the tensile strength of fiber. Besides the governing role of H+ concentration in acids, SO42- also aggravated the corrosion in sulfuric acid with precipitant of CaSO4. The reasons behind the acid-induced low-energy crack opening paths were given to illustrate the formation of spiral cracks on fiber surface in acids. The ubiquitous axial defects were revealed on fiber surface, and comparative results confirmed that such defects originated from the scratching between the filament and bushing during the fiber spinning process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Natural Fiber Reinforced Composites · Fiber-reinforced polymer composites · Advanced Cellulose Research Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Basalt fibers
2. Mineral fibres: basalt
3. Basalt-based fiber-reinforced materials and structural applications in civil engineering10.1016/j.compstruct.2019.02.002 ↗
4. A short review on basalt fiber reinforced polymer composites10.1016/j.compositesb.2014.12.011 ↗
5. Study on mechanical properties of alkali-resistant basalt fiber reinforced concrete10.1016/j.conbuildmat.2020.118424 ↗
6. Effect of alkalinity on the shear performance degradation of basalt fiber-reinforced polymer bars in simulated seawater sea sand concrete environment10.1016/j.conbuildmat.2021.123957 ↗
7. A review on basalt fibre and its composites10.1016/j.compositesb.2014.12.034 ↗
8. Durability of basalt fibers and composites in corrosive environments10.1177/0021998314526628 ↗
9. Corrosion behaviour and crack formation mechanism of basalt fibre in sulphuric acid10.1016/j.corsci.2012.06.028 ↗
10. Corrosion behaviour and mechanism of basalt fibres in acidic and alkaline environments10.1016/j.corsci.2016.04.019 ↗
11. Chemical degradation of basalt fibers
12. Investigation on slag fiber characteristics: Mechanical property and anti-corrosion performance10.1016/j.ceramint.2015.01.001 ↗
13. Gao · 2016
14. Optimization of binder jetting using Taguchi method10.1007/s11837-016-2231-4 ↗
15. Performance analysis and optimum operation of a thermoelectric generator by Taguchi method10.1016/j.apenergy.2015.08.025 ↗
16. Chemical and thermal resistance of basalt fiber in inclement environments10.1007/s11595-013-0731-4 ↗
17. Tensile behavior contrast of basalt and glass fibers after chemical treatment10.1016/j.matdes.2010.04.009 ↗
18. Corrosion behaviour of low dielectric glass fibres in hydrochloric acid10.1016/j.jnoncrysol.2018.12.039 ↗
19. Fractures in GRP — a link with corrosion
20. Mind the helical crack10.1038/464042a ↗
21. Properties and applications of basalt fiber and its composites
22. Molybdenum disilicide-silicon nitride bushing nozzles tailor-made for basalt fibers production10.1016/j.ceramint.2016.04.106 ↗
23. What happens to glass fiber under extreme chemical conditions?10.1016/j.jnoncrysol.2020.120331 ↗
24. Corrosion of E-glass fibers in acidic environments10.1016/S0266-3538(96)00158-3 ↗
25. Slow quasi-periodic curves and spiral cracks in chalcogenide glass thin films
26. Spiral cracking pattern in asphalt materials10.1016/j.matdes.2016.11.077 ↗
27. Development of functional glass fibres with nanocomposite coating: A comparative study10.1016/j.compositesa.2012.08.027 ↗
28. Glass fibers with clay nanocomposite coating: Improved barrier resistance in alkaline environment10.1016/j.compositesa.2011.09.013 ↗
29. Dean · 1999
30. Xie · 2008
31. Factors governing the tensile strength of basalt fibre10.1016/j.compositesa.2019.01.027 ↗
32. Relations between the anionic structure and viscosity of silicate melts—a Raman spectroscopic study
33. Corrosion mechanism of E-glass of chemical resistance glass fiber in acid environment10.1007/s11595-016-1461-1 ↗