Abstract
Abstract Variable-temperature Fourier-transform infrared (FTIR) spectroscopy was used to improve our understanding of chemical and physical properties of importance to gradual, thermoreversible aging in asphalt at cold temperatures. The FTIR peak area growth between 735 and 715 cm−1 follows a straight line upon cooling. Abrupt and significant changes in slope signify wax precipitation onset temperatures (WPT). Cold conditioning increased wax melt out temperatures (WMT), while chemical oxidation increased both WMT and WPT. Thermoreversible aging in an extended bending beam rheometer (EBBR) protocol shows Cold Lake, Alberta, and Laguna, Venezuela binders performing exceptionally well, likely because they are very low in crystallizable fractions (CF).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Asphalt Pavement Performance Evaluation · Infrastructure Maintenance and Monitoring · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (71)
Show source-provided references
1. Eurobitumen, “The Bitumen Industry – A Global Perspective.” Information Series 230 (IS 230), ISBN 978-1-934154-73-1.
2. Performance grading of the Lamont, Alberta C-SHRP pavement trial binders10.1080/10298430600715667 ↗
3. Asphalt pavement cracking: analysis of extraordinary life cycle variability in eastern and northeastern Ontario10.1080/10298430802343169 ↗
4. Non-isothermal kinetic analysis of reversible ageing in asphalt cement10.1080/14680629.2017.1389070 ↗
5. Preliminary experience with improved asphalt cement specifications in the City of Kingston, Ontario, Canada10.1016/j.conbuildmat.2017.09.118 ↗
6. Improved approach to low-temperature and fatigue fracture performance grading of asphalt
7. Five year performance review of a northern Ontario pavement trial: validation of Ontario’s DENT and EBBR test methods
8. Reversible aging in asphalt binders10.1021/ef060463b ↗
9. Performance grading of extracted and recovered asphalt cements10.1016/j.conbuildmat.2018.07.243 ↗
10. Durability assessment of asphalt binder10.1016/j.conbuildmat.2018.01.037 ↗
11. Methods for the quantification of recycled engine oil bottoms in performance-graded asphalt cement10.1061/(ASCE)MT.1943-5533.0002137 ↗
12. Effect of recycled engine oil bottoms on the ductile failure properties of straight and polymer-modified asphalt cements10.1016/j.conbuildmat.2016.08.156 ↗
13. Asphalt cement loss tangent as surrogate performance indicator for control of thermal cracking10.3141/2126-05 ↗
14. X-ray fluorescence detection of waste engine oil residue in asphalt and its effect on cracking in service10.1080/10298436.2010.488729 ↗
15. Effects of physical hardening on stress relaxation in asphalt cements10.3141/2207-05 ↗
16. Physical hardening in asphalt mixtures
17. Effect of waste engine oil residue on quality and durability of SHRP materials reference library binders10.3141/2444-12 ↗
18. J. Erskine, S.A.M. Hesp, F. Kaveh. Another look at accelerated aging of asphalt cements in the pressure aging vessel. Proc. Fifth Eurasphalt & Eurobitumen Congress, Istanbul, Turkey, June 13–15, 2012.
19. Ding · 2020
20. Transitions in unmodified and modified bitumen using FTIR spectroscopy
21. Eckmann · 2004
22. D.A. Anderson, R. Dongre. The SHRP direct tension specification test–its development and use. ASTM STP 1241, J.C. Hardin, Ed., ASTM, Philadelphia (1995), pp. 51–66.10.1520/STP18188S ↗
23. Low-temperature fracture testing of asphalt binders: regular and modified systems10.3141/1728-06 ↗
24. Low-temperature binder specification development thermal stress restrained specimen testing of asphalt binders and mixtures10.3141/1766-02 ↗
25. Compact tension testing of asphalt binders at low temperatures10.1177/0361198106196200105 ↗
26. Development of double edge notched tension (DENT) test for asphalt binders10.1520/JTE100678 ↗
27. Low-temperature thermal cracking of asphalt binder by asphalt binder cracking device10.1177/0361198106196200104 ↗
28. H.U. Bahia, D.A. Anderson. The development of the bending beam rheometer: basics and critical evaluation of the rheometer. In: Physical Properties of Asphalt Cement Binders. ASTM Spec. Techn. Publ., 1241 (1995), pp. 28–50.10.1520/STP18187S ↗
29. Etude statistique sommaire de quelques cas de fissuration thermique
30. F. Migliori, G. Ramond, M. Ballie, B. Brule, C. Exmelin, B. Lombardi, J. Samanos, A.F. Maia, C. Such, S. Watkins. Correlations between the thermal stress cracking of bituminous mixes and their binders’ rheological characteristics. Proc. Eurobitumen Workshop on Performance Related Properties for Bituminous Binders, Luxemburg, Paper No. 046 (1999), pp. 1–5.
31. I. Widyatmoko, R.C. Elliott, M.W. Heslop. Mapping crack susceptibility of bituminous materials with binder surability. Proc. Fifth RILEM International Conference on Cracking in Pavements – Mitigation, Risk Assessment and Prevention, University of Limoges, France, May 5-8, 2004.
32. I. Widyatmoko, M.W. Heslop, R.C. Elliott. The viscous to elastic transition temperature and the in situ performance of bituminous and asphaltic materials. Journal of the Institute of Asphalt Technology, Asphalt Professional, No 14 (2005), pp. 3–7.
33. Repeatability, reproducibility, and sensitivity assessments of thermal and fatigue cracking acceptance criteria for asphalt cement10.1016/j.conbuildmat.2019.117956 ↗
34. Acceptance testing of extracted and recovered asphalt cements for provincial and municipal paving contracts in Ontario
35. TSAR (Thermal Stress Analysis Routine) – Plus, Abatech Inc., Doylestown, PA, 1999.
36. Oxidative aging of asphalt cements from an Ontario pavement trial
37. The colloidal nature of asphalt as shown by its flow properties10.1021/j150378a005 ↗
38. Increase in viscosity of asphalts with time
39. Development of internal structure in asphalts
40. Steric hardening of asphalts
41. Struik · 1978
42. P.C. Blokker, H. Van Hoorn. Durability of bitumen in theory and practice. Proc. Fifth World Petroleum Congress, Section VI, Paper 27 (1959), pp. 417–432.
43. Physical hardening of paving grade asphalts as related to chemical characteristics
44. . A new interpretation of time-dependent physical hardening in asphalt based on DSC and optical thermoanalysis
45. Glass transition behavior and physical hardening of asphalt binders
46. Isothermal low-temperature physical hardening of asphalt
47. P. Kriz, J. Stastna, L. Zanzotto. Effect of stress on physical hardening of asphalts. Proc. Sixth Int. Conf. Pav. Techn., Sapporo, Japan, July 2008, pp. 1-8.
48. Characterization of physical aging by time-resolved rheometry: fundamentals and application to bituminous binders10.1007/s00397-018-1114-8 ↗
49. Physical hardening of asphalt binders relative to their glass transition temperatures10.3141/1661-05 ↗
50. Formation of equilibrium structures in bitumens10.1007/BF00725771 ↗
51. Physical hardening in asphalt
52. L.T. Germinario, T.L. Cutshall. Aging effects on compatibility, stability and morphology of asphalt polymer blends, Part I. Petersen Asphalt Research Conference, July 2002.
53. Surface structuring of wax in complex media10.1061/(ASCE)MT.1943-5533.0001032 ↗
54. On the existence of wax-induced phase separation in bitumen10.1080/10298436.2010.488730 ↗
55. Wax precipitation from North Sea crude oils. 2. Solid-phase content as function of temperature determined by pulsed NMR10.1021/ef00030a020 ↗
56. A 13C NMR and DSC study of the amorphous and crystalline phases in asphalts10.1021/ef980184r ↗
57. Thermal behavior of asphalt cements10.1016/S0040-6031(98)00537-1 ↗
58. P. Kriz, J. Stastna, L. Zanzotto. Effect of thermal history on glass transition and phase compatibility of asphalts. Proc. Fourth Eurasphalt & Eurobitumen Congress, Copenhagen, Denmark, May 21–23, 2008.
59. Modulated differential scanning calorimetry study of physical hardening rates in asphalt cements
60. Low-temperature reversible aging properties of selected asphalt binders based on thermal analysis10.1061/(ASCE)MT.1943-5533.0002625 ↗
61. C.D. Smith, C.C. Schuetz, R.S. Hodgson. Relationship between chemical structures and weatherability of coating asphalts as shown by infrared absorption spectroscopy. Ind. Eng. Chem., Prod. Res. Dev., 5(2) (1966), pp. 153–161.10.1021/i360018a013 ↗
62. D.R. Jones. SHRP Materials Reference Library: Asphalt Cements: A Concise Data Compilation. SHRP-A-645, Strategic Highway Research Program, National Research Council, Washington, DC (1993).
63. AASHTO (American Association of State Highway and Transportation Officials), Accelerated aging of asphalt binder using a pressurized aging vessel (PAV), Designation R 28, Washington, DC (2009).
64. Ontario Ministry of Transportation. LS-308 – Method of Test for Determination of Performance Grade of Physically Aged Asphalt Cement Using Extended Bending Beam Rheometer (BBR) Method. Revision 29 to MTO Laboratory Testing Manual, February 2015.
65. AASHTO (American Association of State Highway and Transportation Officials, 2016), Determination of performance grade of physically aged asphalt binder using the extended bending beam rheometer (BBR) method, TP 122–16, Washington, D.C. (2016).
66. Determination of wax precipitation temperature and amount of precipitated solid wax versus temperature for crude oils using FT-IR spectroscopy10.1021/ef010016q ↗
67. K.O. Oh. Prediction of wax appearance temperature and solid wax amount by reduced spectral analysis using FTIR spectroscopy. United States Patent 8,326,548 B2, December 4, 2012.
68. Comparison of physical and oxidative aging tendencies for Canadian and Northern European asphalt binders
69. Analysis of three premature pavement failures10.1177/0361198106196200106 ↗
70. Mohseni A. LTPPBind®, Version 3.1, Pavement Systems LLC, Bethesda, Maryland. Software written for Federal Highway Administration, McLean, Virginia, 2005.
71. J.C. Illman, T.J. Deahl. Alkylation of asphaltenes. West Conshohocken, PA, Proc. ASTM (1964), p. 21–38.10.1520/STP44532S ↗