Recovering shear capacity of heat-damaged beams using NSM-CFRP strips
Source abstract
Abstract
Abstract The potential of recovering shear capacity of heat-damaged beams using near surface mounted (NSM)-carbon fiber reinforced polymer (CFRP) strips was investigated in this work. Twenty-two under-reinforced concrete beams with shear reinforcement deficiency (150 × 250 × 1400) were cast and heat-treated for two hours in an electric furnace; under different temperatures (300, 500, and 600 °C). Later, control beams were strengthened, whereas post-heated ones repaired with NSM-CFRP strips, directed vertically across the depth of the beams and at different spacing values ranging from 100 to 200 mm. The mechanical behavior of the beams was evaluated under three-point loading test setup; with data collected and analyzed for the characteristics of the relationships between load and deflection or slippage (between concrete and reinforcing steel). Cracking and failure modes were monitored and characterized, as well. The experimental results indicated that the efficiency of repairing heat-damaged reinforced concrete beams using NSM-CFRP strips depended mainly upon damage level and spacing between NSM-CFRP strips. The result showed that using NSM-CFRP allowed restoring load capacity of the beams, damaged at 300 and 500 °C; but not so for those, post-heated to 600 °C. The latter achieved an utmost load capacity recovery of about 91% of original value. Lowering spacing between the CFRP strips contributed to increasing shear load capacity of repaired beams as long as peeling-off failure of the concrete cover across the depth of beam’s soffits was avoided. The flexural stiffness was not recovered for heat-damaged and repaired beams whereas toughness and ductility were noticeably improved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Structural Behavior of Reinforced Concrete · Fire effects on concrete materials · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Study on compressive mechanical capability of concrete after high temperature exposure and thermo-damage constitutive model10.1016/j.conbuildmat.2014.06.052 ↗
2. The nanogranular behavior of (C–S–H) at elevated temperatures (up to 700°C)10.1016/j.cemconres.2006.09.006 ↗
3. Effect of temperature and age of concrete on strength–porosity relation10.14311/516 ↗
4. Static and dynamic mechanical properties of concrete after high temperature exposure10.1016/j.msea.2012.02.058 ↗
5. Research, education and application in India and China in civil engineering
6. Repair of heat-damaged reinforced concrete T-beams using FRC jackets10.1680/macr.2007.59.3.223 ↗
7. Repair of heat-damaged RC shallow beams using advanced composites10.1617/s11527-007-9238-9 ↗
8. Effect of sulfates on bond behavior between carbon fiber reinforced polymer sheets and concrete10.1016/j.matdes.2012.07.018 ↗
9. Repair of shear-deficient and sulfate-damaged reinforced concrete beams using FRP composites10.1016/j.engstruct.2013.05.007 ↗
10. Bond characteristics of near surface mounted CFRP bars10.1016/j.conbuildmat.2013.01.021 ↗
11. Bond strength of near surface mounted FRP plates for retrofit of concrete structures10.1016/j.compstruct.2012.08.038 ↗
12. Bond of NSM systems in concrete strengthening – Examining design issues of strength, groove detailing and bond-dependent coefficient10.1016/j.conbuildmat.2013.06.069 ↗
13. Investigation of bond in concrete structures strengthened with near surface mounted carbon fibers reinforced polymer strips10.1061/(ASCE)1090-0268(2003)7:3(248) ↗
14. Bond behavior of FRP NSM systems in concrete elements10.1016/j.compositesb.2011.10.017 ↗
15. Flexural response of reinforced concrete members strengthened with near-surface-mounted CFRP strips
16. L.D. Lorenzis, A. Nanni, A.L. Tegola, Strengthening of reinforced concrete structures with near surface mounted FRP rods. in: Bibl International Meeting on Composites Materials, PLAST 2000, Milan, Italy, 2000.
17. Interaction forces in RC beams strengthened with near-surface mounted rectangular bars and strips10.1016/j.compositesb.2012.09.038 ↗
18. Flexural response of reinforced concrete (RC) beams strengthened with near surface mounted (NSM) fiber reinforced polymer (FRP) bars10.1016/j.compstruct.2013.10.051 ↗
19. NSM FRP shear strengthening of RC beams with internal stirrups
20. A. Mistry, P.V. Muley, P.R. Barbude, Enhancement of shear strengthening of RCC structures using NSM technique and estimation of flexural stresses using GFRP, in: 12th IRF International Conference, Pune, India, 2014.
21. Effective methods of using CFRP bars in shear strengthening of concrete girders10.1016/j.engstruct.2008.11.016 ↗
22. Strengthening of RC members using near-surface mounted FRP composites: design overview
23. Shear strengthening of concrete members using NSM method10.1016/j.proeng.2013.09.056 ↗
24. Design formula to evaluate the NSM FRP strips shear strength contribution to a RC beam10.1016/j.compositesb.2013.09.001 ↗
25. NSM shear strengthening technique with CFRP laminates applied in high-strength concrete beams with or without pre-cracking10.1016/j.compositesb.2011.09.006 ↗
26. American Concrete Institute · 2008
27. American Society for Testing and Materials International (ASTM). West Conshohocken, PA, 2004.
28. ACI Manual of Concrete Practice, Standard Practice For Selecting Proportions For Normal, Heavyweight, And Mass Concrete (ACI 211.1), Part I: Materials and General Properties of Concrete, Detroit, Michigan, 2008.
29. ACI Manual of Concrete Practice, Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (ACI 440.1R-15), Farmington, USA, 2015.