journal article·2019-02

Combined effects of mineral additions and curing conditions on strength and durability of self-compacting mortars exposed to aggressive solutions in the natural hot-dry climate in North African desert region

Aboubakeur Boukhelkhal, Lakhdar Azzouz, Said Kenai, El-Hadj Kadri, Benchaa Benabed

Publisher page

Abstract

Abstract The long-term behavior of self-compacting concrete (SCC) or mortar (SCM) in standard climate is relatively well studied. However, the performance of SCM under hot-dry climate is little investigated. In fact, strength and durability of SCM can be affected by climatic conditions and can be enhanced by the use of the mineral additives. The present paper analyses the combined effects of both mineral additions and curing conditions on the properties of self-compacting mortar exposed to natural hot-dry climate. Ten mixtures were prepared using blended binder containing three types of mineral additives (marble powder (MP), brick powder (BP) and metakaolin (MK)) in various proportions. In order to evaluate compressive and flexural strengths and ultrasonic pulse velocity (UPV), mortar specimens were stored in water for an initial curing period of 0, 1, 3, 7 and 28 days (T = 20 ± 2 °C and RH = 30%–50%), before being exposed to natural hot-dry climate in a North African desert region (T = 25–48 °C and RH = 8%–33%) until 28 days. The durability against sulfate and acid attacks was assessed by curing mortar specimens in water for seven days, followed by immersion-drying cycles for 56 days and then total immersion in MgSO4, Na2SO4, HCl and H2SO4 solutions until 360 days. The results showed an enhancement in hardened properties of SCM with increasing water-curing period. A water-curing period for a minimum 7 days appears to be necessary in hot-dry climate to achieve acceptable mechanical performances. Metakaolin seems to exhibit the best performance regarding mechanical properties and durability in sulfate mediums. Mineral additions show little influence in reducing damage due to acid attacks.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Building materials and conservation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. ACI Committee 305, Guide to Hot Weather Concreting, Detroit, MI, 2010.
2. Effect of casting temperature on strength and density of plainand blended cement concretes prepared and cured under hot weather conditions10.1016/j.conbuildmat.2016.02.211 ↗
3. Curing optimization for strength and durability of silica fume (SF) and fuel ash concretes under hot weather conditions10.1016/j.conbuildmat.2017.09.173 ↗
4. Meteoroligical station of Laghouat · 2016
5. Properties and durability of repair material of damaged structures in hot environment
6. Effect of curing on the compressive strength, resistance to chloride-ion penetration and porosity of concretes incorporating slag, fly ash or silica fume10.1016/0958-9465(95)00005-W ↗
7. Curing effects, strength and physical property of high strength silica fume concretes10.1061/(ASCE)0899-1561(1989)1:1(46) ↗
8. Effect of curing conditions on the mortars with and without GGBFS10.1016/j.conbuildmat.2006.08.013 ↗
9. Durability of self-compacted concrete containing slag in hot climate
10. Reusing of marble and granite powders in self-compacting concrete for sustainable development10.1016/j.jclepro.2016.02.044 ↗
11. The performance of high-strength flowable concrete made with binary, ternary, or quaternary binder in hot climate10.1016/j.conbuildmat.2013.05.062 ↗
12. Influence of high-temperature and low-humidity curing on chloride penetration in blended cement concrete10.1016/S0008-8846(02)00857-8 ↗
13. Carbonation rates of concretes containing high volume of pozzolanic materials10.1016/j.cemconres.2007.08.014 ↗
14. Effect of curing conditions on the permeability of concrete with high volume mineral admixtures10.1016/j.conbuildmat.2018.01.190 ↗
15. Resistance of limestone mortars with quaternary binders to sulfuric acid solution10.1016/j.conbuildmat.2011.06.050 ↗
16. Khelafi H, Benosman. Influence of natural pozzolan, silica fume and limestone fine on strength, acid resistance and microstructure of mortar10.1016/j.powtec.2014.01.046 ↗
17. Accelerated tests of hardened cement pastes alteration by organic acids: analysis of the pH effect10.1016/j.cemconres.2004.09.009 ↗
18. The effect of SCMs and curing time on resistance ofmortars subjected to organic acids10.1016/j.cemconres.2011.09.017 ↗
19. Behavior of self-compacting concrete made with marble and tile wastes exposed to external sulfate attack10.1016/j.conbuildmat.2016.12.193 ↗
20. Effect of natural pozzolana and marble powder on the properties of self-compacting concrete10.1016/j.conbuildmat.2011.12.109 ↗
21. Effects of marble powder as a partial replacement of cement on some engineering properties of self compacting concrete10.1080/01694243.2016.1184402 ↗
22. Effect of mineral admixtures on properties of self-compacting concrete10.1016/j.cemconcomp.2011.04.005 ↗
23. Effect of rice husk ash and other mineral admixtures on properties of self-compacting high performance concrete10.1016/j.matdes.2015.09.120 ↗
24. Effects of experimental ternary cements on fresh and hardened properties of self-compacting concretes10.1080/01694243.2015.1099864 ↗
25. Effects of granulated blast furnace slag and superplasticizer type on the fresh properties and compressive strength of self-compacting concrete10.1016/j.cemconcomp.2011.08.013 ↗
26. Incorporation of fillers from marble and tile wastes in the composition of self-compacting concretes10.1016/j.conbuildmat.2015.04.052 ↗
27. Workability retention and compressive strength of self-compacting concrete incorporating pumice powder and silica fume10.1016/j.conbuildmat.2016.12.090 ↗
28. Sorptivity of self-compacting concrete containing fly ash and silica fume10.1016/j.conbuildmat.2016.03.071 ↗
29. Strength and durability of low-impact environmental self-compacting concrete incorporating waste marble powder10.34118/jbms.v4i2.29 ↗
30. Effects of limited initial curing durations on mechanical properties of concrete
31. Importance of W/C ratio on compressive strength of concrete in hot climate conditions10.1016/j.buildenv.2006.05.003 ↗
32. Influence of calcined kaolin on mortar properties10.1016/j.conbuildmat.2010.11.017 ↗
33. EN 196-1, Methods of testing cement-Part 1: Determination of strength, 2002.
34. ASTM C597-16, Standard Test Method for Pulse Velocity Through Concrete, ASTM International, West Conshohocken, PA, 2016.
35. “Utilization of limestone powder to improve the properties of self-compacting concrete incorporating high volumes of untreated rice husk ash as fine aggregate10.1016/j.conbuildmat.2012.08.016 ↗
36. Standard test methods for length change of hydraulic-cement mortars exposed to a sulfate solution
37. Standard test methods for chemical resistance of mortars, grouts and monolithic surfacing and polymer concretes
38. Effect of environmental conditions on the properties of fresh and hardened concrete10.1016/S0958-9465(01)00007-5 ↗
39. Mechanical and durability properties of cement mortar with Algerian natural pozzolana10.1007/s10853-006-0227-0 ↗
40. Performance of concrete under different curing conditions10.1016/S0008-8846(96)85023-X ↗
41. The influence of initial water curing on the strength development of ordinary portland and pozzolanic cement concretes
42. Effect of initial water-curing period and curing condition on the properties of self-compacting concrete10.1016/j.matdes.2011.09.053 ↗
43. Effects of the initial water curing time on the corrosion behavior of steel bar corrosion in fly ash concrete10.1016/j.proeps.2009.09.117 ↗
44. Experimental study of early-age behavior of high performance concrete deck slabs under different curing methods10.1016/j.conbuildmat.2005.04.001 ↗
45. Relative strength, pozzolanic activity and cement hydration in superplasticized metakaolin concrete10.1016/0008-8846(96)00148-2 ↗
46. Durability of metakaolin concrete to sulfate attack10.1016/j.cemconres.2006.03.026 ↗
47. The effect of chemical admixtures and mineral additives on the properties of self-compacting mortars10.1016/j.cemconcomp.2005.12.003 ↗
48. Shrinkage of plain and silica fume cement concrete under hot weather10.1016/j.cemconcomp.2007.05.006 ↗
49. Mechanical properties and durability of mortar and concrete containing natural pozzolana and limestone blended cements10.1016/j.cemconcomp.2007.04.009 ↗
50. Ground granulated blast furnace slag effect on the durability of ternary cementitious system exposed to combined attack of chloride and sulfate10.1016/j.conbuildmat.2017.10.062 ↗
51. Performance of self-compacting concrete containing different mineral admixtures10.1016/j.conbuildmat.2011.04.032 ↗
52. Performance of volcanic ash and pumice based blended cement concrete in mixed sulfate environment10.1016/j.cemconres.2006.03.010 ↗
53. G. Escadeillas, H. Hornain, The durability of concretes: The concrete durability vis-à-vis the chemically aggressive environments. In: Jean-Pierre Ollivier, Angelique Vichot, editors, Scientific basis for the formulation of concretes durable in their environment. Presses ENPC; 2008 [In French].
54. Analysis of mortar long-term strength with supplementary cementitious materials cured at different temperatures
55. Characterization of the degradation of self-compacting concretes in sodium sulfate environment: Influence of different mineral admixtures10.1016/j.conbuildmat.2013.05.086 ↗
56. Consequences mecaniques de l’attaque sulfatique externe sur les betons autoplaçants
57. Investigation of the effects of acid rain on the deterioration of cement concrete using accelerated tests established in laboratory10.1016/j.atmosenv.2004.05.017 ↗
58. Effects of fly ash and silica fume on the resistance of mortar to sulphuric acid and sulphate attack10.1016/0008-8846(94)90063-9 ↗
59. Acidic attack of cement-based materials – a review Part 2. Factors of rate of acidic attack and protective measures10.1016/S0950-0618(02)00011-9 ↗
60. Durability of self-compacting concrete containing pumice and zeolite against acid attack, carbonation and marine environment10.1016/j.conbuildmat.2017.12.235 ↗
61. Resistance of different types of concretes to cyclic sulfuric acid and sodium sulfate attack10.1016/j.cemconcomp.2010.07.002 ↗