Abstract

Abstract Ion chelator can improve the self-healing ability of cement-based materials. In this paper, the effects of the mixture of ion chelator and mineral admixture (slag or fly ash) on salt-frost resistance of cement-based materials were investigated. The internal structure and mechanical properties of the mortars with ion chelator and mineral admixture before and after salt-frost cycles as well as curing were studied. The results show that the pore structure, mechanical strength and salt-frost resistance of the mortar mixed with ion chelator and slag are better than those of mortar mixed with ion chelator and fly ash. Compared with the control mortar, the harmful pores (larger than 0.1 mm) ratio of the mortar with ion chealtor and slag declined by 44.5%, while the compressive strength increased by 40.7%. After 100 times salt-frost cycles, the mass loss ratio, harmful pores proportion and compressive strength loss ratio of the mortar with ion chelator and slag had declined by 42.5%, 24.7% and 35% respectively than the control mortar. Curing 28 days after salt-frost, the mortar mixed with ion chelator has good self-healing ability, the compressive strength recovery ratio and harmful pores reduction ratio are 21.18% and 27.04%, respectively. A large amount of needle-like repair products appear in the pores of the mortar mixed with ion chelator. The results of the energy-dispersive spectroscopy and X-ray diffraction tests proved that the main products in the pores and cracks of the mortar are CaCO3 and CaSiO3.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microbial Applications in Construction Materials · Concrete and Cement Materials Research · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Mehta · 1986
2. Concrete durability10.1016/S0958-9465(02)00122-1 ↗
3. Study on the freeze-deicing salt resistance of the pavement concrete
4. Internal frost resistance and salt frost scaling of self-compacting concrete10.1016/S0008-8846(02)00968-7 ↗
5. Aggregate-cement paste transition zone properties affecting the salt-frost damage of high-performance concretes10.1016/j.cemconres.2004.06.009 ↗
6. Effect of sodium monofluorophosphate treatment on microstructure and frost salt scaling durability of slag cement paste10.1016/j.cemconres.2006.02.003 ↗
7. Influence of freeze-thaw cycles on capillary absorption and chloride penetration into concrete10.1016/j.cemconres.2017.05.018 ↗
8. Freeze-thaw resistance, mechanical and transport properties of self-consolidating concrete incorporating coarse recycled concrete aggregate10.1016/j.matdes.2013.07.100 ↗
9. Salt scaling resistance–the effect of curing and pre-saturation10.1016/j.conbuildmat.2011.06.058 ↗
10. A review of salt scaling: II. Mechanisms10.1016/j.cemconres.2007.03.003 ↗
11. Steel reinforcement corrosion in concrete under combined actions: the role of freeze-thaw cycles, chloride ingress, and surface impregnation10.1016/j.conbuildmat.2017.05.078 ↗
12. Limestone filler cement in low w/c concrete: a rational use of energy10.1016/S0008-8846(02)01087-6 ↗
13. Behavior of air-entrained concrete under the compression with constant confined stress after freeze–thaw cycles10.1016/j.cemconcomp.2007.10.006 ↗
14. A review of salt scaling: I. Phenomenology10.1016/j.cemconres.2007.03.005 ↗
15. Frost salt scaling resistance of concrete containing CFBC fly ash10.1617/s11527-008-9438-y ↗
16. Durability of reactive powder concrete under chloride-salt freeze–thaw cycling10.1617/s11527-016-0878-5 ↗
17. Effect of air entrainment on the mechanical properties, chloride migration, and microstructure of ordinary concrete and fly ash concrete10.1061/(ASCE)MT.1943-5533.0002456 ↗
18. D.J. Janssen, M.B. Snyder, Mass loss experience with ASTM C666: with and without deicing salt, 1997.
19. Laboratory freezing-and-thawing durability of fly ash pervious concrete in a simulated field environment
20. Experimental study on salt-frost resistance of superfine mineral admixture concrete
21. Salt-freezing resistance of high-volume mineral admixture concrete
22. Salt scaling resistance of fly ash ceramics concrete
23. Recent advances in intrinsic self-healing cementitious materials10.1002/adma.201705679 ↗
24. A review of self-healing concrete for damage management of structures
25. Self-healing of surface cracks in mortars with expansive additive and crystalline additive10.1016/j.cemconcomp.2012.01.005 ↗
26. Performance recovery concerning the permeability of concrete by means of a microcapsule based self-healing system10.1016/j.cemconcomp.2016.12.005 ↗
27. Bacteria based self healing concrete – a review10.1016/j.conbuildmat.2017.07.040 ↗
28. A “fracture testing” based approach to assess crack healing of concrete with and without crystalline admixtures10.1016/j.conbuildmat.2014.07.008 ↗
29. Effect of crystalline admixtures on the self-healing capability of early-age concrete studied by means of permeability and crack closing tests10.1016/j.conbuildmat.2016.03.196 ↗
30. Self-healing capability of concrete with crystalline admixtures in different environments10.1016/j.conbuildmat.2015.03.091 ↗
31. Effect of ion chelating agent on self-healing performance of cement-based materials10.1016/j.conbuildmat.2018.09.115 ↗
32. Measuring the pore structure of cement asphalt mortar by nuclear magnetic resonance10.1016/j.conbuildmat.2017.01.109 ↗
33. The assessment of porosity and pore size distribution of limestone Portland cement pastes10.1016/j.conbuildmat.2008.08.028 ↗
34. Mercury porosimetry: an inappropriate method for the measurement of pore size distributions in cement-based materials10.1016/S0008-8846(00)00370-7 ↗
35. Characterization of pore structure in cement-based materials using pressurization-depressurization cycling mercury intrusion porosimetry (PDC-MIP)10.1016/j.cemconres.2010.02.011 ↗
36. Deicer scaling mechanisms in concrete