journal article·2021-02Open access

Transport mechanisms as indicators of the durability of precast recycled concrete

F. Fiol, C. Thomas, J.M. Manso, I. López

Abstract

ABSTRACT: The objective of this paper was to analyze the influence of crushed precast concrete waste on the transport mechanisms as indicators of the durability of precast recycled self-compacting concrete (SCC) as an alternative to the coarse fraction of natural aggregate. The replacement percentages were 20%, 50% and 100%, by weight, of the silica gravel 2/12.5 mm. Two types of SCC were manufactured: the first with a minimum compressive strength of 30 MPa (HR-30) and the second with a minimum strength of 45 MPa (HR-45). The recycled SCC?s mechanical characteristics such as compressive strength, splitting tensile strength, flexural strength and modulus of elasticity were analyzed. Regarding the physical properties related to transport mechanisms, the influence of the recycled aggregate on the porosity, absorption, penetration of water under pressure, density of hardened concrete and ultrasonic pulse velocity was analyzed. All these properties were compared with those of a control concrete. The results of the mechanical tests provide values close to those obtained for the control SCC, while, in terms of durability the results fulfil the limit values that are considered for a good quality concrete. Therefore, it can be concluded that the use of crushed precast concrete waste with different degrees of substitution is a viable alternative in the manufacture of more sustainable SCC.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Recycled Aggregate Concrete Performance · Municipal Solid Waste Management · Innovations in Concrete and Construction Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. EC-European-Comission, DIRECTIVE 2008/98/EC OF THE EUROPEAN PARLIAMENT AND OF THE COUNCIL of 19 November 2008 on waste and repealing certain Directives (Text with EEA relevance), n.d.
2. BPCA, Precast Sustainability Strategy and Charter. British Precast Concrete Association., (2013).
3. EU, REGULATION (EU) No 305/2011 OF THE EUROPEAN PARLIAMENT AND OF THE COUNCIL of 9 March 2011, Off. J. Eur. Communities. L 269 (2016) 1–15. https://doi.org/2004R0726 - v.7 of 05.06.2013.
4. Fatigue failure micromechanisms in recycled aggregate mortar by μCT analysis10.1016/j.jobe.2019.101027 ↗
5. Durability of recycled aggregate concrete10.1016/j.conbuildmat.2012.11.106 ↗
6. Mechanical performance of concrete made with aggregates from construction and demolition waste recycling plants10.1016/j.jclepro.2015.03.012 ↗
7. Influence of curing conditions on recycled aggregate concrete10.1016/j.conbuildmat.2018.04.009 ↗
8. Concrete with fine recycled aggregates: a review10.1080/19648189.2013.851038 ↗
9. Macro- and micro- properties of multi-recycled aggregate concrete10.1016/j.jclepro.2019.118843 ↗
10. J. Sainz-Aja, C. Thomas, J.A. Polanco, I. Carrascal, High-frequency fatigue testing of recycled aggregate concrete, Appl. Sci. 10 (2020). https://doi.org/10.3390/app1001001010.3390/app10010010 ↗
11. Self-compacting recycled aggregate concrete using out-of-service railway superstructure wastes10.1016/j.jclepro.2019.04.386 ↗
12. Micro- and macro-porosity of dry- and saturated-state recycled aggregate concrete10.1016/j.jclepro.2018.11.243 ↗
13. The influence of recycled aggregates from precast elements on the mechanical properties of structural self-compacting concrete10.1016/j.conbuildmat.2018.06.132 ↗
14. C. Thomas, J. de Brito, V. Gil, J.A. Sainz-Aja, A. Cimentada, Multiple recycled aggregate properties analysed by X-ray microtomography, Constr. Build. Mater. 166 (2018) 171–180. https://doi.org/https://doi.org/10.1016/j.conbuildmat.2018.01.13010.1016/j.conbuildmat.2018.01.130 ↗
15. C. Pellegrino, P. Cavagnis, F. Faleschini, K. Brunelli, Properties of concretes with Black/Oxidizing Electric Arc Furnace slag aggregate, Cem. Concr. Compos. 37 (2013) 232–240. https://doi.org/https://doi.org/10.1016/j.cemconcomp.2012.09.00110.1016/j.cemconcomp.2012.09.001 ↗
16. F. Lopez-Gayarre, Influencia en la variación de los parámetros de dosificación y fabricación de hormigón reciclado estructural sobre las propiedades fisico mecánicas., Universidad Oviedo., 2008
17. J.C. Arroyo Portero, F. Morán Cabré, Á. García Meseguer, Jimenez Montoya. Hormigón Armado., Madrid, 2018.
18. M. Sánchez de Juan, Estudio sobre la utilización de árido reciclado para la fabricación de hormigón estructural., E.T.S.I. Caminos, Canales y Puertos (UPM), 2004.
19. Durability performance of concrete with recycled aggregates from construction and demolitionn waste plants10.1016/j.conbuildmat.2014.12.103 ↗
20. Performance of recycled aggregate concrete monitored by durability indexes10.1016/S0008-8846(01)00653-6 ↗
21. Comparisons of natural and recycled aggregate concretes prepared with the addition of different mineral admixtures10.1016/j.cemconcomp.2011.05.009 ↗
22. M. Martín-Morales, G.M. Cuenca-Moyano, I. Valverde-Espinosa, I. Valverde-Palacios, Effect of recycled aggregate on physical-mechanical properties and durability of vibro-compacted dry-mixed concrete hollow blocks, Constr. Build. Mater. 145 (2017) 303–310. https://doi.org/https://doi.org/10.1016/j.conbuildmat.2017.04.013.10.1016/j.conbuildmat.2017.04.013 ↗
23. Properties of self-compacting concrete prepared with coarse and fine recycled concrete aggregates10.1016/j.cemconcomp.2009.06.005 ↗
24. Properties of self compacting concrete using recycled coarse aggregate10.1016/j.proeng.2013.01.023 ↗
25. Properties of self-compacting concrete prepared with coarse recycled concrete aggregate10.1016/j.conbuildmat.2009.12.029 ↗
26. T. Barroqueiro, P. da Silva, J. Brito, Fresh-State and Mechanical Properties of High-Performance Self-Compacting Concrete with Recycled Aggregates from the Precast Industry, Materials (Basel). 12 (2019). https://doi.org/10.3390/ma1221356510.3390/ma12213565 ↗
27. Use of coarse recycled aggregates from precast concrete rejects: mechanical and durability performance10.1016/j.conbuildmat.2014.08.034 ↗
28. J.Á. Pérez Benedicto, Estudio experimental sobre propiedades mecánicas del hormigón reciclado con áridos procedentes de la no calidad, E.U. de Arquitectura Técnica (UPM), 2011.
29. M. Velay-Lizancos, P. Vazquez-Burgo, D. Restrepo, I. Martinez-Lage, Effect of fine and coarse recycled concrete aggregate on the mechanical behavior of precast reinforced beams: Comparison of FE simulations, theoretical, and experimental results on real scale beams, Constr. Build. Mater. 191 (2018) 1109–1119. https://doi.org/https://doi.org/10.1016/j.conbuildmat.2018.10.075.10.1016/j.conbuildmat.2018.10.075 ↗
30. AENOR, UNE-EN 1097-6. Ensayos para determinar las propiedades mecánicas y físicas de los áridos. Parte 6: Determinación de la densidad de partículas y la absorción de agua, n.d.
31. EHE-08, Instrucción del Hormigón Estructural, (2008).
32. AENOR, UNE-EN 933-1. Ensayos para determinar las propiedades geométricas de los áridos. Parte 1: Determinación de la granulometría de las partículas., n.d.
33. AENOR, Tests for Geometrical Properties of Aggregates—Part 3: Determination of Particle Shape—Flakiness Index; UNE-EN 933-3:2012, 2012.
34. AENOR, Tests for geometrical properties of aggregates - Part 4: Determination of particle shape - Shape index; UNE-EN 933-4:2008, 2008.
35. AENOR, Tests for mechanical and physical properties of aggregates - Part 5: Determination of the water content by drying in a ventilated oven; UNE-EN 1097-5:2009, 2009.
36. AENOR, Tests for chemical properties of aggregates - Part 1: Chemical analysis; UNE-EN 1744-1:2010, 2010.
37. AENOR, Tests for thermal and weathering properties of aggregates - Part 2: Magnesium sulfate test; UNE-EN 1367-2:2010, 2010.
38. AENOR, Aggregates for concrete. Determination of aggregates crushing value; UNE 83112, n.d.
39. C. Thomas, Hormigón reciclado de aplicación estructural : Durabilidad en ambiente marino y comportamiento a fatiga, Universidad de Cantabria, 2010.
40. A. International, ASTM C192/C192M – 18 Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory, 2018.
41. AENOR, Testing fresh concrete - Part 1: Sampling; UNE-EN 12350-1:2009, 2009.
42. AENOR, UNE-EN 12390-2: Ensayos de hormigón endurecido. Parte 2: Fabricación y curado de probetas para ensayos de resistencia, n.d.
43. AENOR, Testing fresh concrete - Part 8: Self-compacting concrete - Slump-flow test; UNE-EN 12350-8:2011, 2011.
44. AENOR, UNE-EN 12390-3. Ensayos de hormigón endurecido. Parte 3: Determinación de la resistencia a compresión de probetas, España, 2003
45. AENOR, Testing hardened concrete - Part 6: Tensile splitting strength of test specimens; UNE-EN 12390-6:2010, 2010.
46. AENOR, Testing hardened concrete - Part 5: Flexural strength of test specimens; UNE-EN 12390-5:2009, 2009.
47. AENOR, Concrete tests. Determination of the Modulus of Elasticity in compression; UNE 83316., 1996.
48. AENOR, Testing fresh concrete - Part 2: Slump-test; UNE-EN 12350-2:2009, 2009.
49. A. International, ASTM C642 - 13; Standard Test Method for Density, Absorption, and Voids in Hardened Concrete, 2013.
50. AENOR, Testing hardened concrete - Part 8: Depth of penetration of water under pressure; UNE-EN 12390-8:2009, 2009.
51. AENOR, UNE-EN 12390-7. Ensayos de hormigón endurecido. Parte 7: Densidad del hormigón endurecido., España, n.d.
52. AENOR, Testing concrete - Part 4: Determination of ultrasonic pulse velocity; UNE-EN 12504-4., 2006.
53. A.M. Neville, J.J. Brooks, Concrete Technology, Longman Scientific & Technical, 1987.
54. Abrams · 1919
55. Influence of recycled concrete aggregates on strength properties of concrete10.1016/j.conbuildmat.2008.06.007 ↗
56. Properties of HPC with recycled aggregates10.1016/j.cemconres.2005.11.022 ↗
57. B. González Fonteboa, Hormigones con áridos reciclados procedentes de demoliciones: Dosificaciones, propiedades mecánicas y comportamiento estructural a cortante, UNIVERSIDADE DA CORUÑA, 2002
58. T. Ikeda, S. Yamame, A. Sakamoto, Strengths of concrete containing Recycled concret aggregate Demolition and Reuse of Concrete Masonry Japan, (1988) 585–594.10.1201/9781003416562-11 ↗
59. M. Sánchez, P. Alaejos, Estudio sobre las propiedades del hormigón fabricado con áridos reciclados, Monografía, CEDEX, Madrid, 2012.
60. M. Etxeberria, E. Vázquez, A. Marí, M. Barra, Influence of amount of recycled coarse aggregates and production process on properties of recycled aggregate concrete, Cem. Concr. Res. 37 (2007) 735–742. https://doi.org/10.1016/J.CEMCONRES.2007.02.00210.1016/j.cemconres.2007.02.002 ↗
61. Comite Euro-International du Bèton, Strategies for Testing and Assessment of Concrete Structures affected by Reinforcement Corrosion., (1988) 184.
62. V. Andrea, Durabilidad en hormigones armados con árido reciclado. Una evaluación de la corrosión en ambiente marino, Universitat Politècnica de València, Valencia, 2012.
63. E.A. Whitehurst, Soniscope tests concrete structures, [Portland Cement Association], Chicago, 1951
64. Structural recycled aggregate concrete made with precast wastes10.1016/j.conbuildmat.2016.03.203 ↗