journal article·2023-06

Early-age properties and shrinkage induced stress of ultra-high-performance concrete under variable temperature and uniaxial restrained condition

Ci Liu, Dejian Shen, Xiao Yang, Haoze Shao, Hongwei Tang, Lili Cai

Publisher page

Abstract

Researches have been continuously carried out on the mechanical properties and control measures on autogenous shrinkage of ultra-high-performance concrete (UHPC), while studies on the stress evolution and cracking behavior of UHPC under variable temperature and uniaxial restrained condition are insufficient. The development of restrained stress is not only closely associated with the elastic modulus and shrinkage, but also affected by creep. In this research, the volume deformation, stress evolution, and cracking behavior of UHPC incorporating steel fibres under variable temperature and uniaxial restrained condition were investigated by using temperature stress test machine, and the autogenous shrinkage, tensile creep, as well as stress relaxation were analyzed. The development of stress was aggravated by the shrinkage caused by the temperature drop and self-desiccation, which eventually resulted in the premature cracking of UHPC without fibres. The autogenous shrinkage of UHPC obtained from the free strain was reduced gradually when the volume proportion of fibres was raised. Incorporating steel fibres significantly reduced the early-age tensile creep of UHPC, and the tensile creep of UHPC changed little when the volume proportion of steel fibres was raised from 1.67% to 2.50%. The combined effect of creep and damage reduced the restrained stress by 77.3%, 76.1%, 76.1%, and 75.1% for UHPC incorporating 0%, 0.83%, 1.67%, and 2.50% volume proportion of steel fibres under the restrained condition, respectively.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete Properties and Behavior · Innovative concrete reinforcement materials · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (99)

Show source-provided references
1. Tensile response of low clinker UHPFRC subjected to fully restrained shrinkage10.1016/j.cemconres.2019.105804 ↗
2. Influence of low curing temperatures on the tensile response of low clinker strain hardening UHPFRC under full restraint10.1016/j.cemconres.2019.105940 ↗
3. ASTM C1856/C1856M-2017 · 2017
4. GB/T 31387-2015, Reactive powder concrete, General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China and Standardization Administration of the People’s Republic China, China, 2015 (in Chinese).
5. Enhancing cracking resistance of ultra-high-performance concrete slabs using steel fibres10.1680/macr.14.00116 ↗
6. Comparative study on the effect of steel and polyoxymethylene fibers on the characteristics of Ultra-High Performance Concrete (UHPC)
7. New development of ultra-high-performance concrete (UHPC)10.1016/j.compositesb.2021.109220 ↗
8. Shrinkage and cracking of restrained ultra-high-performance fiber-reinforced concrete slabs at early age10.1016/j.conbuildmat.2014.09.097 ↗
9. Pullout and flexural performance of silane groups and hydrophilic groups grafted polypropylene fibre reinforced UHPC10.1016/j.conbuildmat.2021.122335 ↗
10. Evaluation and regulation of ultra-high performance concrete (UHPC) crack resistance based on physicochemical multi-factor coupling approach10.1016/j.conbuildmat.2021.124100 ↗
11. Effects of saturated lightweight sand content on key characteristics of ultra-high-performance concrete10.1016/j.cemconres.2017.08.018 ↗
12. Early age autogenous shrinkage cracking risk of an ultra-high performance concrete (UHPC) wall: modelling and experimental results10.1016/j.engfracmech.2021.108024 ↗
13. Shrinkage mitigation of an ultra-high performance concrete submitted to various mixing and curing conditions10.3390/ma14143982 ↗
14. Evaluation method for cracking resistant behavior of reactive powder concrete10.1016/j.conbuildmat.2011.08.060 ↗
15. Early-age autogenous shrinkage, tensile creep, and restrained cracking behavior of ultra-high-performance concrete incorporating polypropylene fibers10.1016/j.cemconcomp.2023.104948 ↗
16. Shrinkage properties of ultra-high performance concrete (UHPC)10.1166/asl.2011.1505 ↗
17. Partial substitution of silica fume with fine glass powder in UHPC: Filling the micro gap10.1016/j.conbuildmat.2017.02.084 ↗
18. Mechanical and fracture mechanics properties of ultra-high-performance concrete10.1016/j.conbuildmat.2019.03.298 ↗
19. Internal curing by superabsorbent polymers in ultra-high performance concrete10.1016/j.cemconres.2015.05.005 ↗
20. Investigation of mechanical properties and shrinkage of ultra-high performance concrete: Influence of steel fiber content and shape10.1016/j.compositesb.2019.107021 ↗
21. Effect of polypropylene fiber on early-age properties and stress relaxation of ultra-high-performance concrete under different degrees of restraint
22. Restrained shrinkage behavior of internally-cured UHPC using calcined bauxite aggregate in the ring test and UHPC-concrete composite slab10.1016/j.cemconcomp.2022.104805 ↗
23. Tensile response of ultra high performance PE fiber reinforced concretes (PE-UHPFRC) under imposed shrinkage deformations10.1617/s11527-021-01621-0 ↗
24. Mechanisms of autogenous shrinkage for Ultra-High Performance Concrete (UHPC) prepared with pre-wet porous fine aggregate (PFA)
25. Experimental study and theoretical prediction on shrinkage-induced restrained stresses in UHPC-RC composites under normal curing and steam curing10.1016/j.cemconcomp.2020.103602 ↗
26. Effects of fibers on the mechanical properties of UHPC: A review
27. Relationship between flowability, entrapped air content and strength of UHPC mixtures containing different dosage of steel fiber10.3390/app6080216 ↗
28. Effects of steel fiber content and shape on mechanical properties of ultra high performance concrete10.1016/j.conbuildmat.2015.11.028 ↗
29. Energy absorption capacity of a sustainable Ultra-High Performance Fibre Reinforced Concrete (UHPFRC) in quasi-static mode and under high velocity projectile impact10.1016/j.cemconcomp.2016.02.012 ↗
30. Effect of hybrid fibers on fresh properties, mechanical properties, and autogenous shrinkage of cost-effective UHPC10.1061/(ASCE)MT.1943-5533.0002212 ↗
31. Experimental investigation on the autogenous shrinkage of steam cured ultra-high performance concrete10.1016/j.conbuildmat.2017.11.172 ↗
32. Study on autogenous shrinkage characteristic and mechanism of ultra-high performance cementitous composite
33. Effect of undercalcined MgO and hybrid fiber on the autogenous shrinkage of reactive powder concrete
34. Early-age autogenous shrinkage and tensile creep of hooked-end steel fiber reinforced concrete with different thermal treatment temperatures10.1016/j.cemconcomp.2022.104550 ↗
35. B.A. Graybeal. Material property characterization of ultra-high performance concrete (NO. FHWA-HRT-06-103), 2006.
36. Short-term tensile creep and shrinkage of ultra-high performance concrete10.1016/j.cemconcomp.2009.01.002 ↗
37. Experimental studies and modeling of creep of UHPC10.1016/j.conbuildmat.2018.04.157 ↗
38. Creep of UHPC in tension and compression: Effect of thermal treatment10.1016/j.cemconcomp.2011.12.002 ↗
39. Time-dependent properties of ultrahigh-performance concrete: compressive creep and shrinkage10.1061/(ASCE)MT.1943-5533.0004219 ↗
40. Effects of type and content of fibers, water-to-cement ratio, and cementitious materials on the shrinkage and creep of ultra-high performance concrete10.3390/polym14101956 ↗
41. UHPFRC tensile creep at early age10.1617/s11527-008-9371-0 ↗
42. Advanced techniques for the study of shrinkage-induced cracking of concrete with recycled aggregates at early age10.1016/j.conbuildmat.2019.117340 ↗
43. Restrained cracking failure behavior of concrete containing MgO compound expansive agent under adiabatic condition at early age
44. Concrete thermal failure criteria, test method, and mechanism: A review10.1016/j.conbuildmat.2021.122762 ↗
45. Investigation on the internal relative humidity of superabsorbent polymer–modified concrete exposed to various ambient humidities at early age10.1061/(ASCE)MT.1943-5533.0004708 ↗
46. The cracking risk of hardening concrete exposed to realistic curing temperature regimes and restraint conditions – Experimental investigations of important parameters10.1016/j.conbuildmat.2022.127662 ↗
47. Effect of shrinkage-reducing polycarboxylate admixture on cracking behavior of ultra-high strength mortar10.1016/j.cemconcomp.2021.104117 ↗
48. Properties of early-age concrete relevant to cracking in massive concrete10.1016/j.cemconres.2019.05.015 ↗
49. Early-age cracking risk and relaxation by restrained autogenous deformation of ultra high performance concrete
50. New results on early-age cracking risk of special concrete10.1520/CCA12304 ↗
51. K. Habel, J.P. Charron, E. Denarié, E. Brühwiler, Autogenous deformations and viscoelasticity of UHPFRC in structures. Part I: experimental results, Mag. Concr. Res. 58 (3) (2006) 135-145. https://doi.org/10.1680/macr.2006.58.3.135.10.1680/macr.2006.58.3.135 ↗
52. Thermo-mechanical response of UHPFRC at early age — Experimental study and numerical simulation10.1016/j.cemconres.2008.01.009 ↗
53. Ultra-high-performance fiber-reinforced concrete: shrinkage strain development at early ages and potential for cracking10.1520/JTE20160114 ↗
54. Effect of polyvinyl alcohol fiber on the cracking risk of high strength concrete under uniaxial restrained condition at early age10.1016/j.conbuildmat.2021.124206 ↗
55. Cracking behavior of ultra-high strength mortar with CaO-based expansive agent and superabsorbent polymer10.1016/j.conbuildmat.2022.129281 ↗
56. T/CBMF37-2018/T/CCPA7-2018, Fundamental characteristics and test methods of ultra-high performance concrete, China Building Materials Federation and China Concrete & Cement-based Products Association, China, 2018 (in Chinese).
57. GB/T 50080-2016, Standard for test method of performance on ordinary fresh concrete, Ministry of Housing and Urban-Rural Development of the People’s Republic of China and General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China, China, 2016 (in Chinese).
58. GB/T 2419-2005, Test method for fluidity of cement mortar. General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China and Standardization Administration of the People’s Republic China, China, 2005 (in Chinese).
59. Rheology of fiber reinforced cementitious materials: classification and prediction10.1016/j.cemconres.2009.08.032 ↗
60. GB/T 50081-2019, Standard for Test Methods of Concrete Physical and Mechanical Properties, Ministry of Housing and Urban-Rural Development of the People’s Republic of China and State Administration for Market Regulation, China, 2019 (in Chinese).
61. Effect of different fiber combinations and optimisation of an ultra-high performance concrete (UHPC) mix applicable in structural elements10.1016/j.conbuildmat.2021.125777 ↗
62. T/CECS 10107-2020, Technical requirements for ultra high performance concrete, China Association for Engineering Construction Standardization, China, 2020 (in Chinese).
63. Evaluation of behavior and cracking potential of early-age cementitious systems using uniaxial restraint tests: A review10.1016/j.conbuildmat.2019.117146 ↗
64. Testing system for determining the mechanical behaviour of early age concrete under restrained and free uniaxial shrinkage10.1007/BF02473424 ↗
65. Size effect of ultra-high-performance concrete under compression: effects of steel fiber characteristics and water-to-binder ratio10.1016/j.conbuildmat.2022.127170 ↗
66. Exploring mechanical and durability properties of ultra-high performance concrete incorporating various steel fiber lengths and dosages10.1016/j.conbuildmat.2014.11.017 ↗
67. Evaluation of modulus of elasticity of ultra-high performance concrete10.1016/j.conbuildmat.2017.07.158 ↗
68. Material and bond properties of ultra high performance fiber reinforced concrete with micro steel fibers10.1016/j.compositesb.2013.10.081 ↗
69. Effect of curing, fibre content and exposures on compressive strength and elasticity of UHPC10.1680/adcr.13.00090 ↗
70. Experimental test methods to determine the uniaxial tensile and compressive behaviour of ultra high performance fibre reinforced concrete (UHPFRC)10.1016/j.conbuildmat.2012.04.030 ↗
71. Tensile behavior of ultra high performance hybrid fiber reinforced concrete10.1016/j.cemconcomp.2011.09.009 ↗
72. Tensile characteristics of ultra-high-performance concrete10.1680/jmacr.17.00126 ↗
73. Thermal deformation and stress of alkali-activated slag concrete under semi-adiabatic condition: Experiments and simulations10.1016/j.cemconres.2022.106887 ↗
74. fib, fib Model Code for Concrete Structures 2010, Wilhelm Ernst & Sohn, Berlin, Germany, 2013.10.1002/9783433604090 ↗
75. Determination of time-zero and its effect on autogenous deformation evolution10.1080/19648189.2011.9695290 ↗
76. Time-zero and deformational characteristics of high performance concrete with and without superabsorbent polymers at early ages10.1016/j.conbuildmat.2020.120262 ↗
77. G. Sant, P. Lura, J. Weiss, A discussion of analysis approaches for determining ‘time-zero’ from chemical shrinkage and autogenous strain measurements in cement paste, Proceedings of international RILEM conference on Volume Changes of Hardening Concrete: Testing and Mitigation, 2006, pp. 20-23.10.1617/2351580052.040 ↗
78. Effects of SAP characteristics on internal curing of UHPC matrix10.1016/j.conbuildmat.2021.122530 ↗
79. Effect of temperature history and restraint degree on cracking behavior of early-age concrete10.1016/j.conbuildmat.2018.10.066 ↗
80. Influence of ground granulated blast furnace slag on the early-age anti-cracking property of internally cured concrete10.1016/j.conbuildmat.2019.06.149 ↗
81. Effects of shrinkage reducing admixture and wollastonite microfiber on early-age behavior of ultra-high performance concrete10.1016/j.cemconcomp.2013.11.008 ↗
82. Nano-engineered ultra-high performance concrete for controlled autogenous shrinkage using nanocellulose10.1016/j.cemconres.2020.106217 ↗
83. Influence of Barchip fiber length on early-age behavior and cracking resistance of concrete internally cured with super absorbent polymers10.1016/j.conbuildmat.2019.03.209 ↗
84. Experimental study on the relationship between shrinkage and interior humidity of concrete at early age10.1680/macr.2010.62.3.191 ↗
85. Effect of internal curing with super absorbent polymers on autogenous shrinkage of concrete at early age10.1016/j.conbuildmat.2015.12.115 ↗
86. Estimation of temperature effects on autogenous shrinkage of concrete by a new prediction model10.1016/j.conbuildmat.2012.03.005 ↗
87. Improving test methods to measure early age autogenous shrinkage in concrete based on air cooling, IES
88. Utilization of natural sisal fibers to manufacture eco-friendly ultra-high performance concrete with low autogenous shrinkage10.1016/j.jclepro.2021.130105 ↗
89. Factors contributing to early age shrinkage cracking of slag concretes subjected to 7-days moist curing10.1617/s11527-007-9269-2 ↗
90. Tensile creep behavior of high strength concretes at early ages10.1007/BF02479631 ↗
91. Tensile creep and cracking resistance of concrete with different water-to-cement ratios at early age10.1016/j.conbuildmat.2017.04.056 ↗
92. Creep at early ages of ultrahigh-strength concrete: experiment and modelling10.1680/jmacr.17.00551 ↗
93. Cracking failure behavior of high strength concrete containing nano-CaCO3 at early age
94. Effect of fiber types on creep behavior of concrete10.1016/j.conbuildmat.2015.12.149 ↗
95. Early age setting, shrinkage and tensile characteristics of ultra high performance fiber reinforced concrete10.1016/j.conbuildmat.2012.12.015 ↗
96. Maturity computer for controlled curing and hardening of concrete
97. Comparison of thermal cracking potential evaluation criteria for mass concrete structures10.1617/s11527-021-01840-5 ↗
98. The practical application of a self-developed temperature stress testing machine in development of expansive concrete blended with calcium sulfoaluminate additives10.1016/j.cemconres.2022.107045 ↗
99. Stress prediction in very early-age concrete subject to restraint under varying temperature histories10.1016/j.cemconcomp.2017.07.006 ↗