Microstructure, deformation and durability of high-strength non-steam-cured concrete with C-S-H seed
Source abstract
Abstract
The effect of the early strength agent named calcium silicate hydrate polycarboxylate ether nanocomposite (C-S-H seed), fly ash and slag on the development of microstructure, autogenous deformation and durability, as well as the mechanism of interaction between microscopic (e.g., pore structure) and macroscopic properties of concrete, were investigated. Results showed that C-S-H seed increased the compressive strength of concrete before 7 d. The addition of C-S-H seed decreased both relative humidity and capillary pore diameter due to rapid hydration, which resulted in high negative capillary pressure and autogenous deformation of up to 40%. The higher fly ash and slag contents decreased early-age autogenous deformation. Further analysis showed that the addition of C-S-H seed decreased the percentage of pores>1000 nm and the most probable pore diameter of concrete, thus increasing resistance to chloride migration into concrete. The chloride diffusion coefficient was linearly related to the amount of cementitious material together with the water-to-binder ratio. The C-S-H seed decreased the availability of pores of critical diameter (14 nm) of concrete exposed to water freezing, leading to an increase in the freeze–thaw resistance of concrete. In addition, the C-S-H seed also reduced the overall porosity of concrete, leading to an increase in resistance to sulfate attack. Similar trends were observed for increased fly ash and slag content. Besides, the concentrations of AP and Ca 2+ significantly affected sulfate resistance.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. Durability and microstructure of steam cured and autoclaved PHC pipe piles10.1016/j.conbuildmat.2019.03.166 ↗
2. Performance evaluation of steam cured HPC pipe piles produced with metakaolin based mineral additives10.1016/j.conbuildmat.2018.09.044 ↗
3. Effect of ground quartz sand on properties of high-strength concrete in the steam-autoclaved curing10.1016/S0008-8846(00)00395-1 ↗
4. Z. Qi, F. Liu, M. Deng, J. Hu, Research on cleaner production potential of pipe pile industry based on material energy flow analysis, IOP Conference Series: Earth and Environmental Science, IOP Publishing, 2021, p. 012161.10.1088/1755-1315/621/1/012161 ↗
5. Improving the energy efficiency in buildings while reducing the waste using autoclaved aerated concrete made from power industry waste10.1016/j.enbuild.2012.10.029 ↗
6. Energy-efficient algorithms of the steam curing for the in situ production of precast concrete members10.1016/j.enbuild.2013.05.019 ↗
7. Evaluation Method and Mitigation Strategies for Shrinkage Cracking of Modern Concrete10.1016/j.eng.2021.01.006 ↗
8. Effects of steam curing on strength and porous structure of concrete with low water/binder ratio10.1016/j.conbuildmat.2010.06.049 ↗
9. Steam-cured concrete incorporating mineral admixtures10.1016/S0008-8846(02)01028-1 ↗
10. Zhang · 2014 · 996
11. Mechanical strength and hydration exothermic behavior of cemented paste backfill with early-strength agent under low temperature
12. Experimental study on selection of early-strength agent for low-strength cementitious materials prepared with manganese tailings10.1007/s12665-018-7415-5 ↗
13. Effect of triisopropanolamine on compressive strength and hydration of cement-fly ash paste10.1016/j.conbuildmat.2018.05.117 ↗
14. Synergistic use of sodium bicarbonate and aluminum sulfate to enhance the hydration and hardening properties of Portland cement paste10.1016/j.conbuildmat.2021.124248 ↗
15. Chloride erosion resistance of calcium formate incorporated cement mortar under chloride attack10.1016/j.conbuildmat.2021.125611 ↗
16. Effect of triethanolamine on cement hydration toward initial setting time10.1016/j.conbuildmat.2017.02.072 ↗
17. Effect of calcium silicate hydrate–polycarboxylate ether (CSH–PCE) nanocomposite as accelerating admixture on early strength enhancement of slag and calcined clay blended cements10.1016/j.cemconres.2019.01.007 ↗
18. F.b. Zou, C.L. Hu, F.z. Wang, Enhancement of early-age strength of the high content fly ash blended cement paste by sodium sulfate and C–S–H seeds towards a greener binder - ScienceDirect, Journal of Cleaner Production 244 (2020) 118566.10.1016/j.jclepro.2019.118566 ↗
19. Effect of calcium silicate hydrate – polycarboxylate ether (C-S-H–PCE) nanocomposite as accelerating admixture on early strength enhancement of slag and calcined clay blended cements10.1016/j.cemconres.2019.01.007 ↗
20. Acceleration effect of synthesised calcium silicate hydrate with different morphologies and Ca/Si on cement hydration10.1680/jadcr.18.00016 ↗
21. Microstructure development and autogenous shrinkage of mortars with C-S-H seeding and internal curing, Cement and Concrete Research 129 (2020) 105967-.10.1016/j.cemconres.2019.105967 ↗
22. Enhanced performances of cement and powder silane based waterproof mortar modified by nucleation CSH seed10.1016/j.conbuildmat.2020.118511 ↗
23. Effect of CS-Hs-PCE and sodium sulfate on the hydration kinetics and mechanical properties of cement paste10.1016/j.conbuildmat.2020.121096 ↗
24. Microstructure development and autogenous shrinkage of mortars with CSH seeding and internal curing10.1016/j.cemconres.2019.105967 ↗
25. Influences of limestone powder on the resistance of concretes to the chloride ion penetration and sulfate attack10.1016/j.powtec.2018.07.041 ↗
26. Review on the deterioration and approaches to enhance the durability of concrete in the freeze–thaw environment10.1016/j.conbuildmat.2022.126371 ↗
27. Effect of C-S–H seed/PCE nanocomposites and triisopropanolamine on portland cement properties: Hydration kinetic and strength10.1016/j.jobe.2022.104946 ↗
28. Properties evolution of cement-metakaolin system with CSH/PCE nanocomposites10.1016/j.conbuildmat.2021.122707 ↗
29. Fly ash and slag10.1016/j.cemconres.2019.105826 ↗
30. Mechanical and durability properties of sustainable self-compacting concrete with recycled concrete aggregate and fly ash, slag and silica fume10.1016/j.conbuildmat.2019.117115 ↗
31. H Yan, B Yang, Y. Yang, A hydrated calcium silicate early strength agent and its preparation method [P], Chinese patent: CN 112979205 A, 2021 06 18.
32. Effect of nCSH-PCE and slag powder on the autogenous shrinkage of high-strength steam-free pipe pile concrete10.1016/j.conbuildmat.2022.126815 ↗
33. Influence of Elevated Temperatures and Cooling Method on the Microstructure Development and Phase Evolution of Alkali-Activated Slag10.3390/ma15062022 ↗
34. Effect of autogenous deformation on the cracking risk of slag cement concretes10.1016/j.cemconcomp.2010.12.003 ↗
35. Experimental and theoretical analysis on coupled effect of hydration, temperature and humidity in early-age cement-based materials10.1016/j.ijheatmasstransfer.2019.118784 ↗
36. Investigation of moisture transport in cement-based materials using low-field nuclear magnetic resonance imaging10.1680/jmacr.19.00211 ↗
37. Evolution of distribution and content of water in cement paste by low field nuclear magnetic resonance10.1007/s11771-013-1591-y ↗
38. 64–2019 Interpretation of technical requirements for autoclave free production of prestressed high strength concrete pipe piles
39. Mechanical properties of recycled coarse aggregate concrete with different quality and the fitting of bolomi formula
40. Effectiveness of a calcium silicate hydrate–Polycarboxylate ether (CSH–PCE) nanocomposite on early strength development of fly ash cement10.1016/j.conbuildmat.2018.01.053 ↗
41. A review of the impact of micro-and nanoparticles on freeze-thaw durability of hardened concrete: Mechanism perspective10.1016/j.conbuildmat.2018.08.029 ↗
42. Study on the durability and failure mechanism of concrete modified with nanoparticles and polypropylene fiber under freeze-thaw cycles and sulfate attack10.1016/j.coldregions.2021.103301 ↗
43. Experimental investigations on the effects of ambient freeze-thaw cycling on dynamic properties and rock pore structure deterioration of sandstone10.1016/j.coldregions.2018.06.015 ↗
44. Robust evaluation of superabsorbent polymers as an internal curing agent in cementitious composites10.1007/s10853-020-05131-2 ↗
45. Effects of a novel polymer-type shrinkage-reducing admixture on early age microstructure evolution and transport properties of cement pastes10.1016/j.cemconcomp.2018.10.011 ↗
46. Thermodynamic limitation of self-desiccation10.1016/0008-8846(94)00123-G ↗
47. Influence of temperature on autogenous deformation and relative humidity change in hardening cement paste10.1016/S0008-8846(99)00021-6 ↗
48. On the action of capillary pressure in fresh concrete10.1016/0008-8846(76)90050-8 ↗
49. Capillary pressure in fresh cement-based materials and identification of the air entry value10.1016/j.cemconcomp.2008.03.002 ↗
50. Effects of novel polymer-type shrinkage-reducing admixture on early age autogenous deformation of cement pastes10.1016/j.cemconres.2017.08.007 ↗
51. Study on prediction of concrete service life I-theoretical model
52. Enhancing the reliability of evaluating chloride ingress in concrete using the ASTM C 1202 rapid chloride penetrability test10.1520/JAI13403 ↗
53. Effect of magnesia expansion agent with different activity on mechanical property, autogenous shrinkage and durability of concrete10.1016/j.conbuildmat.2022.127506 ↗
54. Durability characteristics of fly ash concrete containing lightly-burnt MgO10.1016/j.conbuildmat.2014.01.080 ↗
55. D.J. Janssen, M.B. Snyder, Resistance of concrete to freezing and thawing, 1994.
56. Studies on frozen ground of China10.1007/BF02837484 ↗
57. A working hypothesis for further studies of frost resistance of concrete
58. Theory of volume changes in hardened portland-cement paste during freezing
59. Crystallization in pores10.1016/S0008-8846(99)00002-2 ↗
60. Influence of freezing rate on the cryo-deformation and cryo-damage of cement-based materials during freezing-thaw cycles
61. Study on the freezing temperature of saline soil10.1007/s11440-017-0537-1 ↗
62. Current knowledge of external sulfate attack10.1680/adcr.14.00089 ↗
63. Numerical simulation of cementitious materials degradation under external sulfate attack10.1016/j.cemconcomp.2009.12.005 ↗
64. Chemo-mechanical analysis of concrete cracking and degradation due to external sulfate attack: A meso-scale model10.1016/j.cemconcomp.2010.12.001 ↗
65. Effect of interfacial transition zone on the transport of sulfate ions in concrete10.1016/j.conbuildmat.2018.10.140 ↗
66. Taylor · 1997
67. Modeling the effects of solution temperature and concentration during sulfate attack on cement mortars10.1016/S0008-8846(01)00727-X ↗