Compression failure mechanism in small scale timber specimens
Source abstract
Abstract
Understanding the failure mechanism of wood loaded in compression parallel to the grain has been shown to be an important parameter in the design of timber beams strengthened with fibre-reinforced plastics (FRP). In this paper, a constitutive relationship for wood under uniaxial compression load parallel to the grain was determined experimentally. Several parameters, such as silviculture, moisture content and radial position in the log in relation to the pith from where the specimen was sawn, were considered. Small clear-wood specimens were used. The strain localisation in the failure region (kinkband) was monitored using the digital image correlation method. The results show that silviculture and moisture content are two very important parameters which influence the compression failure mechanism. Furthermore, there is a significant difference in behaviour between specimens from the juvenile region of the log and specimens from mature wood. Based on experimental results, two numerical models were built, considering either a global or a local constitutive relationship. It was demonstrated that both numerical models yield accurate results and that, depending on the experimental equipment available, a constitutive relationship could be extracted and used as input in these numerical models. (C) 2013 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Mechanical Behavior of Composites · Natural Fiber Reinforced Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. André A, Kliger R. Strengthening of timber beams using FRP, with emphasis on compression strength: a state of the art review. In: Proceedings of the Asia–Pacific conference on FRP in structures 2009 (APFIS 2009), Seoul, South Korea.
2. Kliger R, Al-Emrani M, Johansson M, Crocetti R. Strengthening glulam beams with steel and composite plates. In: Proceedings of the Asia–Pacific conference on FRP in structures 2007 (APFIS 2007), Hong Kong, China, p. 291–296.
3. André A. Benefits of strengthening timber with fibre-reinforced polymers. PhD Thesis. Department of Civil and Environmental Engineering, Chalmers University of Technology, Sweden; 2011.
4. Ductile design of glued-laminated timber beams10.1061/(ASCE)1084-0680(2009)14:3(113) ↗
5. American National Standard for Wood Products. Structural glued laminated timber. ANSI A190.1-2002. American National Standards Institute.
6. Compression failure mechanism in small-scale wood specimens reinforced with CFRP: an experimental study10.1016/j.conbuildmat.2012.12.038 ↗
7. Phenomena of fracture in wood10.1515/hfsg.1963.17.3.65 ↗
8. Poulsen JS. Compression in clear wood. PhD Thesis, Department of Structural Engineering and Materials, Series R, No. 39, Lyngby, Denmark; 1998.
9. On the axial propagation of kinkbands in fibre composites: part I experiments10.1016/S0020-7683(98)00029-8 ↗
10. Mechanics of composite strengthening
11. Fracture of composite10.1016/B978-0-12-341801-2.50007-2 ↗
12. Micromechanics10.1016/0045-7949(83)90141-4 ↗
13. Compressive failure of laminated and woven composites10.1520/CTR10485J ↗
14. Kinkband formation in wood and fibre composites – morphology and analysis10.1016/S0020-7683(02)00174-9 ↗
15. Predictions of compressive strength and kink band orientation for wood species10.1016/j.mechmat.2009.11.015 ↗
16. Compressive failure of fibre composites10.1016/0022-5096(93)90068-Q ↗
17. Kinkband formation in wood species under compressive loading10.1007/s11340-007-9098-9 ↗
18. Johansson G, Johansson M, Kliger R, Perstorper M. Fuktberoende formändringar hos byggnadsvirke – Inverkan av råvaruegenskaper., ISSN 0534-0411, Chalmers University of Technology, 1999 [in Swedish].
19. Hoffmeyer P. Failure of wood as influenced by moisture and duration of load. PhD Thesis, State University of New York, Syracuse, New York, 1990.
20. GOM Optical Measuring Techniques. ARAMIS user manual, ARAMIS 5M v6.3.0. Gesellschaft für Optische Messtechnik (GOM), 2010.
21. Accurate characterization of machine compliance for simple compression testing10.1007/BF02317861 ↗
22. Dassault Systèmes Simulia Corp. Abaqus User’s Manual, 2009. Version 6.9.
23. Glos P. Timber Engineering Step 1, Lecture A7 – Solid timber – Strength classes, 1995.
24. Prediction of elastic parameters for wood
25. Kretschmann DE, Moody RC, Pellerin RF, Bendtsen BA, Cahill JM, McAlister RH, Sharp DW. Effect of various proportions of juvenile wood on laminated veneer lumber. Res. Pap. FPL-RP-521. Madison, WI: US Department of Agriculture, Forest Service, Forest Products Laboratory; 1993.