Internal curing effect on strength of recycled concrete and its enhancement in concrete-filled thin-wall steel tube
Source abstract
Abstract
Abstract This paper investigates the efficiency of basic internal curing provided by waste clay brick in concrete and extra internal curing provided by steel tube restraint. Five different replacement proportions of normal aggregate (NA) by recycled brick aggregate (RBA) and Eight different concrete filled in thin-wall steel tube (CFTST) columns with and without the RBA are examined and evaluated with respect to measured axial compression strength development. Results show that the proportion of compressive strengths in the later curing period to that in the whole period is gradually increased with the RBA. The 28-day internal curing effect of RAC with all RBA reaches to 39.6% compressive strength. Under the premise of ensuring the performance of RAC and as much as possible the use of RBA, the replacement rate of RBA between 40% and 60% by volume is suitable for RBA to product RAC. The confinement effect of steel tube to normal concrete or RAC reaches to 16.5% and 8.0%, and the extra internal curing effect of steel tube to RAC reaches to 12% and 6.5% for stub columns and intermediate length columns respectively. Finally, based on the internal curing effect, a modified formula for bearing capacity of composite columns is proposed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Recycled Aggregate Concrete Performance · Structural Behavior of Reinforced Concrete · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Properties evaluation of concrete using local used bricks as coarse aggregate10.4236/eng.2014.65025 ↗
2. Analysis of regression for strength index of concrete performed brick masonry
3. M Spisakova, M Kozlovska, Deconstruction of buildings-Sustainable ways of construction, In: Proceedings of the 13th International Multidisciplinary Scientific Geoconference: Energy and Clean Technologies, Albena, Bulgaria, June (2013) 16-22.10.5593/SGEM2013/BD4/S18.006 ↗
4. Properties of concrete using crushed brick as aggregate
5. Properties of concrete using crushed clinker brick as coarse aggregate
6. Crushed bricks as coarse aggregate for concrete
7. Use of recycled brick masonry aggregate and recycled brick masonry aggregate concrete in sustainable construction
8. Reactivity of crushed clay brick aggregate10.1016/j.conbuildmat.2013.11.014 ↗
9. Valorization of brick wastes in the fabrication of concrete blocks10.17222/mit.2015.202 ↗
10. Performance evaluation of a resinous cement mortar modified with crushed clay brick and tire rubber aggregate10.1016/j.conbuildmat.2016.05.119 ↗
11. Experimental research of concrete floor blocks with crushed bricks and tiles aggregate10.1016/j.conbuildmat.2015.07.163 ↗
12. Strength and ductility of confined concrete10.1061/(ASCE)0733-9445(1992)118:6(1590) ↗
13. Confined concrete-filled tubular columns10.1061/(ASCE)0733-9445(2005)131:3(488) ↗
14. Recycled concrete as an aggregate for concrete-a review
15. Study on the influence of attached mortar content on the properties of recycled concrete aggregate10.1016/j.conbuildmat.2008.04.012 ↗
16. Recycling and reuse of construction and demolition waste in concrete-filled steel tubes: A review10.1016/j.conbuildmat.2016.09.063 ↗
17. Combined strength of lightweight aggregate concrete-filled steel tube
18. Stability behavior of lightweight aggregate concrete filled steel tubular columns under axial compression
19. Behavior of lightweight aggregate concrete filled steel tubular slender column under axial compression
20. Failure of lightweight aggregate concrete-filled steel tubular columns10.12989/scs.2004.4.1.001 ↗
21. Direct tensile strength of lightweight concrete with different specimen depths and aggregate sizes10.1016/j.conbuildmat.2014.04.055 ↗
22. Shrinkage cracking of lightweight concrete made with cold-bonded fly ash aggregate10.1016/j.cemconres.2003.11.024 ↗
23. Internal curing of high-performance concrete with pre-soaked fine lightweight aggregate for prevention of autogenous shrinkage cracking10.1016/j.cemconres.2008.02.001 ↗
24. Evaluation of the influence of specific surface treatments of RBA on a set of properties of concrete10.3390/ma9030156 ↗
25. Prevention of autogenous shrinkage in high strength concrete by internal curing using wet lightweight aggregates10.1016/S0008-8846(01)00608-1 ↗
26. Influence of cement paste matrix properties on the autogenous curing of high-performance concrete10.1016/S0958-9465(03)00082-9 ↗
27. Effect of saturated lightweight sand substitution on shrinkage in 0.35 w/b concrete
28. Internal curing of high-performance blended cement mortars
29. Influence of ground waste clay brick on properties of fresh and hardened concrete10.1016/j.conbuildmat.2015.08.100 ↗
30. JGJ 52-2006, Standard and inspection method of normal concrete with gravel or pebble quality, Beijing: Chinese standards Institution, 1992 (BS EN 772-3, Methods of test for masonry units - Part3: Determination of net volume and percentage of voids of clay masonry units by hydrostatic weighing, London: British Standards Institution, 1998).
31. GB/T 17431.2-2010, Lightweight Aggregates and Its Test Methods II: Lightweight Aggregates Test Methods, Beijing: Chinese standards Institution, 2011 (BS 1881-122, Testing concrete - Method for determination of water absorption, London: British Standards Institution, 1983).
32. Influence of natural aggregates typology on recycled concrete strength properties10.1016/j.conbuildmat.2016.04.037 ↗
33. Effect of different types of aggregates on the performance of concrete-filled steel tubular stub columns10.1617/s11527-015-0742-z ↗
34. Finite element modelling of concrete-filled steel stub columns under axial compression10.1016/j.jcsr.2013.07.001 ↗
35. GB/T 50081-2002, Standard for Test Method of Mechanical Properties of Normal Concrete, Beijing: Chinese standards Institution, 2002 (BS EN 12390-3, Testing hardened concrete - Part 3: Compressive strength of test specimens, London: British Standards Institution, 2009).
36. Use of porous ceramic waste aggregates for internal curing of high-performance concrete10.1016/j.cemconres.2009.01.007 ↗
37. GB 50010-2010, Code for concrete structures design, Beijing: Chinese standards Institution, 2010 (BS EN 1992-1-1, Design of concrete structures - General rules and rules for buildings, London: British Standards Institution, 2004).
38. Behavior of concrete-filled steel tubular stub columns and beams using dune sand as part of fine aggregate10.1016/j.conbuildmat.2013.10.049 ↗
39. Nonlinear analysis on concrete-filled rectangular tubular composite columns10.12989/sem.2000.10.6.577 ↗
40. AISC-LRFD · 1999
41. AIJ-CFT · 1997
42. BS 5400, Steel, concrete and composite bridges - Part 5: code of practice for design of composite bridge, London: British Standards Institution, 2005.
43. Flexural behaviour of concrete-filled steel tubes10.1016/j.jcsr.2003.08.009 ↗
44. Mechanical properties of confined recycled aggregate concrete under axial compression10.1016/j.conbuildmat.2011.06.062 ↗
45. Material and structural response of steel tube confined recycled earthquake waste concrete subjected to axial compression10.1680/jmacr.14.00357 ↗