Abrasion resistance and mechanical strength of underwater repair concrete curing under hydrostatic pressure
Source abstract
Abstract
Damages of hydraulic concrete structures caused by erosion are a significant repair problem. Modern concrete enables performing the repair works without using the so-called dry dock. The repairs are often carried out at great depth. A special container, which could simulate placing and curing concrete under hydrostatic pressure, was used to study the concreting depth’s influence on the concrete’s future abrasion resistance. Two compositions of the underwater repair concrete were tested. The maximum grains size was 8 and 16 mm. Also, a viscosity-modifying admixture was used. The designed composites met the standard requirements in maintaining consistency in time and limiting the wash-out losses. The concrete specimens, taken for testing the abrasive resistance and compressive strength, were initially cured in the container for 28 days under pressure from 0 to 0.5 MPa. The pressure range corresponds to curing the concrete at a depth of up to 50 m. The abrasion tests were conducted using Böhme’s disk. The results show that the hydrostatic pressure does not negatively affect the strength and abrasion resistance of the underwater concrete. The abrasion resistance is not directly related to compressive strength. It has been observed that the higher is hydrostatic pressure, the higher is abrasion resistance of the concrete’s top layer compared to the bottom layer. The hydrostatic pressure acting when placing and curing the concrete mix causes releasing the bigger air voids. Therefore, the specimens taken from the top layer are less porous, which was confirmed by testing the apparent density.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. 2016
2. Mathematical model of abrasive wear of high performance concrete10.1016/j.wear.2006.12.008 ↗
3. High-Speed Flow Erosion on a New Roller Compacted Concrete Dam During Construction10.1016/S1001-6058(11)60216-3 ↗
4. Experimental Study on the Mechanism of the Combined Action of Cavitation Erosion and Abrasion at High Speed Flow10.1186/s40069-019-0374-8 ↗
5. Impact abrasion of hydraulic structures concrete10.51400/2709-6998.1801 ↗
6. Concrete–ice abrasion mechanics10.1016/j.cemconres.2015.01.001 ↗
7. Abrasion resistance of concrete micro-reinforced with polypropylene fibers10.1016/j.conbuildmat.2011.07.044 ↗
8. Application of high performance polypropylene fibers in concrete lining of water tunnels10.1016/j.matdes.2013.09.075 ↗
9. Fracture behaviour of heat cured fly ash based geopolymer concrete10.1016/j.matdes.2012.08.005 ↗
10. Abrasion resistance of high-strength concrete in hydraulic structures10.1016/j.wear.2005.02.079 ↗
11. Energy efficiency and CO2 emissions from the global cement industry
12. Abrasion resistance of concrete containing marginal aggregates10.1016/j.conbuildmat.2014.05.084 ↗
13. Abrasion erosion of concrete by water-borne sand10.1016/j.cemconres.2005.03.018 ↗
14. Abrasion resistance of alkali-activated slag concrete designed by Taguchi method10.1016/j.conbuildmat.2015.08.128 ↗
15. Abrasion resistance of concrete containing nano-particles for pavement10.1016/j.wear.2005.08.006 ↗
16. Abrasion Properties of Steel Fiber Reinforced Silica Fume Concrete According to Los Angeles and Water Abrasion Tests10.5755/j01.ms.20.4.6460 ↗
17. Effect of hydraulic parameters on abrasion erosion of fiber reinforced concrete in hydraulic structures10.1016/j.conbuildmat.2020.120966 ↗
18. Hydro-abrasive erosion of high performance fiber-reinforced concrete10.1016/j.wear.2008.11.010 ↗
19. Surface abrasion resistance of high-volume fly ash concrete modified by graphene oxide: Macro- and micro-perspectives10.1016/j.conbuildmat.2019.117686 ↗
20. Effects of fluidal fly ash on abrasion resistance of underwater repair concrete10.1016/j.wear.2017.01.051 ↗
21. Influence and mechanism of micro/nano-mineral admixtures on the abrasion resistance of concrete10.1016/j.conbuildmat.2018.11.224 ↗
22. Abrasive wear of concrete measured by different accelerated tests and natural exposure
23. Testing of Concrete Abrasion Resistance in Hydraulic Structures on the Lower Sava River. Strojniški vestnik – Journal of
24. Simulation of water pressure on washout of underwater concrete repair
25. The influence of pore pressure upon concrete10.1680/macr.1981.33.114.3 ↗
26. Simulation of the behavior of pressurized underwater concrete10.1016/j.aej.2015.03.017 ↗
27. Concrete strength loss from water pressurisation
28. Kawai, T. (1988). Non-dispersible underwater concrete using polymers – The production, performance and potential of polymers in concrete. 5th International Congress on Polymers, Brighton. September 24-27, 1987.
29. Behaviour of cement concrete under common salt solution both under hydrostatic and atmospheric pressures10.1016/0008-8846(81)90013-2 ↗
30. Influence of hydrostatic pressure on compressive strength of self-consolidating concrete
31. EN 206+A1. Concrete: Specification, Performance, Production and Conformity. European Committee for Standardization: Brussels, Belgium, 2018.
32. EN 12350-5. Testing fresh concrete – Part 5: Flow table test. European Committee for Standardization: Brussels, Belgium, 2019.
33. EN 12350-8. Testing fresh concrete – Part 8: Self-compacting concrete – Slump-flow test. European Committee for Standardization: Brussels, Belgium, 2019.
34. EN 12350-9. Testing fresh concrete – Part 9: Self-compacting concrete – V-funnel test. European Committee for Standardization: Brussels, Belgium, 2010.
35. Test Method for Determining the Resistance of Freshly Mixed Concrete to Washing Out in Water
36. Bond strength of underwater repair concretes under hydrostatic pressure10.1016/j.conbuildmat.2014.08.020 ↗
37. EN 14157. Natural stone test methods – Determination of the abrasion resistance. European Committee for Standardization: Brussels, Belgium. 2017.
38. EN 12390-3. Testing hardened concrete – Part 3: Compressive strength of test specimens. European Committee for Standardization: Brussels, Belgium. 2019.
39. EN 480-11. Admixtures for Concrete, Mortar and Grout, Test Methods, Determination of Air Void Characteristics in Hardened Concrete. European Committee for Standardization: Brussels, Belgium. 2005.
40. Study of the anti-abrasion performance and mechanism of coral reef sand concrete10.1016/j.conbuildmat.2021.123263 ↗
41. Evaluation and Prediction on the Hydraulic Abrasion Performance of High Belite Cement-Based Concrete10.1007/s12205-021-1826-7 ↗
42. Influence of Different Particle Sizes of Blast-Furnace Slag as a Fine Aggregate on Mechanical Strength and Abrasion Resistance of Concrete10.1007/s12633-019-00332-0 ↗
43. Abrasion resistance of ultra-high performance concrete with coarse aggregate10.1617/s11527-021-01750-6 ↗
44. Improving the abrasion resistance of hydraulic-concrete containing surface crack by adding silica fume10.1016/j.conbuildmat.2006.03.001 ↗
45. Influence of various material parameters on the abrasion resistance of concrete by sand blasting
46. EN 1340. Concrete kerb units – Requirements and test methods. European Committee for Standardization: Brussels, Belgium. 2003.
47. ASTM C1138. Standard Test Method for Abrasion Resistance of Concrete (Underwater Method). ASTM International, West Conshohocken, USA. 2019.
48. Studying the abrasion damage of concrete for hydraulic structures under various flow conditions10.1016/j.cemconcomp.2022.104849 ↗