Abstract Hydraulic cements based on the alkali aluminosilicate chemistry tend to be more reactive than Type I Portland cement. An experimental investigation was conducted in order to evaluate the effects of storage in air and in sealed condition on the properties and performance of alkali aluminosilicate cements. Different storage durations up to 28 days were considered in this experimental study. Hydraulic cements were evaluated based on their morphology, chemistry and mineralogy, hydration kinetics, strength development characteristics, and microstructure of the resultant hydration products. The early-age hydration kinetics and strength development characteristics of the alkali aluminosilicate cement were found to be altered by storage, especially when the cement was exposed to air. Older cements also produced hydration products that were more susceptible to microcracking when dried under vacuum. Longer-term strength development characteristics of cements were less influenced than their shorter-term strength development characteristics with duration of storage in sealed or exposed condition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Concrete Properties and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Industrially interesting approaches to “low-CO 2” cements10.1016/j.cemconres.2004.01.021 ↗
2. Sustainable development and climate change initiatives10.1016/j.cemconres.2007.09.008 ↗
3. Advances in alternative cementitious binders10.1016/j.cemconres.2010.11.012 ↗
4. New cements for the 21st century: the pursuit of an alternative to Portland cement10.1016/j.cemconres.2011.03.016 ↗
5. Alkali-activated materials
6. Alkali-activated binders: a review: part 1. Historical background, terminology, reaction mechanisms and hydration products10.1016/j.conbuildmat.2007.10.015 ↗
7. Alkali-activated binders by use of industrial by-products10.1016/j.cemconres.2004.06.019 ↗
8. Waddell · 2008
9. High-temperature resistance in alkali-activated cement10.1111/j.1551-2916.2010.03887.x ↗
10. Resistance of alkali-activated slag concrete to acid attack10.1016/S0008-8846(03)00125-X ↗
11. An experimental study on corrosion resistance of concrete with ground granulate blast-furnace slag10.1016/j.cemconres.2004.11.010 ↗
12. Geopolymer technology: the current state of the art10.1007/s10853-006-0637-z ↗
13. On the development of fly ash-based geopolymer concrete
14. Rangan · 2008
15. Synthesis and strength optimization of one-part geopolymer based on red mud10.1016/j.conbuildmat.2016.02.099 ↗
16. Effects of alkali on one-part alkali-activated cement synthesized by calcining bentonite with dolomite and Na 2 CO 310.1016/j.clay.2017.01.020 ↗
17. Characterisation of one-part geopolymer binders made from fly ash10.1007/s12649-016-9582-5 ↗
18. One-part alkali-activated materials: a review10.1016/j.cemconres.2017.10.001 ↗
19. Synthesis and characterization of alkali aluminosilicate hydraulic cement that meets standard requirements for general use10.1016/j.conbuildmat.2017.10.002 ↗
20. Development of a new CO2 sequestration process utilizing the carbonation of waste cement10.1021/ie0496176 ↗
21. Surface modification of fly ash for active catalysis
22. Alkali-activated fly ashes: a cement for the future10.1016/S0008-8846(98)00243-9 ↗
23. A calorimetric study of early hydration of alkali-slag cements10.1016/0008-8846(95)00126-W ↗
24. Effect of chemical admixtures on properties of high-calcium fly ash geopolymer10.1007/s12613-011-0448-3 ↗
25. The coexistence of geopolymeric gel and calcium silicate hydrate at the early stage of alkaline activation10.1016/j.cemconres.2004.10.042 ↗
26. Accelerated curing of compacted calcium silicate mortars on exposure to CO210.1111/j.1151-2916.1974.tb11420.x ↗
27. Promoter-induced enhancement of the crystallization rate of zeolites and related molecular sieves10.1038/381298a0 ↗