Development of biogenic silica biocoatings to improve the performance of recycled aggregate concrete
Source abstract
Abstract
This study evaluates the effectiveness of improving the durability of recycled aggregate concrete (RAC) through the controlled deposition of biogenic silica (SiO 2 ). This process is optimised by growing diatoms in two artificial environments as a mean to produce a protective coating. Concrete samples with protective bio-coatings grown in two different environments were tested for durability against uncoated control samples and results suggest that the biocoating provides significant benefits. Increases of 30–50% in ultrasonic pulse velocity were demonstrated for bio-coated concrete samples suggesting that the diatom treatment produces surface densification thus increasing the mechanical strength of bio-coated concrete. Tests of chloride ion diffusion and resistance to freeze-thaw cycles showed reductions in permeability due to the biocoating of 29–34% and 34–45%, for each test respectively. Improvements in corrosion resistance were also shown in resistivity tests. In addition, SEM and BSEM microscopy provides evidence to support the conclusions of physical tests: diatoms migrate to fill surface pores and micro-cracks reducing the porosity of the concrete’s surface matrix resulting in surface densification and decreased permeability.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Recycled Aggregate Concrete Performance · Innovative concrete reinforcement materials · Innovations in Concrete and Construction Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (73)
Show source-provided references
1. Efficiencies of carbonation and nano silica treatment methods in enhancing the performance of recycled aggregate concrete10.1016/j.conbuildmat.2021.125080 ↗
2. Influence of amount of recycled coarse aggregates and production process on properties of recycled aggregate concrete10.1016/j.cemconres.2007.02.002 ↗
3. An overview of study on recycled aggregate concrete in China (1996-2011)10.1016/j.conbuildmat.2011.12.074 ↗
4. A comprehensive review on recycled aggregate and recycled aggregate concrete10.1016/j.resconrec.2021.105565 ↗
5. Limiting the maximum fine and coarse recycled aggregates-type a used in structural concrete10.1016/j.conbuildmat.2023.131273 ↗
6. Structural Code; Royal Decree 470/2021, Spanish Ministry of the Presidency, Relations with the Courts and Democratic Memory, Madrid, Spain, 2021.
7. Structural concrete with simultaneous incorporation of fine and coarse recycled concrete aggregates: Mechanical, durability and long-term properties10.1016/j.conbuildmat.2017.07.215 ↗
8. Cost-benefit analysis of the production of ready-mixed high-performance concrete made with recycled concrete aggregate: A case study in Thailand10.1016/j.heliyon.2020.e04135 ↗
9. Effect of design parameters on compressive and split tensile strength of self-compacting concrete with recycled aggregate: An overview10.3390/app11136028 ↗
10. Influence of quality of recycled aggregates on the mechanical properties of recycled aggregate concretes: An overview10.1016/j.conbuildmat.2022.127071 ↗
11. Durability of recycled aggregate concrete – A review10.1016/j.cemconcomp.2018.03.008 ↗
12. Tests and simulation of the bond-slip between steel and concrete with recycled aggregates from CDW10.3390/buildings11020040 ↗
13. Concrete produced with recycled concrete aggregate exposed to treatment methods
14. REVIEW ARTICLE - CIVIL ENGINEERING A Review of Corrosion and Protection of Steel in Concrete10.1007/s13369-018-3303-2 ↗
15. Durability of concrete: Degradation phenomena involving detrimental chemical reactions10.1016/j.cemconres.2007.09.015 ↗
16. Use of bacteria to repair cracks in concrete10.1016/j.cemconres.2009.08.025 ↗
17. Investigating the effects of bacterial activity on compressive strength and durability of natural lightweight aggregate concrete reinforced with steel fibers10.1016/j.conbuildmat.2020.119032 ↗
18. Bacteria-based self-healing concrete exposed to frost salt scaling10.1016/j.cemconcomp.2023.105016 ↗
19. A.K. Parashar, P. Nagar, Effect of Bacillus Family Bacteria on the Mechanical and Durability Properties of Concrete Mix: A Review, in: L.N. in M. Engineering (Ed.), Shukla, A.K., Sharma, B.P., Arab. A., Kumar, P. Recent Adv. Mech. Eng., FLAME 2022, Springer, Singapore, 2023: pp. 521–530. 〈https://doi.org/10.1007/978-981-99-1894-2〉.10.1007/978-981-99-1894-2_44 ↗
20. Biomineralization, bacterial selection and properties of microbial concrete: A review
21. State-of-art review of bacteria-based self-healing concrete: Biomineralization process, crack healing, and mechanical properties10.1016/j.conbuildmat.2023.131198 ↗
22. Ethyl silicate for surface protection of concrete: Performance in comparison with other inorganic surface treatments10.1016/j.cemconcomp.2013.05.008 ↗
23. Effects and mechanisms of surface treatment of hardened cement-based materials with colloidal nanoSiO2 and its precursor10.1016/j.conbuildmat.2013.11.062 ↗
24. Innovative application of silicon nanoparticles (SN): Improvement of the barrier effect in hardened Portland cement-based materials10.1016/j.conbuildmat.2014.11.054 ↗
25. Effects of Spraying Various Nanoparticles at Early Ages on Improving Surface Characteristics of Concrete Pavements10.1007/s40999-019-00407-4 ↗
26. Effect of SiO2 sol/silane emulsion in reducing water and chloride ion penetration in concrete10.3390/coatings10070682 ↗
27. Durability of concrete superficially treated with nano-silica and silane/ nano-clay coatings10.1177/0361198120953160 ↗
28. A study on impact of different surface treatment agents on the durability of airport pavement concrete
29. Effect of nano-silica on mechanical, microstructural and durability properties of cement-based materials: A review
30. Diatomaceous lessons in nanotechnology and advanced materials10.1002/adma.200803778 ↗
31. Diatoms green nanotechnology for biosilica-based drug delivery systems10.3390/pharmaceutics10040242 ↗
32. The biology of biofouling diatoms and their role in the development of microbial slimes10.1080/08927010802254583 ↗
33. Innovative approach for the protection of recycled concrete by biogenic silica biodeposition10.1016/j.conbuildmat.2023.130475 ↗
34. Improving the performance of recycled concrete by biodeposition of biogenic silica as a surface coating10.1016/j.conbuildmat.2023.133781 ↗
35. Influence of light and temperature on the growth rate of estuarine benthic diatoms in culture10.1007/BF00395586 ↗
36. UNE-EN 197-1. Cement. Part 1: Composition, specifications and conformity criteria for commo on cements; AENOR: Madrid, Spain, 2011.
37. Mechanical and microstructural characterization of non-structural precast concrete made with recycled mixed ceramic aggregates from construction and demolition wastes10.1016/j.jclepro.2018.01.191 ↗
38. Recycled precast concrete kerbs and paving blocks, a technically viable option for footways
39. Mechanical and microstructural properties of recycled concretes mixed with ceramic recycled cement and secondary recycled aggregates. A viable option for future concrete10.1016/j.conbuildmat.2020.121455 ↗
40. Influence of the amount of mixed recycled aggregates on the properties of concrete for non-structural use10.1016/j.conbuildmat.2011.06.073 ↗
41. M. Sánchez de Juan, Estudio sobre la utilización de árido reciclado para la fabricación de hormigón estructural, Polytechnic University of Madrid, 2004. https://doi.org/10.20868/UPM.thesis.381.10.20868/UPM.thesis.381 ↗
42. Recycling aggregates for self-compacting concrete production: A feasible option
43. R. Martínez-García, Evaluation of the use of recycled concrete aggregates for the production of self-compacting concretes and cement mortars, University of León, 2021. 〈http://buleria.unileon.es/handle/10612/13363〉.
44. UNE-EN 12620:2003+A1. Aggregates for concrete; AENOR: Madrid, Spain, 2009.
45. UNE-EN 1992-1-1. Eurocode 2: Design of concrete structures. Part 1-1: General rules and rules for buildings; AENOR: Madrid, Spain, 2020.
46. UNE-EN 933-1. Tests for geometrical properties of aggregates. Part 1: Determination of pa rticle size distribution. Sieving method; AENOR: Madrid, Spain, 2012.
47. UNE-EN 1097-6. Tests for mechanical and physical properties of aggregates. Part 6: Determination of particle density and water absorption; AENOR: Madrid, Spain, 2014.
48. UNE-EN 933-11. Tests for geometrical properties of aggregates. Part 11: Classification test for the constituents of coarse recycled aggregate; AENOR: Madrid, Spain, 2009.
49. .UNE-EN 206:2013+A2. Concrete. Specification, performance, production and conformity; AENOR: Madrid, Spain, 2021..
50. UNE-EN 12390-2. Testing hardened concrete. Part 2: Making and curing specimens for strength tests; AENOR: Madrid, Spain, 2020.
51. Modeling the response time of diatom assemblages to simulated water quality improvement and degradation in running waters10.1139/F10-162 ↗
52. The Use of Crusher-run Aggregates of Reinforced Concrete Frames When Reconstructing Hydraulic Structures10.1016/j.proeng.2016.08.156 ↗
53. Large-scale geographical and environmental drivers of shallow lake diatom metacommunities across Europe10.1016/j.scitotenv.2019.135887 ↗
54. Growth Analysis and Frustule Characterization of Benthic Diatomic Isolates for Nanotechnological Applications Article
55. UNE-EN 14407. Water quality. Guidance for the identification and enumeration of benthic diatom samples from rivers and lakes; AENOR: Madrid, Spain, 2015.
56. UNE-EN 13946.Water quality. Guidance for the routine sampling and preparation of benthic diatoms from rivers and lakes; AENOR: Madrid, Spain, 2014.
57. G. Hofmann, M. Werum, H. Lange-Bertalot, Diatomeen im Süßwasser-Benthos von Mitteleuropa: Bestimmungsflora Kieselalgen für die ökologische Praxis; über 700 der häufigsten Arten und ihre Ökologie, 2011.
58. UNE-EN 12390-3 Testing hardened concrete. Part 3: Compressive strength of test specimens; AENOR: Madrid, Spain, 2020.
59. UNE-EN 12504-4. Testing concrete in structures. Part 4: Determination of ultrasonic pulse velocity; AENOR: Madrid, Spain, 2022.
60. UNE 83987. Concrete durability. Test methods. Measurement of chloride diffusion coefficient in hardened concrete. Multiregime method; AENOR: Madrid, Spain, 2014.
61. EN 1339. Concrete paving flags. Requirements and test methods; AENOR: Madrid, Spain, 2004.
62. UNE 83988-1. Concrete durability. Test methods. Determination of the electrical resistivity. Part 1: Direct test (reference method); AENOR:Madrid, Spain, 2008.
63. Improvement of mechanical properties of recycled aggregate concrete basing on a new combination method between recycled aggregate and natural aggregate10.1016/j.conbuildmat.2017.05.084 ↗
64. Influence of moisture states of natural and recycled aggregates on the slump and compressive strength of concrete10.1016/S0008-8846(03)00186-8 ↗
65. Enhancing the durability properties of concrete prepared with coarse recycled aggregate10.1016/j.conbuildmat.2012.02.032 ↗
66. Creep and shrinkage of recycled aggregate concrete10.1016/j.conbuildmat.2009.02.018 ↗
67. Concrete compressive strength by means of ultrasonic pulse velocity and moduli of elasticity
68. Estimation of compressive strength of self-compacted concrete with fibers consisting nano-SiO2 using ultrasonic pulse velocity10.1016/j.conbuildmat.2013.03.082 ↗
69. Continuous tracking of the relationship between resistivity and pore structure of cement pastes10.1016/j.conbuildmat.2013.11.067 ↗
70. Determination of reinforced concrete durability with on-site resistivity measurements10.1617/s11527-016-0884-7 ↗
71. Mechanical, rheological, durability and microstructural properties of high performance self-compacting concrete containing SiO2 micro and nanoparticles10.1016/j.matdes.2011.08.037 ↗
72. Application of bacterial biomass in biocementation process to enhance the mechanical and durability properties of concrete
73. Preliminary attempt of hardened mortar sealing by colloidal nanosilica migration10.1016/j.conbuildmat.2014.05.040 ↗