Abstract

Alkali-activated materials (AAMs) are emerging as sustainable alternatives to traditional binders in the construction industry. While the compatibility of various admixtures, such as superplasticizers, water reducers, and retarders, has been studied in one-part AAMs, a significant gap exists in understanding the effects of viscosity-modifying admixtures (VMAs). This study investigates the compatibility and impact of incorporating VMAs into one-part alkali-activated slag (AAS) paste, as well as the associated environmental impacts of using VMAs.Two factors were considered: the effect of different addition of VMAs methods (adding VMA separately, undissolved in water, or dissolved in water) and timings (early addition, 1 min after dry mixing the powder ingredients, and delayed addition, 25 min after mixing and resting). Initial flow diameter, flow retention, setting time, rheological properties (yield stress and plastic viscosity), heat of hydration, compressive strength (at 3, 7, and 28 days), and drying shrinkage were evaluated. Findings showed that delayed and separate addition of VMA significantly prolonged setting times due to slower distribution within the paste, regardless of the water-to-binder (w/b) ratio. Increasing the w/b ratio diluted the paste and reduced the significance of the method and timing of VMA addition on all measured properties. This research provides critical insights into the strategic use of VMAs to enhance the control of the rheological performance of AAS systems, contributing to the advancement of sustainable construction materials. • Adding VMA separately or combined with mixing water will impact AAS rheological properties differently. • Separate addition of VMA than mixing water significantly prolonged setting times • The timing of VMA addition greatly influences the rheological properties of one-part AAS. • Adding VMA reduces the drying shrinkage of one-part AAS. • Minor influence of timing and adding method of VMA at high w/c mixtures.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (71)

Show source-provided references
1. Experimental study on eco-friendly one-part alkali-activated slag-fly ash-lime composites under CO2 environment: reaction mechanism and carbon capture capacity10.1016/j.conbuildmat.2024.135779 ↗
2. Enhancement of setting times and hardening of alkali-activated slag binder using CO2-modified slag10.1016/j.cemconcomp.2022.104797 ↗
3. A state-of-the-art review on the setting behaviours of ground granulated blast furnace slag- and metakaolin-based alkali-activated materials10.1016/j.conbuildmat.2023.130389 ↗
4. Research on dynamic mechanical properties of alkali activated slag concrete under temperature-loads coupling effects10.1016/j.conbuildmat.2017.08.015 ↗
5. Hydration kinetics of cement composites with different admixtures at low temperatures10.1016/j.conbuildmat.2019.07.153 ↗
6. Effect of phosphonate addition on sodium carbonate activated slag properties10.1016/j.cemconcomp.2021.103986 ↗
7. Effect of organic phosphonate on fresh properties of alkali-activated slag composites under different systems: Na2SO4, Na2SiO3, Na2CO310.1016/j.conbuildmat.2024.137698 ↗
8. Y. Qin, C. Qu, C. Ma, L. Zhou, One-Part Alkali-Activated Materials: State of the Art and Perspectives, (2022).10.3390/polym14225046 ↗
9. Suitability of commercial superplasticizers for one-part alkali-activated blast-furnace slag mortar
10. 3D printing of calcined clay-limestone-based cementitious materials10.1016/j.cemconres.2021.106553 ↗
11. Effect of viscosity modifier admixture on Portland cement paste hydration and microstructure10.1016/j.conbuildmat.2019.04.020 ↗
12. Performance of new viscosity modifying admixtures in enhancing the rheological properties of cement paste10.1016/S0008-8846(03)00233-3 ↗
13. Effects of the charge density of anionic copolymers on the properties of fresh cement pastes10.1016/j.conbuildmat.2020.120207 ↗
14. Effects of adsorption group and molecular weight of viscosity-modifying admixtures on the properties of cement paste10.1061/(ASCE)MT.1943-5533.0004296 ↗
15. Short- and long-term properties of lime mortars with water-reducers and a viscosity-modifier
16. Rheological properties of cement-based materials using a biopolymer viscosity modifying admixture (BVMA) under different dispersion conditions10.1016/j.cemconcomp.2021.104224 ↗
17. Can superabsorbent polymers be used as rheology modifiers for cementitious materials in the context of 3D concrete printing?10.1016/j.conbuildmat.2023.130777 ↗
18. The use of extrusion rheometry in the development of extruded fiber-reinforced cement composites
19. Influence of viscosity modifying admixtures on the rheological behavior of cement and mortar pastes10.1007/s13367-012-0004-3 ↗
20. Development of 3D printable engineered cementitious composites with ultra-high tensile ductility for digital construction10.1016/j.matdes.2019.108088 ↗
21. Optimization of biopolymer additives for 3D printable cementitious systems: A design of experiment approach
22. Xanthan Gum contribution to cement slurry performance
23. Rheological behaviour and printability optimization of geopolymer ink for direct ink writing10.1016/j.clay.2025.107791 ↗
24. Development of a novel viscosity modifier agent for cementitious materials: preliminary study10.1061/(ASCE)MT.1943-5533.0003625 ↗
25. Investigating the interaction of limestone calcined clay and OPC-based systems with a methyl hydroxyethyl cellulose-based viscosity modifier used for 3D printable concrete10.1061/JMCEE7.MTENG-17728 ↗
26. Performance characteristics of cement grouts made with various combinations of high-range water reducer and cellulose-based viscosity modifier10.1016/S0008-8846(03)00214-X ↗
27. Stability of self-consolidating concrete containing different viscosity modifiers
28. Waste-based one-part alkali activated materials10.3390/ma14112911 ↗
29. Effects of solid activator and fly ash on rheology and thixotropy of one-part alkali-activated pastes10.3151/jact.20.139 ↗
30. Single and multi-response optimization of retarded admixture on alkali activated slag rheological behavior by the taguchi method10.1016/j.conbuildmat.2024.139812 ↗
31. Influence of mixing protocols on flow retention of one-part alkali activated slag systems10.1016/j.conbuildmat.2024.138467 ↗
32. The effectiveness of different superplasticizers in ambient cured one-part alkali activated pastes10.1016/j.cemconcomp.2018.12.027 ↗
33. Using viscosity modifiers to reduce effective diffusivity in mortars10.1061/(ASCE)MT.1943-5533.0000524 ↗
34. Effects of mixing water temperatures on properties of one-part alkali-activated slag paste10.1016/j.conbuildmat.2020.121030 ↗
35. ASTM, U.S. Int’l, Standard Test Method for Time of Setting of Concrete Mixtures by Penetration Resistance C 403/C 403M, (1999).
36. Effect of ingredients adding sequences on rheological properties of alkali-activated slag paste10.1007/s41062-024-01462-0 ↗
37. Isothermal calorimetry in the standard ASTM C1679-08
38. ASTM C109 / C109M - 2002. Standard test method for compressive strength of hydraulic cement Mortars (Using 2-in. or [50 mm] Cube Specimens)
39. ASTM international, Standard Test Method for Length Change Of Hardened Cement Mortar And Concrete (ASTM C157), 04 (2017) 1–7.
40. The interrelationship between surface chemistry and rheology in alkali activated slag paste10.1016/j.conbuildmat.2014.04.127 ↗
41. Porosity effects on rheological and mechanical behavior of self-compacting concrete
42. N. ELsayed, A. Soliman, Alkali-Activated Concrete Workability and Effect of Various Admixtures: A Review, in: 2024: pp. 729–738. https://doi.org/10.1007/978-3-031-35471-7_52.10.1007/978-3-031-35471-7_52 ↗
43. Fresh, hardened, and microstructural properties of ambient cured one-part alkali-activated self-consolidating concrete
44. On the mechanisms of shrinkage reducing admixture in alkali activated slag binders
45. Effects of type and dosage of alkaline activator and temperature on the properties of alkali-activated slag mixtures10.1016/j.conbuildmat.2006.07.002 ↗
46. Effects of delayed addition of polycarboxylate ether on one-part alkali-activated fly ash/slag pastes: Adsorption, reaction kinetics, and rheology10.1016/j.conbuildmat.2022.126611 ↗
47. Recent progress in understanding setting and hardening of alkali-activated slag (AAS) materials10.1016/j.cemconcomp.2022.104795 ↗
48. L. Struble, G.-K. Sun, Viscosity of Portland Cement Paste as a Function of Concentration, 1995.10.1016/1065-7355(94)00023-7 ↗
49. Very early-age reaction kinetics and microstructural development in alkali-activated slag10.1016/j.cemconcomp.2014.09.001 ↗
50. Hydration of cementitious materials, present and future10.1016/j.cemconres.2011.03.026 ↗
51. Kinetics study of geopolymerization of fly ash using isothermal conduction calorimetry10.1007/s10973-016-5823-x ↗
52. Evaluation of rheology and strength development of alkali-activated slag with different silicates sources10.1016/j.cemconcomp.2022.104415 ↗
53. Ambient-cured alkali-activated slag paste incorporating micro-silica as repair material: effects of alkali activator solution on physical and mechanical properties10.1016/j.conbuildmat.2019.116911 ↗
54. Multi-objective optimization of one-part alkali-activated mortar mixes using Taguchi-Grey relational analysis10.1016/j.conbuildmat.2023.134761 ↗
55. Structural evolution of an alkali sulfate activated slag cement10.1016/j.jnucmat.2015.11.016 ↗
56. Preparation of cleaner one-part geopolymer by investigating different types of commercial sodium metasilicate in China10.1016/j.jclepro.2018.08.060 ↗
57. Effect of temperature and aluminium on calcium (alumino)silicate hydrate chemistry under equilibrium conditions10.1016/j.cemconres.2014.10.015 ↗
58. Study of fly ash characterization as a cementitious material
59. Partially burnt wood fly ash characterization and its application in low-carbon mortar and concrete10.1016/j.conbuildmat.2023.132946 ↗
60. Optimization of alkali-activated ladle slag composites mix design using taguchi-based TOPSIS method10.1016/j.conbuildmat.2022.126946 ↗
61. Pore solution in alkali-activated slag cement pastes. Relation to the composition and structure of calcium silicate hydrate10.1016/S0008-8846(03)00254-0 ↗
62. The efficiency of borax as an additive on properties of one-part fly ash/slag-based alkali-activated materials
63. Optimizing concrete for circularity: a comparative life cycle assessment of geopolymer and ordinary concrete10.1007/s11356-024-34863-w ↗
64. Biases in life cycle assessment of circular concrete10.1016/j.rser.2023.114237 ↗
65. Environmental impact assessment for performance-oriented geopolymer concrete research10.1061/(ASCE)MT.1943-5533.0004526 ↗
66. BRITISH STANDARD,BS EN ISO 14040 (2006), Environmental management - Life cycle assessment: Principles and framework, 32 p.
67. Pre-mix Concrete EPD Environmental Product Declaration Australasia, n.d. 〈www.lifecyclelogic.com.au〉.
68. Recycling and optimum utilization of engineering sediment waste into low-carbon geopolymer paste for sustainable infrastructure10.1016/j.jclepro.2022.135549 ↗
69. LCA allocation procedure used as an incitative method for waste recycling: an application to mineral additions in concrete10.1016/j.resconrec.2010.04.001 ↗
70. An environmental evaluation of geopolymer based concrete production: reviewing current research trends10.1016/j.jclepro.2011.03.012 ↗
71. Construction materials from stainless steel slags: technical aspects, environmental benefits, and economic opportunities10.1111/jiec.12314 ↗