journal article·2014-04

A study of the effect of light-burnt dolomite on the hydration of alkali-activated Portland blast-furnace slag cement

Wan-Hee Yang, Dong-Woo Ryu, Dong-Cheol Park, Woo-Jae Kim, Chee-Ho Seo

Publisher page

Abstract

Abstract This study used the typical powder alkaline material anhydrous sodium sulfate (Na2SO4) as an activator in a system in which Portland cement (10–20%) and ground granulated blast-furnace slag (GGBS, 80–90%) are generally mixed and added to light-burnt dolomite (LBD), one of the economical lime materials. Their effect on the hydration and strength of the cement was then analyzed. According to the analysis, the 1st peak of the minute heat of hydration increased after mixing the LBD. On the other hand, for the 2nd peak, a slight delay was observed. As a result of the mixing, the cumulative heat of hydration increased. Although the rate of setting decreased, the strength of the material improved after the 3rd, 7th and 28th days. In other words, it was confirmed that the pore structure of the paste became dense after 28 days of aging.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Grouting, Rheology, and Soil Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Mehta · 2006
2. International Energy Agency (IEA), World Business Council for Sustainable Development (WBCSD). Cement Technology Roadmap 2009. Paris (FR): Corlet; 2010.
3. Shi · 2006
4. Resistance of alkali-activated slag concrete to carbonation10.1016/S0008-8846(01)00574-9 ↗
5. Corrosion resistance of alkali-activated slag cement10.1680/adcr.2003.15.2.77 ↗
6. Strength and shrinkage properties of alkali-activated slag concrete containing porous coarse aggregate10.1016/S0008-8846(98)00203-8 ↗
7. Effect of admixtures on properties of alkali-activated slag concrete10.1016/S0008-8846(00)00349-5 ↗
8. Effect of elevated temperature curing on properties of alkali-activated concrete10.1016/S0008-8846(99)00143-X ↗
9. Strength and shrinkage properties of alkali-activated slag concrete placed into a large column10.1016/S0008-8846(99)00011-3 ↗
10. Effect of pore size distribution on drying shrinkage of alkali-activated slag concrete10.1016/S0008-8846(00)00327-6 ↗
11. An experimental study on the freezing–thawing and chloride resistance of concrete using high volumes of GGBS10.5345/JKIBC.2012.12.3.315 ↗
12. An experimental study on the carbonation and drying shrinkage of concrete using high volumes of ground granulated blast-furnace slag10.5345/JKIBC.2012.12.4.393 ↗
13. An experimental study on early strength and drying shrinkage of high strength concrete using high volumes of ground granulated blast-furnace slag(GGBS)10.5345/JKIBC.2013.13.4.391 ↗
14. Magnesia modification of alkali-activated slag fly ash cement10.1007/s11595-011-0182-8 ↗
15. Effect of magnesia on properties and microstructure of alkali-activated slag cement
16. KS ISO 9597. Specifies the methods for determining standard consistence, setting times and soundness of cements. International Organization for Standardization, 2008.
17. KS L 5105. Testing method for compressive strength of hydraulic cement mortars. Korean Industrial Standards, 2007.
18. Pozzolanic reaction in the presence of chemical activators:Part II. Reaction products and mechanism10.1016/S0008-8846(00)00214-3 ↗
19. Investigation on some factors affecting the characteristics of alkali-phosphorus slag cement10.1016/0008-8846(89)90004-5 ↗
20. Properties of alkali-activated slag concrete
21. Hydration Portland Cem
22. Mindess S, Young JF. Concrete. Englewood Cliffs NJ (USA): Prentice-Hall International Inc., 1981.