Abstract

Abstract In recent years, upon increasingly exploiting natural sandstone, the natural ecology has been damaged severely. To reduce the impact of market demand on natural resources, replacing natural resources with recycled materials, such as desulfurization slag and slag powder, is a very important topic at present. This study used desulfurization slag that had been passed through #4 sieves and slag at a fineness of approximately 4000 cm 2 /g to replace fine aggregates (0, 10, 20 and 40%) and cement (0, 10, 20 and 40%), respectively, via a volumetric method to make cement mortar for testing its fresh properties. The hard properties and volume stability were tested at different ages in order to discuss the variance in the material volume stability under different mix proportions. The results show that the slump flow of the mix proportion with the slag powder is higher than the slump flow of the mix proportion without addition by 11.5–39%. The addition of desulfurization slag and slag powder increases the setting time. The compressive strength and the ultrasonic pulse velocity decrease as the replacement of desulfurization slag increases, and both increase with age. Under the influence of high temperature, a high compressive strength can be reached at an early age. When the addition level of desulfurization slag is the maximum, 40%, the weight loss is higher than observed at the other addition levels. The autoclave expansion increases as the desulfurization slag replacement increases and the amount of slag decreases. After high temperature catalysis, the expansion response increases as the curing time and desulfurization slag replacement increase and the slag powder decreases. The high temperature has an apparent effect on the volume stability of slag powder cement mortar with desulfurization slag, and the expansion response of all mix proportions is within safe specifications (0.06%).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovations in Concrete and Construction Materials · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Chen · 2014
2. Engineering properties of cement less concrete produced from GGBFS and recycled desulfurization slag10.1016/j.conbuildmat.2014.04.017 ↗
3. Tan · 2008
4. Zheng Ruibin, Proceedings of the TCI – Concrete Science and Technology, Vol. 3, No. 4, 2009, pp. 64–74.
5. Engineering properties of controlled low strength desulfurization slags (CLSDS)10.1016/j.conbuildmat.2016.03.138 ↗
6. Wei · 2015
7. A study of the replacement of desulphurization slag for sand to ready-mixed soil materials (RMSM)10.12989/cac.2016.17.3.423 ↗
8. Engineering properties of alkali-activated binders by use of desulfurization slag and GGBFS10.1016/j.conbuildmat.2014.05.056 ↗
9. Utilization of desulfurization/granulated blast furnace slag as controlled low strength material without Portland cement
10. Application of high-temperature rapid catalytic technology to forecast the volumetric stability behavior of containing steel slag mixtures10.1016/j.conbuildmat.2013.09.030 ↗
11. Properties of compressed concrete paving units made produced using desulfurization slag10.1002/ep.12129 ↗
12. Chen · 2015
13. A study of the engineering properties of CLSM with a new type of slag10.1016/j.conbuildmat.2015.10.198 ↗
14. Ju · 2011
15. Li Luo · 2008
16. Alkali aggregate reaction in alkali slag cement mortars10.1007/BF02838542 ↗
17. Sulfate attack on alkali-activated slag concrete10.1016/S0008-8846(01)00659-7 ↗
18. Hydration of alkali-activated slag: Thermodynamic modeling10.1680/adcr.2007.19.2.81 ↗
19. Syu · 2013
20. Lin · 2014
21. Effect of storage and curing conditions at elevated temperatures on aerogel-incorporated mortar samples based on UHPC recipe10.1016/j.conbuildmat.2015.12.162 ↗
22. Zhang · 2009 · 111
23. Wang · 2006
24. Pathways to a Low-carbon Economy, 2009, Version 2 of the Global Greenhouse Gas Abatement Cost Curve McKinsey & Company.
25. ASTM C150 · 2005
26. ASTM C 989-04 · 1999
27. ASTM C778 · 2013
28. ASTM D6103 · 1997
29. ASTM C403 · 1999
30. ASTM C39 · 2005
31. ASTM C597 · 2002
32. ASTM C151 · 2016
33. ASTM C1012 · 2004
34. ASTM C1437-15 · 2015