journal article·2024-12

Steering the early strength of clinker-free cementitious mortar by chemical environment

Wenjing Yu, Jun Yao, Siqi Zhang, Yongguang Bu, Xiaoyan Huang, Yuhui Zhao, Xinli Mu, Wen Ni

Publisher page

Abstract

Granulated blast furnace slag-steel slag-desulfurization gypsum (GBFS-SS-DG) based low-carbon cementitious system shows great potential as a sustainable alternative to Portland cement, yet it is still challenging due to the low early compressive strength. Herein, we propose a strategy to strengthen the early strength of mortar by adjusting its chemical environment with additives. Consequently, screening available inorganic and organic early strength agents, the fluidity, setting time and mechanical strength of GBFS-SS-DG were significantly improved. With the addition of calcium formate, the compressive strength of mortar was increased by 1.93 and 11.8 MPa, respectively, at the age of 1 and 3 days. And both sodium carbonate and sodium sulfate effectively reduced the setting time of GBFS-SS-DG by 165 and 232 minutes, respectively. A series of characterization techniques revealed that the early strength agents expedited the formation rate of hydration products (ettringite and calcium aluminium silicate hydrate), lead to a denser microstructure, and significantly reduced the unreacted gypsum and porosity, thus facilitating the development of early strength of the mortar. More importantly, replacing cement with GBFS-SS-DG cementitious material reduced energy consumption and CO 2 emissions by 3.5 and 12.27 times, respectively. This work provides new insights for strengthening mortar structure strength by regulating its chemical environment with additives.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Innovations in Concrete and Construction Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Readily implementable techniques can cut annual CO2 emissions from the production of concrete by over 20%10.1088/1748-9326/11/7/074029 ↗
2. UNEP, International resource panel: Global material flows database, (2020). 〈https://www.resourcepanel.org/global-material-flows〉.
3. Climate and health damages from global concrete production10.1038/s41558-020-0733-0 ↗
4. Sustainability of waste management systems: Final disposal
5. Properties and hydration of blended cements with steelmaking slag10.1016/j.cemconres.2007.03.008 ↗
6. Steel slag and its applications in cement and concrete technology: a review10.1016/j.conbuildmat.2021.122783 ↗
7. Preparation of high performance blended cements and reclamation of iron concentrate from basic oxygen furnace steel slag10.1016/j.resconrec.2011.09.003 ↗
8. Comprehensive utilization of steel slag: a review10.1016/j.powtec.2023.118449 ↗
9. Influence of steel slag on mechanical properties and durability of concrete10.1016/j.conbuildmat.2013.06.044 ↗
10. Effect of direct electric curing on the mechanical properties, hydration process, and environmental benefits of cement-steel slag composite10.1016/j.conbuildmat.2023.133382 ↗
11. Cement substitution with secondary materials can reduce annual global CO2 emissions by up to 1.3 gigatons10.1038/s41467-022-33289-7 ↗
12. The mechanism of hydration reaction of granulated blast furnace slag-steel slag-refining slag-desulfurization gypsum-based clinker-free cementitious materials
13. Global strategies and potentials to curb CO2 emissions in cement industry10.1016/j.jclepro.2012.10.049 ↗
14. Durability behavior of steelmaking slag masonry mortars10.1016/j.matdes.2016.02.080 ↗
15. Use of iron and steel industry by-product (GGBS) in cement paste and mortar10.1016/j.resconrec.2012.09.002 ↗
16. Hydration mechanism and orthogonal optimisation of mix proportion for steel slag–slag-based clinker-free prefabricated concrete10.1016/j.conbuildmat.2019.117036 ↗
17. Green concrete with ground granulated blast-furnace slag activated by desulfurization gypsum and electric arc furnace reducing slag10.1016/j.jclepro.2020.122212 ↗
18. The mechanism of hydrating and solidifying green mine fill materials using circulating fluidized bed fly ash-slag-based agent10.1016/j.jhazmat.2021.125625 ↗
19. Microwave pre-curing of Portland cement-steel slag powder composite for its hydration properties10.1016/j.conbuildmat.2018.09.088 ↗
20. Properties and characterization of high-performance steam-cured cement-based materials modified by phase change materials10.1016/j.jclepro.2021.129669 ↗
21. Cementitious properties of super-fine steel slag10.1016/j.powtec.2013.04.016 ↗
22. The influence of inorganic admixtures on early cement hydration from the point of view of thermodynamics10.1016/j.conbuildmat.2020.119777 ↗
23. Stiffening control of cement-based materials using accelerators in inline mixing processes: possibilities and challenges10.1016/j.cemconcomp.2021.103972 ↗
24. Hydration and mechanical properties of cement-marble powder system incorporating triisopropanolamine10.1016/j.conbuildmat.2020.121068 ↗
25. Effect of TIPA on mechanical properties and hydration properties of cement-lithium slag system10.1016/j.jenvman.2020.111274 ↗
26. Understanding the role of C–S–H seed/PCE nanocomposites, triethanolamine, sodium nitrate and PCE on hydration and performance at early age10.1016/j.cemconcomp.2023.105002 ↗
27. Effect of early-strength-enhancing agents on setting time and early mechanical strength of belite-barium calcium sulfoaluminate cement10.1007/s10973-017-6837-8 ↗
28. Effects of combined accelerating admixtures on mechanical strength and microstructure of cement mortar10.1016/j.conbuildmat.2021.124642 ↗
29. Influence of the activator concentration of sodium silicate on the thermal properties of alkali-activated slag pastes10.1016/j.conbuildmat.2015.11.023 ↗
30. Preliminary interpretation of the induction period in hydration of sodium hydroxide/silicate activated slag10.3390/ma13214796 ↗
31. Hydration and properties of sodium sulfate activated slag10.1016/j.cemconcomp.2012.12.010 ↗
32. Study on the drying shrinkage of alkali-activated coal gangue-slag mortar and its mechanisms10.1016/j.conbuildmat.2019.07.258 ↗
33. Influence of activator on the strength and drying shrinkage of alkali-activated slag mortar10.1016/j.conbuildmat.2007.10.011 ↗
34. The effects of sodium sulfate on the performance of gypsum-based steel slag composites
35. GB 17671, National Standard of the People's Republic of China: Method of testing cements-determination of strength, China (2021).
36. GB 1346 · 2011
37. GB 2419, National Standard of the People's Republic of China: Test methods for flowability of cement paste, China (2005).
38. Life cycle assessment of coal gangue composite cements: From sole OPC towards low-carbon quaternary binder10.1016/j.jclepro.2023.137674 ↗
39. Effect of different sulphate carriers on Portland cement hydration in the presence of triethanolamine10.1016/j.conbuildmat.2021.123528 ↗
40. Heat-cured concrete: Improving the early strength and pore structure by activating aluminosilicate internal curing agent with triisopropanolamine10.1111/jace.16458 ↗
41. Effect of triisopropanolamine on compressive strength and hydration of steaming-cured cement-fly ash paste10.1016/j.conbuildmat.2018.10.087 ↗
42. Action of triethanolamine on the hydration of tricalcium aluminate10.1016/0008-8846(73)90060-4 ↗
43. Influence of the combination of calcium oxide and sodium carbonate on the hydration reactivity of alkali-activated slag binders10.1016/j.jclepro.2017.10.077 ↗
44. Hydration kinetics and performance of sodium carbonate-activated slag-based systems containing reactive MgO and metakaolin under carbonation10.1016/j.cemconcomp.2022.104617 ↗
45. Effects of CaCl2 on hydration and properties of lime(CaO)-activated slag/fly ash binder10.1016/j.cemconcomp.2017.09.001 ↗
46. Effects of carbonation degree on the hydration reactivity of steel slag in cement-based materials10.1016/j.conbuildmat.2023.130653 ↗
47. Effect of calcium formate on the hydration of tricalcium silicate10.1016/0008-8846(83)90050-9 ↗
48. Effects of calcium formate on early-age strength and microstructure of high-volume fly ash cement systems10.1680/jmacr.20.00118 ↗
49. Effect of triisopropanolamine on compressive strength and hydration of cement-fly ash paste10.1016/j.conbuildmat.2018.05.117 ↗
50. Effect of early strength agent on the hydration of geopolymer mortar at low temperatures
51. Influence of alkali lactates on hydration of supersulfated cement10.1016/j.conbuildmat.2019.117844 ↗
52. Effects of lithium carbonate on performances of sulphoaluminate cement-based dual liquid high water material and its mechanisms10.1016/j.conbuildmat.2017.11.130 ↗
53. Ministry of Ecology and Environment of the People's Republic of China, Solid waste - Extraction procedure for leaching toxicity - Horizontal vibration method, China, (2010) 〈https://www.mee.gov.cn/ywgz/fgbz/bz/bzwb/jcffbz/201002/t20100209_185623.shtml〉.
54. Influence of calcium hydroxide addition on arsenic leaching and solidification/stabilisation behaviour of metallurgical-slag-based green mining fill10.1016/j.jhazmat.2020.122161 ↗
55. Immobilization of hazardous ferronickel slag treated using ternary limestone calcined clay cement10.1016/j.conbuildmat.2020.118837 ↗
56. Engineering properties, sustainability performance and life cycle assessment of high strength self-compacting geopolymer concrete composites10.1016/j.conbuildmat.2023.131613 ↗
57. Techno-socio-economic aspects of Portland cement, Geopolymer, and Limestone Calcined Clay Cement (LC3) composite systems: A-State-of-Art-Review10.1016/j.conbuildmat.2023.132484 ↗