Abstract

The construction industry faces increasing environmental challenges due to freshwater scarcity and river sand depletion, prompting a shift toward sustainable materials and methods. One promising approach is the use of seawater and sea sand in concrete, which conserves freshwater, reduces river sand exploitation, and aligns with global sustainability goals by utilizing abundant local resources. This study investigates the mechanical performance and durability of reinforced concrete (RC) beams made with different combinations of seawater, sea sand, river water, and river sand, subjected to varying durations of exposure to a marine environment. The experimental program includes testing concrete cubes, cylinders, and RC beams to assess parameters such as compressive and tensile strengths, load-deflection behavior, cracking patterns, stiffness, and ultimate load capacity. The use of Sulfate Resistant Cement (SRC) and anti-corrosive coatings on the steel reinforcement was incorporated to mitigate chloride-induced corrosion and sulfate attack. Results show that concrete mixtures incorporating seawater and sea sand consistently outperformed those made with river water and river sand, particularly in terms of early-stage strength development and long-term durability. For instance, the compressive strength of seawater-sea sand mixtures was up to 24.4 % higher than their river water-river sand counterparts, while ultimate load capacities of beams were increased by up to 23.5 % in the same conditions. Beams exposed to seawater demonstrated a gradual reduction in performance with prolonged exposure, but seawater-sea sand beams maintained superior stiffness and load-carrying capacity over time compared to river water-based mixtures. Furthermore, beams using seawater and sea sand exhibited more ductile flexural failure modes, characterized by gradual crack widening and higher ductility, compared to the brittle shear failure observed in river water-river sand beams. The application of SRC and anti-corrosive coatings played a significant role in maintaining the structural integrity of the beams, limiting the detrimental effects of chloride ingress and sulfate expansion. This study highlights the potential benefits of seawater and sea sand in concrete for marine structures, especially when coupled with protective measures such as SRC and anti-corrosive coatings. Future work should explore larger-scale applications and investigate the performance of alternative cementitious materials and coatings in harsher marine environments.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Concrete Corrosion and Durability · Maritime and Coastal Archaeology · Structural Behavior of Reinforced Concrete

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Bearing capacity of seawater sea sand recycled aggregate concrete beams reinforced with glass fiber reinforced polymer bars10.1177/13694332231174256 ↗
2. Durability of seawater and sea sand concrete filled filament wound FRP tubes under seawater environments10.1016/j.compositesb.2020.108409 ↗
3. A review of low-carbon technologies and projects for the global cement industry10.1016/j.jes.2023.01.021 ↗
4. Flexural behaviour of reinforced one-part geopolymer concrete beams
5. Flexural durability of BFRP bars reinforced geopolymer-based coral aggregate concrete beams conditioned in marine environments
6. The durability of seawater sea-sand concrete beams reinforced with metal bars or non-metal bars in the ocean environment10.1177/1369433219870580 ↗
7. Flexural performance of steel bar reinforced sea sand concrete beams exposed to tidal environment10.3390/app122312321 ↗
8. Flexural behavior of seawater sea-sand concrete beams reinforced with BFRP bars/grids and BFRP-wrapped steel tubes10.1016/j.compstruct.2021.113956 ↗
9. Hybrid fibre reinforced polymer and seawater sea sand concrete structures: a systematic review on short-term and long-term structural performance10.1016/j.conbuildmat.2021.124335 ↗
10. Bearing behavior and serviceability evaluation of seawater sea-sand concrete beams reinforced with BFRP bars10.1016/j.conbuildmat.2020.118294 ↗
11. A purine derivative for the modulation of the corrosion behavior of nickel aluminum bronze in seawater: a comprehensive and in-depth investigation on the corrosion inhibition mechanism10.1016/j.corsci.2024.112340 ↗
12. Ductile, durable, and reliable alternative to FRP bars for reinforcing seawater sea-sand recycled concrete beams: steel/FRP composite bars10.1016/j.conbuildmat.2020.121264 ↗
13. Time-dependent reliability analysis of reinforced concrete beams considering marine environmental actions10.1016/j.engstruct.2023.116252 ↗
14. Stochastic analysis of flexural strength of RC beams subjected to chloride induced corrosion10.1590/1516-1439.013215 ↗
15. Synergetic optimizing particle size distributions of aggregate and cementitious materials: toward lower chloride diffusivity of concrete10.1016/j.conbuildmat.2024.136979 ↗
16. Investigation on the compressive strength, chloride migration of MK-FA-LS blended cementitious materials with electrochemical techniques
17. Effect of curing on the coupled attack of sulfate and chloride ions on low-carbon cementitious materials including slag, fly ash, and metakaolin10.1016/j.conbuildmat.2024.137307 ↗
18. A chloride diffusion model for cementitious material with pore-solution viscosity enhancement
19. A solution for sea-sand reinforced concrete beams10.1016/j.conbuildmat.2019.01.146 ↗
20. Non-destructive characterization of pore structure and chloride diffusion coefficient of cementitious materials with modified non-contact electrical resistivity method
21. Durability and long-term performance of fiber reinforced polymer (FRP) composites: a review10.1016/j.istruc.2024.105881 ↗
22. Axial compressive behavior of slender circular columns made of green concrete and double layers of steel and gfrp reinforcement10.1061/JCCOF2.CCENG-4123 ↗
23. Deterioration of mechanical properties of basalt/carbon hybrid FRP bars in SWSC under seawater corrosive environment10.1016/j.conbuildmat.2021.125979 ↗
24. Shear behaviour of seawater sea-sand coral aggregate concrete beams reinforced with FRP strip stirrups10.1016/j.engstruct.2023.116332 ↗
25. Shear failure mechanism and parametric study for seawater sea-sand engineered cementitious composites beams reinforced by FRP bars: Finite element analysis10.1016/j.conbuildmat.2023.133497 ↗
26. FRP bars reinforced seawater sea-sand engineered cementitious composites beams with various salinities: Shear behaviors and cost effectiveness
27. Design methods and recommendations for flexural concrete beams reinforced with steel-fiber composite bars10.1016/j.engstruct.2024.118139 ↗
28. Axial compressive behavior of low-alkalinity seawater sea-sand concrete column reinforced with hydrophobic longitudinal SFCBs and FRP hoops10.1016/j.engstruct.2024.118446 ↗
29. Three-fold benefits of using CO2 to cure seawater sea sand concrete10.1016/j.conbuildmat.2023.132868 ↗
30. Durability control of sea-sand concrete components utilizing strong electric field during early curing period10.1016/j.conbuildmat.2022.128221 ↗
31. Effects of seawater and sea sand on early creep of concrete under different stress levels10.1016/j.conbuildmat.2024.135765 ↗
32. Corrosion inhibition of steel reinforcements in seawater sea sand concrete by alkali-activated slag based coatings10.1016/j.conbuildmat.2023.132210 ↗
33. Olive leaf extract as a green corrosion inhibitor of reinforced concrete contaminated with seawater10.1016/j.arabjc.2020.01.016 ↗
34. Development of admixtures on seawater sea sand concrete: A critical review on Concrete hardening, chloride ion penetration and steel corrosion10.1016/j.conbuildmat.2023.134219 ↗
35. Seawater-mixed lightweight aggregate concretes with dune sand, waste glass and nanosilica: experimental and life cycle analysis10.1186/s40069-023-00613-4 ↗
36. Effect of nano cementitious composites on corrosion resistance and residual bond strength of concrete10.1016/j.rineng.2023.101064 ↗
37. Improving the thermal insulation and mechanical properties of concrete using Nano-SiO210.1016/j.rineng.2021.100303 ↗
38. Ca-LDH-modified cementitious coating to enhance corrosion resistance of steel bars
39. Enhancement of interfacial corrosion resistance between aluminum powder–modified zinc silicate–potassium silicate coating and steel bars for sand-based autoclaved aerated concrete10.1016/j.colsurfa.2024.134533 ↗
40. Influence of the profile type and bar orientation on the performance of intumescent coatings applied to steel tension bars10.1016/j.firesaf.2022.103678 ↗
41. Seawater-mixed concretes containing natural and sea sand aggregates – A review10.1016/j.rineng.2023.101457 ↗
42. Bond behavior between graphene modified epoxy coated steel bars and concrete
43. Investigation of bond behavior between waterborne epoxy-coated steel reinforcing bars (WECR) and concrete
44. Mechanical properties and durability of FRP-reinforced coral aggregate concrete structures: a critical review
45. BFRP bars reinforced geopolymer-based coral aggregate concrete beams with sustainable and high seawater erosion resistance: Flexural durability, economic, and ecological analysis10.1016/j.engstruct.2025.119910 ↗
46. Evaluation of the use of Egyptian black sand for water reuse10.1088/1757-899X/698/2/022072 ↗
47. Heavy minerals, including monazite, in Egypt’s black sand deposits10.1016/0022-5088(89)90013-1 ↗
48. Evaluation of sea water as a mixing/curing of the concrete
49. Effects of sulphate resistant cement on marine structural concretes10.1016/j.matpr.2021.10.326 ↗
50. BS EN 197-1, “Composition, specifications and conformity criteria for common cements,” British Standards Institution, 2011.
51. ECP 203, “Egyptian Code for the Design and Construction of Concrete Structures,” Tests guide, part II (aggregates test), pp. 2–13, 2018.
52. BS EN 12390-3, “Testing hardened concrete - Compressive strength of test specimens,” British Standards Institution, 2019.
53. ASTM C496, “Standard Test Method for Splitting Tensile Strength of Cylindrical Concrete Specimens,” American Society for Testing and Materials, 2017.
54. Compressive performance and analytical modeling of early strength seawater sea sand engineered cementitious composites
55. Fresh, hardened, durability and microstructure properties of seawater concrete: a systematic review10.1016/j.jcou.2024.102815 ↗
56. Effects of seawater and sea sand on early creep of concrete under different stress levels10.1016/j.conbuildmat.2024.135765 ↗