Concrete carbonation in tropical urban and urban/marine environments after 20 years of natural exposure
Source abstract
Abstract
This work is part of the DURACON project, which seeks to characterize the durability of concrete exposed to environmental conditions prevailing in Ibero-America and is based on the exposure of unreinforced and reinforced concrete specimens in marine and urban environments in each participating Ibero-American country. This research presents the results obtained from exposing unreinforced and steel-reinforced concrete specimens to prevailing environmental conditions in twelve natural exposure sites in Mexico during an exposure period of approximately 20 years to determine an empirical model that allows predicting the value of the carbonation rate, k′ CO2, as a function of the nth-root of time (NRT) for the concretes evaluated. The concrete specimens, plain and reinforced, exposed to the elements in these cities were manufactured with two types of concrete, one with a w/c ratio = 0.65 and the other with a w/c ratio = 0.45. The tests mainly focused on measuring the concrete carbonation front depth during the ∼ 20 years of exposure and the measurement of environmental parameters at the exposure sites, such as temperature, relative humidity, rainfall, and atmospheric CO 2 concentration. The electrochemical parameters of the reinforcing steel (half-cell potential, Ecorr, and current density, icorr) in the reinforced specimens were also obtained after ∼ 20 years of exposure to corroborate which sites showed lower or higher corrosion activity. This model to obtain k′ CO2 as a function of the environmental parameters of the Mexican exposure sites and the physical properties of the concretes was compared with the value of k CO2 obtained from the square root of time (SRT) model. It was found that the k′ CO2 values were 30 % higher on average than the k CO2 obtained with the empirical SRT equation. However, it should be noted that k′ CO2 must be linked to the corresponding n th-root of time, whereas the value of n to obtain k CO2 is constant and equal to ½. An agreement was also obtained between the probability of activation of the reinforcing steel, using the corrosion parameters (E corr and icorr), and the probability of e CO2 ≤ 15 mm (lowest concrete cover used in this study).
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete Corrosion and Durability · Microbial Applications in Construction Materials · Infrastructure Maintenance and Monitoring
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Manual of Inspecting · 1998
2. Manual of Rehabilitation of Concrete Structures · 2003
3. O. Troconis de Rincón and DURACON Collaborators, Effect of the marine environment on reinforced concrete durability in Iberoamerican countries: DURACON project/CYTED, Corrosion Science, v. 49, pp. 2832-2843, 2007.10.1016/j.corsci.2007.02.009 ↗
4. Concrete Carbonation in Ibero-American Countries DURACON Project: Six-year Evaluation10.5006/1385 ↗
5. Reinforced Concrete Durability in Marine Environments DURACON Project: Long-Term Exposure10.5006/1893 ↗
6. S. Mindess, J.F. Young, and D. Darwin, Concrete, 2nd ed., Prentice Hall, Pearson Education, Inc., Upper Sadle River, NJ, 07458, USA, 2003.
7. C. Andrade Manual de Inspección de obras dañadas por corrosión de varillas, España, ACOR, Anes Gráficas, S. A., septiembre, 1988 (In Spanish).
8. Concrete Cracking by localized Steel Corrosion – Geometric Effects
9. Residual Life of Corroding Reinforced Concrete Structures in Marine Environment10.1061/(ASCE)0899-1561(2003)15:4(344) ↗
10. Moreno · 1999
11. Artificial neural network model to estimate the long-term carbonation depth of concrete exposed to natural environments
12. NMX-C-414-ONNCCE-2017 “Industria de la Construcción - Cementantes Hidráulicos - Especificaciones y Métodos de Ensayo,” Organismo Nacional de Normalización y Certificación de la Construcción y Edificación, S.C., Ceres 7, Crédito Constructor, Benito Juárez, CP 03940, Ciudad de México, México.
13. ASTM C136. Standard Test Method for Sieve Analysis of Fine and Coarse Aggregates, American Standard for Testing Materials International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA, 19428-2959 USA, 2006.
14. ASTM C-39. Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens. American Standard for Testing Materials International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA, 19428-2959 USA, 2021.
15. ASTM C-496. Standard Test Method for Splitting Tensile Strength of Cylindrical Concrete Specimens, American Standard for Testing Materials International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA, 19428-2959 USA, 2017.
16. ASTM C-469. Standard Test Method for Static Modulus of Elasticity and Poisson's Ratio of Concrete in Compression, American Standard for Testing Materials International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA, 19428-2959 USA, 2022.
17. ASTM C-642. Standard Test Method for Density, Absorption, and Voids in Hardened Concrete, American Standard for Testing Materials International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA, 19428-2959 USA, 2021.
18. G. Fagerlund, Methods of characterization of pore structure, in 3 contributions to RILEM Committee pore structure and properties of materials, Report 41, Lund, Sweden, 1973.
19. ASTM C-1876. Standard Test Method for Bulk Electrical Resistivity or Bulk Conductivity of Concrete, American Standard for Testing Materials International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA, 19428-2959 USA, 2019.
20. ASTM C876. Standard Test Method for Half-Cell Potentials of Uncoated Reinforcing Steel in Concrete, American Standard for Testing Materials International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA, 19428-2959 USA, 1999.
21. U. Angst, F. Moro, M. Geiker, S. Kessler, H. Beushausen, C. Andrade, J. Lahdensivu, A. Koloio, K. Imamoto, Sv Greve-Dierfeld, M. SerdarRILEM Tech 5 Lett , 2020, , 85–100.10.21809/rilemtechlett.2020.127 ↗
22. Parrott · 1987
23. A review on effects of curing, sheltering, and CO2 concentration upon natural carbonation of concrete10.1016/j.conbuildmat.2016.09.056 ↗
24. Experimental investigations on the effect of concrete quality, exposure conditions and duration of initial moist curing on carbonation rate in concretes exposed to urban, inland environment10.1016/j.conbuildmat.2020.118443 ↗
25. H.K. Wierig. Longtime studies on the carbonation of concrete under normal outdoor exposure, Proc., RILEM Seminar on the Durability of Concrete Structures under Normal Outdoor Exposure, Institut für Baustoffkunde und Materialprüfung der Universität, Hannover, (1984), pp. 239–249.
26. Evaluation of pathological problems associated with carbonation and sulfates in a concrete tower with more than 50 years in service
27. López Celis · 2006
28. A. Torres Acosta, J.T. Pérez Quiroz, P.Castro Borges, C. Andrade, N. Rebolledo Ramos, F.Almeraya Calderón, C. Gaona Tiburcio, E.I. Moreno, T. Pérez López, M. Sosa Bas, M. Martínez Madrid, W. Martínez Molina, E. Alonso Guzmán. “Concrete carbonation in urban and urban/marine environments in Mexico and Spain,” 3rd National Congress ALCONPAT 2008, Chihuahua; Chihuahua, Mexico, 12-14 November, 2008. (In Spanish).
29. A.A. Torres-Acosta, A.A., P.Y. González-Calderón. “Opuntia Ficus Indica (OFI) mucilage as corrosion inhibitor of steel in CO2-contaminated mortar,” Materials MDPI, Special Issue "New Findings of Portland Cementitious Materials," Vol. 14, Issue 5, (2021) 1316, https://doi.org/10.3390/ma14051316.10.3390/ma14051316 ↗
30. Considerations to avoid corrosion rate estimate error of the reinforcing steel if based only on concrete’s electrical resistivity