journal article·2022-11Open access

The effect of slag chemistry on CO2 binding capacity of C3S-slag (-gypsum) system

Yu Zhang, Oğuzhan Çopuroğlu

Abstract

In this paper, the authors investigated the correlation between slag chemistry and CO2 binding capacity of the blended system. To simplify the composition of mixture, model paste containing C3S, slag covering the common composition range and gypsum was employed. After accelerated carbonation test, three CO2-binding phases were identified in the system as: carbonated Ca-Al AFm phases, carbonated hydrotalcite-like phase, and calcium carbonate, irrespective of slag chemistry and the addition of gypsum. On the other hand, carbonated Ca-Al AFm phases played a minor role in absorbing CO2, sharing less than 5% of CO2 among all carbonate phases. Hydrotalcite-like phase was able to bind up to ∼10% CO2, depending on the Mg/Al atomic ratio of raw slag. CaCO3, originated from the carbonation of portlandite and C−S−H gel phase, took up more than 85% CO2 after carbonation. Moreover, the carbonation degree of C−S−H gel phase was found to be negatively related with the Al2O3 content and Ca/Si ratio of raw slag.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Layered Double Hydroxides Synthesis and Applications · Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. Advances in alternative cementitious binders10.1016/j.cemconres.2010.11.012 ↗
2. The greenhouse gas implications of using ground granulated blast furnace slag as a cement substitute10.1016/j.jclepro.2015.02.082 ↗
3. Environmental impact analysis of blast furnace slag applied to ordinary Portland cement production10.1016/j.jclepro.2015.12.071 ↗
4. Benefits of slag and fly ash10.1016/0950-0618(95)00014-3 ↗
5. Blast furnace slag cement concrete with high slag content (CEM III/B)–Experiences with the durability in The Netherlands since the 1920’s
6. Utilization and efficiency of ground granulated blast furnace slag on concrete properties–A review10.1016/j.conbuildmat.2015.12.153 ↗
7. Effect of supplementary cementing materials on concrete resistance against carbonation and chloride ingress10.1016/S0008-8846(99)00249-5 ↗
8. Carbonation of concrete containing mineral admixtures10.1061/(ASCE)0899-1561(2003)15:2(134) ↗
9. Carbonation of CH and C-S–H in composite cement pastes containing high amounts of BFS10.1016/j.cemconres.2009.10.020 ↗
10. Effects of different mineral admixtures on carbonation resistance of lightweight aggregate concrete10.1016/j.conbuildmat.2013.02.038 ↗
11. Service life of metakaolin-based concrete exposed to carbonation: Comparison with blended cement containing fly ash, blast furnace slag and limestone filler10.1016/j.cemconres.2017.04.013 ↗
12. Carbonation resistance of cements containing supplementary cementitious materials and its relation to various parameters of concrete10.1016/j.conbuildmat.2018.05.162 ↗
13. Development of porosity of cement paste blended with supplementary cementitious materials after carbonation10.1016/j.conbuildmat.2017.03.176 ↗
14. Understanding the carbonation of concrete with supplementary cementitious materials: a critical review by RILEM TC 281-CCC10.1617/s11527-020-01558-w ↗
15. Lagerblad, B., Carbon dioxide uptake during concrete life cycle: State of the art. 2005: Swedish Cement and Concrete Research Institute Stockholm.
16. Progressive changes in the structure of hardened C3S cement pastes due to carbonation10.1111/j.1151-2916.1991.tb06859.x ↗
17. Assessment of the protective effect of carbonation on portlandite crystals10.1016/j.cemconres.2015.04.001 ↗
18. Real-time investigation of reaction rate and mineral phase modifications of lime carbonation10.1016/j.conbuildmat.2012.04.036 ↗
19. Carbonation of C-S–H and C–A–S–H samples studied by 13C, 27Al and 29Si MAS NMR spectroscopy10.1016/j.cemconres.2015.01.019 ↗
20. Study of carbonation rate of synthetic CSH by XRD
21. Influence of water vapour and carbon dioxide on free lime during storage at 80 C, studied by Raman spectroscopy10.1016/j.saa.2013.04.033 ↗
22. Polymorphism of CaCO3, precipitated in a constant-composition environment10.1002/aic.690440810 ↗
23. The role of sulfate groups in controlling CaCO3 polymorphism10.1016/j.gca.2010.08.010 ↗
24. Composition and microstructure of 20-year-old ordinary Portland cement–ground granulated blast-furnace slag blends containing 0 to 100% slag10.1016/j.cemconres.2010.02.012 ↗
25. Hydration of slag-blended cements10.1016/j.cemconcomp.2012.05.007 ↗
26. The hydration of slag, part 2: reaction models for blended cement10.1007/s10853-006-0874-1 ↗
27. Carbonation behaviors of calcium silicate hydrate (CSH): Effects of aluminum10.1016/j.conbuildmat.2022.126825 ↗
28. Wu, B. and G. Ye. Carbonation mechanism of different kind of CSH: rate and products. in Int. RILEM Conference on Materials, Systems and Structures in Civil Engineering 2016-Segment on Concrete with Supplementary Cementitious Materials. 2016. RILEM.
29. Effect of carbonation in supercritical CO2 on the properties of hardened cement paste of different alkalinity10.1016/j.conbuildmat.2016.07.040 ↗
30. Microstructural changes of hydrated cement blended with fly ash upon carbonation10.1016/j.cemconres.2020.106192 ↗
31. Hydration and carbonation of monoclinic C2S and C3S studied by Raman spectroscopy10.1002/jrs.1599 ↗
32. Growth of calcium carbonate induced by accelerated carbonation of tricalcium silicate10.1021/acssuschemeng.0c02260 ↗
33. The effect of slag chemistry on the reactivity of synthetic and commercial slags10.1016/j.conbuildmat.2022.127493 ↗
34. Effect of silicate modulus and metakaolin incorporation on the carbonation of alkali silicate-activated slags10.1016/j.cemconres.2010.02.003 ↗
35. Hydration of alite containing aluminium10.1179/1743676110Y.0000000007 ↗
36. The influence of sodium salts and gypsum on alite hydration10.1016/j.cemconres.2015.04.015 ↗
37. Investigation of the carbonation front shape on cementitious materials: Effects of the chemical kinetics10.1016/j.cemconres.2007.04.002 ↗
38. Measurement methods of carbonation profiles in concrete: Thermogravimetry, chemical analysis and gammadensimetry10.1016/j.cemconres.2007.04.015 ↗
39. Investigation of the carbonation mechanism of CH and CSH in terms of kinetics, microstructure changes and moisture properties10.1016/j.cemconres.2013.11.015 ↗
40. Phase evolution, micromechanical properties, and morphology of calcium (alumino) silicate hydrates C-(A-) SH under carbonation10.1016/j.cemconres.2021.106683 ↗
41. Structural features of C-S–H (I) and its carbonation in air—a Raman spectroscopic study. Part II: carbonated phases10.1111/j.1551-2916.2006.01429.x ↗
42. Calcite, vaterite and aragonite forming on cement hydration from liquid and gaseous phase10.1023/A:1025158213560 ↗
43. The hydration of slag, part 2: reaction models for blended cement10.1007/s10853-006-0874-1 ↗
44. De Belie, N.e.a., Properties of fresh and hardened concrete containing supplementary cementitious materials. Vol. 25. 2018: Springer.10.1007/978-3-319-70606-1 ↗
45. Physico-chemical properties of synthetic hydrotalcites in relation to composition10.1346/CCMN.1980.0280107 ↗
46. Anion-exchange properties of hydrotalcite-like compounds10.1346/CCMN.1983.0310409 ↗
47. Synthesis of anionic clay minerals (mixed metal hydroxides, hydrotalcite)10.1016/0167-2738(86)90067-6 ↗
48. The influence of TiO2 on the structure and derivative properties of silicate melts
49. FTIR, Raman and NMR investigation of CaO–SiO2–P2O5 and CaO–SiO2–TiO2–P2O5 glasses10.1016/j.jnoncrysol.2015.04.017 ↗
50. Effect of Al2O3 on the viscosity and structure of calcium silicate-based melts containing Na2O and CaF210.1016/j.jnoncrysol.2012.04.009 ↗
51. Surface kinetics of nitrogen dissolution and its correlation to the slag structure in the CaO-SiO2, CaO-Al2O3, and CaO-SiO2-Al2O3 slag system10.1016/j.jnoncrysol.2011.03.023 ↗
52. Relationship between NMR 29 Si chemical shifts and FT-IR wave numbers in calcium silicates
53. Carbonation behavior of hydraulic and non-hydraulic calcium silicates: potential of utilizing low-lime calcium silicates in cement-based materials10.1007/s10853-016-9909-4 ↗
54. Kinetics of enforced carbonation of cement paste10.1016/j.cemconres.2020.106013 ↗
55. Thermodynamic properties of Portland cement hydrates in the system CaO–Al2O3–SiO2–CaSO4–CaCO3–H2O10.1016/j.cemconres.2007.06.002 ↗
56. Thermodynamic equilibrium calculations in cementitious systems10.1617/s11527-010-9592-x ↗
57. Carbonation of calcium sulfoaluminate mortars10.1016/j.cemconcomp.2017.03.003 ↗
58. The thermal decomposition of Mg–Al hydrotalcites: effects of interlayer anions and characteristics of the final structure. Chemistry–A10.1002/1521-3765(20021216)8:24<5571::AID-CHEM5571>3.0.CO;2-R ↗
59. Thermogravimetric analysis-mass spectrometry (TGA-MS) of hydrotalcites containing CO3 2−, NO3−, Cl−, SO4 2− or ClO4−
60. Structure and reactivity of synthetic CaO-Al2O3-SiO2 glasses10.1016/j.cemconres.2019.03.004 ↗
61. The Influence of Limestone and Al2O3 Content in the Slag on the Performance of the Composite Cements10.1016/j.proeng.2015.06.164 ↗
62. Ability of the R3 test to evaluate differences in early age reactivity of 16 industrial ground granulated blast furnace slags (GGBS)10.1016/j.cemconres.2020.105998 ↗
63. Taylor, H.F., Cement chemistry. Vol. 2. 1997: Thomas Telford London.10.1680/cc.25929 ↗
64. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag — Part II: Effect of Al2O310.1016/j.cemconres.2011.08.005 ↗
65. The role of the alumina content of slag, plus the presence of additional sulfate on the hydration and microstructure of Portland cement-slag blends10.1016/j.cemconres.2014.07.018 ↗
66. Richardson · Cement and Concrete Research · 2004 · 34 · 173310.1016/j.cemconres.2004.05.034 ↗
67. Effects of Ca/Si ratio, aluminum and magnesium on the carbonation behavior of calcium silicate hydrate10.3390/ma12081268 ↗
68. The role of aluminium in CASH during chemical attack on concrete
69. Calcium alumino-silicates hydrates (CASH) carbonation kinetics
70. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag—Part I: Effect of MgO10.1016/j.cemconres.2011.05.002 ↗
71. MgO content of slag controls phase evolution and structural changes induced by accelerated carbonation in alkali-activated binders10.1016/j.cemconres.2013.12.003 ↗
72. Structural evolution of synthetic alkali-activated CaO-MgO-Na2O-Al2O3-SiO2 materials is influenced by Mg content10.1016/j.cemconres.2017.05.006 ↗
73. Variability of the nitrogen surface area of hydrated cement paste10.1016/0008-8846(76)90058-2 ↗
74. High CO2 Storage Capacity in Alkali-Promoted Hydrotalcite-Based Material. In Situ Detection of Reversible Formation of Magnesium Carbonate. Chemistry–A10.1002/chem.201000687 ↗
75. Rapid exchange between atmospheric CO2 and carbonate anion intercalated within magnesium rich layered double hydroxide10.1021/am5060405 ↗
76. Carbonation behavior of calcium silicate hydrate (CSH): Its potential for CO2 capture10.1016/j.cej.2021.134243 ↗