Influence of warm rolling and heat treatment in the alpha-gamma area of a three-layer strip on the appearance of ears during cup deep drawing
Source abstract
Abstract
Eearing is the most common defect that may occur during cup deep drawing. A removal of excess material from drawn parts causes a wastage of the material. Therefore, it is necessary to minimize earing as much as possible. A negative effect of warm rolling and annealing in the alpha-gamma area on the earing in the case of an explosive-welded three-layer strip consisting of CuZn10 clad layers and the central DC04 steel layer is described in this article. Warm rolling of all samples started in the alpha-gamma area (850 C) of the steel layer. Some of them were reheated to the same temperature after each pass while others were not reheated after the last three passes. In both cases, ears appeared. The final annealing was carried out at temperatures between 700-930 C. Regardless of the thermomechanical history of the samples, the final annealing in the alpha-gamma area (750, 800 and 850) C caused earing, even in the case of a sample exposed to a higher degree of cold deformation, including intermediate recrystalization annealing at 700 C, which, after the final annealing at 700 C, does not have the tendency to create ears. Because of this negative effect, annealing and prolonged warm rolling in the alpha-gamma area should be avoided. Key words: three-
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgy and Material Forming · Metal Forming Simulation Techniques · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.