Development and design of composite cementitious material at long-time circular elevated temperature in metallurgy environment
Source abstract
Abstract
Abstract A new approach conducted the development and design of materials from the problems, requirements and methods in engineering was analyzed carefully and verified by a two years trial in actual engineering. In this case, decomposition of hydrates, reduction of cohesive force and expansion which was caused by temperature change and water evaporation were regarded as the major reasons for thermal damage of concrete structure at long-time circular elevated temperature in metallurgy environment. Moreover, five material modification methods were adopted to enhance the thermal durability, which were the modification of composition and microstructure of hydrates, extra new binders, the revisement of porosity and pore distribution, the increase of anti-crack property, and the supplement of hydrophobic performance, respectively. Different mix proportions of cement mortar were designed and the effect on thermal durability were analyzed by mechanical experiments and microstructure observations. Ultimately, a new composite cementitious material was developed and proved by the engineering trial.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fire effects on concrete materials · Concrete and Cement Materials Research · Concrete Properties and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. The application of materials science to the design of engineering alloys10.1016/0025-5416(74)90158-X ↗
2. Comments on “The application of materials science to the design of engineering alloys, a review”10.1016/0025-5416(75)90150-0 ↗
3. Reply to comments on “The application of materials science to the design of engineering alloys, a review”10.1016/0025-5416(75)90151-2 ↗
4. Optimization of material and shape for nuclear microprobe apertures10.1016/0168-583X(96)00054-7 ↗
5. Materials design in the performance of all-ceramic crowns10.1016/j.biomaterials.2003.09.050 ↗
6. Structural optimization of ferromagnetic materials based on the magnetic reluctivity for magnetic field problems10.1016/j.cma.2008.04.019 ↗
7. Material considerations in product design: a survey on crucial material aspects used by product designers10.1016/j.matdes.2007.06.002 ↗
8. Identification of nonlinear membership function for failure of structural material and its application to structural optimization10.1016/0165-0114(94)90298-4 ↗
9. Topology optimization for the design of periodic microstructures composed of electromagnetic materials10.1016/j.finel.2008.10.006 ↗
10. Optimization of the material structure and composition of cement based composites10.1016/0958-9465(96)00018-2 ↗
11. The role of materials identification and selection in engineering design10.1016/j.matdes.2005.05.003 ↗
12. The effects of high temperature on compressive and flexural strengths of ordinary and high-performance concrete10.1016/j.firesaf.2005.12.002 ↗
13. Self-consolidating concrete subjected to high temperature mechanical and physicochemical properties10.1016/j.cemconres.2009.08.001 ↗
14. Effect of temperature on structural quality of the cement paste and high-strength concrete with silica fume10.1016/j.nucengdes.2005.05.011 ↗
15. The use of thermal analysis in assessing the effect of temperature on a cement paste10.1016/j.cemconres.2004.06.015 ↗
16. Experimental study of micro/macro crack development and stress–strain relations of cement-based composite materials at elevated temperatures10.1016/j.cemconres.2003.08.029 ↗
17. Effects of stress during heating on strength and stiffness of concrete at elevated temperature10.1016/j.cemconres.2010.08.016 ↗
18. Residual fracture energy of cement paste, mortar and concrete subject to high temperature10.1016/j.tafmec.2005.11.007 ↗
19. Comparison of the strength and durability performance of normal- and high-strength pozzolanic concretes at elevated temperatures10.1016/S0008-8846(01)00580-4 ↗
20. Influence of PFA on cracking of concrete and cement paste after exposure to high temperatures10.1016/S0008-8846(03)00216-3 ↗
21. Residual strength and pore structure of high-strength concrete and normal strength concrete after exposure to high temperatures10.1016/S0958-9465(98)00034-1 ↗
22. Compressive behavior of fiber reinforced high-performance concrete subjected to elevated temperatures10.1016/j.cemconres.2004.02.011 ↗
23. Permeability of high-performance concrete subjected to elevated temperature (600°C)10.1016/j.conbuildmat.2008.09.023 ↗
24. On residual strength of high-performance concrete with and without polypropylene fibres at elevated temperatures10.1016/j.firesaf.2005.11.004 ↗
25. Mechanical properties and microstructure of high strength concrete containing polypropylene fibres exposed to temperatures up to 200°C10.1016/j.cemconres.2005.03.007 ↗
26. Thermal and mechanical properties of fiber reinforced high performance self-consolidating concrete at elevated temperatures10.1016/j.cemconres.2011.06.012 ↗
27. Phase studies of pozzolanic stabilized calcium silicate hydrates at 180°C10.1016/j.cemconres.2004.05.021 ↗
28. Thermal degradation of polymer concrete10.1016/0950-0618(87)90054-7 ↗
29. Thermal characteristics of high-strength polymer–cement composites with lightweight aggregates and polypropylene fiber10.1016/j.conbuildmat.2011.03.023 ↗
30. Viscosity-enhancing admixtures for cement-based materials – an overview10.1016/S0958-9465(98)80006-1 ↗
31. Cement hydration and microstructure formation in the presence of water-soluble polymers10.1016/j.cemconres.2008.10.003 ↗
32. Experimental evidence of a moisture clog effect in cement-based materials under temperature10.1016/j.cemconres.2009.07.015 ↗
33. Chinese National Standard GB 275-2007. Common Portland cement, Beijing, China [in Chinese].
34. Chinese National Standard GB 18046-2000. Ground granulated blast furnace slag used for cement and concrete, Beijing, China [in Chinese].
35. Chinese National Standards GB/T 17671-1999. Method of testing cements – determination of strength, Beijing, China [in Chinese].
36. Chinese National Standards GB/T 2419-2005. Test method for fluidity of cement mortar, Beijing, China [in Chinese].
37. Influence of EVA and acrylate polymers on some mechanical properties of cementitious repair mortars10.1016/j.conbuildmat.2009.02.021 ↗
38. Study on the performance of a new type of water-repellent admixture for cement mortar10.1016/j.cemconres.2004.02.019 ↗