Mechanical Properties and Fatigue Life Estimation of Selective-Laser-Manufactured Ti6Al4V Alloys in a Comparison Between Annealing Treatment and Hot Isostatic Pressing
Source abstract
Abstract
Selective laser melting (SLM) offers a novel approach for manufacturing intricate structures, broadening the application of titanium alloy parts in the aerospace industry. After the build period, heat treatments of annealing (AT) and hot isostatic pressing (HIP) are often implemented, but a comparison of their mechanical performances based on the specimen orientation is still lacking. In this study, horizontally and vertically built Ti6Al4V SLM specimens that underwent the aforementioned treatments, together with their microstructural and defect characteristics, were, respectively, investigated using metallography and X-ray imaging. The mechanical properties and failure mechanism, via fracture analysis, were obtained. The critical factors influencing the mechanical properties and the correlation of the fatigue lives and failure origins were also estimated. The results demonstrate that the mechanical performances were determined by the α-phase morphology and defects, which included micropores and fewer large lack-of-fusion defects. Following the coarsening of the α phase, the strength decreased while the plasticity remained stable. With the discrepancy in the defect occurrence, anisotropy and scatter of the mechanical performances were introduced, which was significantly alleviated with HIP treatment. The fatigue failure origins were governed by defects and the α colony, which was composed of parallel α phases. Approximately linear relationships correlating fatigue lives with the X-parameter and maximum stress amplitude were, respectively, established in the AT and HIP states. The results provide an understanding of the technological significance of the evaluation of mechanical properties.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Aero Engine Corporation of China Beijing Institute of Aeronautical Materials, Beijing 100095, China
Beijing Key Laboratory of Aeronautical Materials Testing and Evaluation, Beijing 100095, China
Key Laboratory of Aeronautical Materials Testing and Evaluation, Aero Engine Corporation of China, Beijing 100095, China
Funding
AECC Science and Technology Innovation Platform Project · National Major Science and Technology Project
References (41)
Show source-provided references
1. Production of Ti-6Al-4V acetabular shell using selective laser melting: Possible limitations in fabrication10.1108/RPJ-11-2015-0159 ↗
2. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: Processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
3. Titanium alloys for aerospace applications10.1002/adem.200310095 ↗
4. Consolidation phenomena in laser and powder-bed based layered manufacturing10.1016/j.cirp.2007.10.004 ↗
5. Optimisation of process parameters to address fundamental challenges during selective laser melting of Ti-6Al-4V: A review10.1016/j.ijmachtools.2018.01.003 ↗
6. A study of the microstructural evolution during selective laser melting10.1016/j.actamat.2010.02.004 ↗
7. Metal fabrication by additive manufacturing using laser and electron beam melting technologies10.1016/S1005-0302(12)60016-4 ↗
8. Microstructures and mechanical properties of Ti6Al4V parts fabricated by selective laser melting and electron beam melting10.1007/s11665-013-0658-0 ↗
9. Microstructure and mechanical property of selective laser melted Ti6Al4V dependence on laser energy density10.1108/RPJ-12-2015-0193 ↗
10. On the texture formation of selective laser melted Ti-6Al-4V10.1007/s11661-014-2218-0 ↗
11. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti-6Al-4V10.1016/j.msea.2013.04.099 ↗
12. Gibson, I., Rosen, D.W., and Stucker, B. (2015). Additive Manufacturing Technologies, Springer.10.1007/978-1-4939-2113-3 ↗
13. A review of defect modeling in laser material processing
14. Gong, H., Gu, H., Zeng, K., Dilip, J.J.S., Pal, D., and Stucker, B. (2014, January 4–6). Melt pool characterization for selective laser melting of Ti-6Al-4V pre-alloyed powder. Proceedings of the 25th Annual International Solid Freeform Fabrication Symposium, Austin, TX, USA.
15. Heat treatment of Ti6Al4V produced by selective laser melting: Microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
16. Experimental study on mechanical properties of laser powder bed fused Ti-6Al-4V alloy under post-heat treatment10.1016/j.engfracmech.2022.108264 ↗
17. Tensile behavior of Ti-6Al-4V alloy fabricated by selective laser melting: Effects of microstructures and as-built surface quality
18. Effect of the build orientation on the mechanical properties and fracture modes of L-PBF Ti-6Al-4V10.1016/j.msea.2014.07.086 ↗
19. A review of the fatigue properties of additively manufactured Ti-6Al-4V
20. Fatigue performance of laser additive manufactured Ti-6Al-4V in very high cycle fatigue regime up to 109 cycles10.3389/fmats.2015.00072 ↗
21. Microstructure and mechanical behavior of Ti-6Al-4V produced by rapid-layer manufacturing for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
22. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: Fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
23. Investigation on the effect of heat treatment and process parameters on the tensile behaviour of SLM Ti-6Al-4V parts10.1007/s00170-018-3162-8 ↗
24. Effect of self-accommodation on α/α boundary populations in pure titanium10.1016/S1359-6454(03)00035-1 ↗
25. Effect of crystallographic orientation on mechanical anisotropy of selective laser melted Ti-6Al-4V alloy10.1016/j.matchar.2017.01.014 ↗
26. Fatigue life of additively manufactured Ti-6Al-4V in the very high cycle fatigue regime
27. Application of X-ray CT method for discontinuity and porosity detection in 316L stainless steel parts produced with SLM technology10.1016/j.acme.2014.02.003 ↗
28. Microstructure-properties relationships of Ti-6Al-4V parts fabricated by selective laser melting10.1007/s40684-018-0062-1 ↗
29. Fatigue performance evaluation of selective laser melted Ti-6Al-4V10.1016/j.msea.2014.01.041 ↗
30. Porosity regrowth during heat treatment of hot isostatically pressed additively manufactured titanium components10.1016/j.scriptamat.2016.05.002 ↗
31. Additive manufacturing of fatigue resistant materials: Challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
32. Fatigue strength of a Ti-6Al-4V alloy produced by selective laser melting10.1134/S0036029516100049 ↗
33. Analysis of fatigue properties and failure mechanisms of Ti6Al4V in the very high cycle fatigue regime using ultrasonic technology and 3D laser scanning vibrometry10.1016/j.ultras.2013.03.002 ↗
34. Evaluation of fatigue crack propagation behavior in Ti-6Al-4V manufactured by selective laser melting10.1016/j.ijfatigue.2017.07.014 ↗
35. Laser powder-bed fusion additive manufacturing: Physics of complex melt flow and forming mechanisms of pores, spatter, and denudation zones10.1016/j.actamat.2016.02.014 ↗
36. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium10.1016/j.msea.2013.11.038 ↗
37. On the nature and crystallographic orientation of subsurface cracks in high cycle fatigue of Ti-6Al-4V10.1007/BF02656635 ↗
38. Fatigue life evaluation of Ti-6Al-4V welded joints manufactured by electron beam melting10.1111/ffe.13490 ↗
39. Murakami, Y. (2002). Metal Fatigue: Effects of Small Defects and Nonmetallic Inclusions, Academic Press.
40. High- and low-cycle fatigue behavior of additively manufactured Ti6Al4V and influence of surface finish10.1016/j.engfailanal.2025.109825 ↗
41. Pertuz-Comas, A.D., González-Estrada, O.A., Martínez-Díaz, E., Villegas-Bermúdez, D.F., and Díaz-Rodríguez, J.G. (2023). Strain-based fatigue experimental study on Ti-6Al-4V alloy manufactured by electron beam melting. J. Manuf. Mater. Process., 7.10.3390/jmmp7010025 ↗