Abstract
Salt crystallization is one of the most common causes of decay in porous building materials. Plasters and renders, mainly due to their location at the surface of walls, where most often salt accumulation occurs, are particularly subjected to salt decay. Despite the relevance of the problem, there are no standard salt weathering tests for the assessment of the durability of plasters and renders against salt decay. This research proposes a salt weathering procedure, based on an adaptation of the RILEM TC 271-ASC recommendation, and it validates it by applying it to three plaster types (based on hydrated lime, natural hydraulic lime and hydrated lime-cement). Combined stone/plaster specimens are prepared and contaminated with 10 % (weight salt/weight solution) sodium sulphate and sodium chloride solutions. The damage development is assessed by visual and photographic monitoring, gravimetric measurements of the material loss, assessment of salt distribution in the specimens, and SEM observations supported by EDX mapping on thin sections. The results show that the test procedure is effective in causing damage in the tested plasters, within the time period of the test (about 4 months), and that damage increases with subsequent cycles. The decay severity and type differ depending on type of salt and/or of plaster. Suggestions for further improvement of the procedure are provided. • Proposal for an accelerated salt weathering test for assessment of plaster durability. • The test is based on an adaptation of the RILEM TC 271-ASC procedure. • The test has been validated on 3 plaster types, applied on a stone substrate. • The test has been proven effective to induce damage in the studied plasters. • The decay severity and type differ depending on type of salt and/or of plaster.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Building materials and conservation · Hygrothermal properties of building materials · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Salts in Masonry: An Overview of the Problem
2. Salt weathering: a selective review10.1144/GSL.SP.2002.205.01.05 ↗
3. Goudie · 1997
4. A coupled multiphase model for hygrothermal analysis of masonry structures and prediction of stress induced by salt crystallization10.1016/j.conbuildmat.2012.12.045 ↗
5. A multi-scale approach for the analysis of the mechanical effects of salt crystallisation in porous media10.1016/j.ijsolstr.2017.08.009 ↗
6. Towards a more effective and reliable salt crystallization test for porous building materials: state of the art
7. Predicting salt damage in practice: a theoretical insight into laboratory tests10.21809/rilemtechlett.2017.41 ↗
8. Salt crystallization damage: how realistic are existing ageing tests?
9. Recommendation of RILEM TC 271-ASC: New accelerated test procedure for the assessment of resistance of natural stone and fired-clay brick units against salt crystallization
10. A new accelerated salt weathering test by RILEM TC 271-ASC: preliminary round robin validation10.1617/s11527-022-02067-8 ↗
11. K. Tuutti, Corrosion of steel in concrete, Stockholm, 1982.
12. Chemo-mechanics of salt damage in stone10.1038/ncomms5823 ↗
13. Brocken · 1998
14. Salt transport in plaster/substrate layers10.1617/s11527-006-9151-7 ↗
15. The influence of the pore structure on the moisture transport in lime plaster-brick systems as studied by NMR10.1016/j.conbuildmat.2017.03.086 ↗
16. Development of a new accelerated salt crystallization test
17. Encapsulated crystallisation inhibitor as a long-term solution to mitigate salt damage in hydraulic mortars10.1016/j.cemconcomp.2024.105682 ↗
18. Effect of mixed in crystallization modifiers on the resistance of lime mortar against NaCl and Na2SO4 crystallization10.1016/j.conbuildmat.2018.11.006 ↗
19. CEN, EN 196-1 - Methods of testing cement - Part 1: Determination of strength, (2005).
20. CEN, EN 1015-3 - Methods of test for mortar for masonry - Part 3: Determination of consistence of fresh mortar (by flow table), (1999).
21. A new method for making artificially weathered stone specimens for testing of conservation treatments10.1016/j.culher.2015.01.002 ↗
22. MS-A.1 Determination of the resistance of wallettes against sulphates and chlorides10.1007/BF02486406 ↗
23. Groot · 1993
24. T. Wijffels, R. van Hees, The influence of the loss of water of the fresh mortar to the substrate on the hygric characteristics of so-called restoration plaster, in: Proceeding of the Int. Workshop on Urban Heritage and Building Maintenance VII, 2000: pp. 49–54.
25. CEN, EN 1015-11 - Methods of test for mortar for masonry - Part 11: Determination of flexural and compressive strength of hardened mortar, (1999).
26. van der Klugt · 1994
27. Selection of plasters and renders for salt laden masonry substrates10.1016/j.conbuildmat.2008.09.013 ↗
28. Development of a new accelerated salt crystallization test
29. How does sodium sulfate crystallize? Implications for the decay and testing of building materials10.1016/S0008-8846(00)00381-1 ↗
30. Impact of the kinetics of salt crystallization on stone damage during rewetting/drying and humidity cycling10.1115/1.4007924 ↗
31. Salt crystal purification by deliquescence/crystallization cycling10.1209/0295-5075/95/48002 ↗
32. Irreversible dilation of NaCl contaminated lime-cement mortar due to crystallization cycles10.1016/j.cemconres.2005.10.008 ↗
33. A new accelerated salt weathering test by RILEM TC 271-ASC: preliminary round robin validation10.1617/s11527-022-02067-8 ↗
34. Towards a more effective and reliable salt crystallization test for porous building materials: state of the art
35. Experimental research on hygroscopic behaviour of porous specimens contaminated with salts10.1016/j.conbuildmat.2004.02.007 ↗
36. Evaluating the salt content of salt-contaminated samples on the basis of their hygroscopic behavior. Part I: fundamentals, scope and accuracy of the method10.1016/j.culher.2006.02.009 ↗
37. Evaluating the salt content of salt-contaminated samples on the basis of their hygroscopic behaviour: Part II: experiments with nine common soluble salts10.1016/j.culher.2006.03.002 ↗
38. A comparative study of hygroscopic moisture content, electrical conductivity and ion chromatography for salt assessment in plasters of historical buildings10.1016/j.conbuildmat.2008.09.029 ↗
39. Effect of salt crystallisation on the shear behaviour of masonry walls: an experimental study10.1016/j.conbuildmat.2012.07.086 ↗
40. Salt weathering: influence of evaporation rate, supersaturation and crystallization pattern10.1002/(SICI)1096-9837(199903)24:3<191::AID-ESP942>3.0.CO;2-G ↗
41. Gonçalves · 2007
42. Experimental research on hygroscopic behaviour of porous specimens contaminated with salts10.1016/j.conbuildmat.2004.02.007 ↗
43. D. Gulotta, Comparative estimation of the pore filling of single salts in natural stone, in: B. Lubelli, A. Kamat, W. Quist (Eds.), Fifth International Conference on Salt Weathering of Buildings and Stone Sculptures, TU Delft Open, 2021.