High-temperature behavior of expanded-perlite-modified cement mortars: An experimental investigation
Source abstract
Abstract
This study investigates the mechanical, thermal, and microstructural response of cement mortars incorporating expanded perlite (EP) as a volumetric replacement for natural sand (25–40 %). A 50:50 blend of fine and coarser EP grades was preconditioned to a saturated-surface-dry (SSD) state, enabling the target workability to be achieved without superplasticizer (SP), unlike the reference mortar. Increasing EP content reduced bulk density and mechanical strength due to the low stiffness of the aggregate and a weakened interfacial transition zone. Upon exposure to elevated temperatures (100–1000 °C), EP-modified mortars exhibited higher mass loss below 400 °C associated with the release of absorbed water, while at temperatures exceeding 800 °C the porous EP inclusions effectively mitigated explosive spalling and preserved physical integrity. Thermogravimetric (TG–DTG) analysis confirmed that the fundamental hydration chemistry remained unchanged, with apparent peak amplification attributable to binder-fraction normalization effects rather than altered phase composition. SEM–EDS observations showed that the thermally stable silicate skeleton of EP remains intact after binder dehydration and contributes to post-heating structural continuity. In addition to confirming the expected density–strength trade-off, the study provides a controlled high-temperature performance dataset based on quantified EP moisture conditioning and a closed water budget, a gradation-engineered EP aggregate blend, and standardized ISO 834 fire exposure up to 1000 °C. The results support mix-design-oriented guidance, indicating that 25–30 % EP offers a balanced compromise between mechanical capacity and density reduction, whereas 40 % EP provides the highest integrity and spalling resistance at 800–1000 °C but with very limited residual strength at 1000 °C, indicating suitability mainly for protective and non-load-bearing roles. • Mechanical thermal response of cement mortars incorporating expanded perlite as volumetric replacement for natural sand (25-40%). • Increasing expanded perlite content reduced compressive strength and density. • EP replacement offers balance trade-off between strength.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fire effects on concrete materials · Concrete and Cement Materials Research · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Effect of expanded perlite aggregates and temperature on the strength and dynamic elastic properties of cement mortar
2. A critical review on high temperature performance of sustainable cementitious materials10.1038/s44296-025-00081-9 ↗
3. A comprehensive study of perlite in building materials: balancing sustainability and performance
4. Development of Passive Fire Protection Mortars
5. Effect of Expanded Perlite Aggregate Plaster on the Behavior of High-Temperature Reinforced Concrete Structures
6. Effect of expanded perlite on physical and mechanical properties of cement mortar10.1063/5.0063810 ↗
7. Mechanical properties and size effects in lightweight mortars containing expanded perlite aggregate10.1617/s11527-010-9662-0 ↗
8. Influence of perlite and aerogel addition on the performance of cement-based mortars at elevated temperatures
9. Effect of the expanded perlite dose on the fire performance of gypsum plasters
10. Effect of perlite particles on the properties of oil-well class G cement
11. K. Purandara, G. Udayakumar, Gopinatha Nayak, 2018, Elevated Temperature Performance of Expanded Perlite Aggregate Cement Mortar as a Protective Cover for Concrete [Internet]. 2018. www.sciencepubco.com/index.php/IJET.
12. Properties of Fine Graded Perlite-Based Lightweight Cement Mortars Subjected to Elevated Temperatures
13. Investigation of physical and mechanical properties of mortars produced by polymer coated perlite aggregate
14. Fire-Insulating Cementitious Composite for Tunnel Structures: Performance and Fire Tests
15. Expanded perlite aggregate characterization for use as a lightweight construction raw material
16. Chemical, mineralogical and structural features of native and expanded perlite from Macedonia10.4154/gc.2019.18 ↗
17. EN 1097-6:2022. Tests for Mechanical and Physical Properties of Aggregates — Part 6: Determination of Particle Density and Water Absorption [Internet]. Brussels, Belgium; 2022. 〈https://standards.iteh.ai/catalog/standards/cen/7eb55eec-cf2d-449c-bdf5-45534b169181/en-1097-6-2022〉.
18. EN 1015-3:2000/A2:2007; Methods of Test for Mortar for Masonry—Part 3: Determination of Consistence of Fresh Mortar (by Flow Table). Brussels, Belgium: European Committee for Standardization; 2007.
19. European Committee for Standardization. EN 1015-11: Methods of Test for Mortar for Masonry — Part 11: Determination of Flexural and Compressive Strength of Hardened Mortar. Brussels, Belgium; 2007.
20. ISO 834-1:1999 — Fire-resistance tests — Elements of building construction — Part 1: General requirements. Geneva, Switzerland; 1999.
21. European Committee for Standardization (CEN). EN 1991-1-2:2002 – Eurocode 1: Actions on structures – Part 1-2: General actions – Actions on structures exposed to fire. Brussels, Belgium; 2002.
22. Perlite as High Temperature Insulation [Internet]. 2013. 〈https://www.perlite.org/wp-content/uploads/2018/03/perlite-high-temp-applications.pdf〉.
23. The use of thermal analysis in assessing the effect of temperature on a cement paste
24. EN 1015-10:1999 Methods of test for mortar for masonry — Part 10: Determination of dry bulk density of hardened mortar. Brussels, Belgium: CEN; 1999.
25. Effect of expanded perlite on the mechanical properties and thermal conductivity of lightweight concrete10.1016/j.enbuild.2010.11.008 ↗
26. Evaluation of self compacting concrete performance incorporated with presoaked lightweight aggregates
27. Evaluation of the thermo-physical, mechanical, and fire resistance performances of limestone calcined clay cement (LC3)-based lightweight rendering mortars
28. Bentz D.P., Weiss W.J. Internal Curing: A 2010 State-of-the-Art Review [Internet]. Gaithersburg, MD; 2011. 〈https://nvlpubs.nist.gov/nistpubs/ir/2011/NIST.IR.7765.pdf〉.10.6028/NIST.IR.7765 ↗
29. Allameh Haery H. Elastic and mechanical properties of expanded perlite and perlite/epoxy foams [Internet]. [Newcastle, Australia]: Open Research Newcastle; 2017. 〈https://hdl.handle.net/1959.13/1342439〉.
30. Investigation of Physical-Mechanical Properties and Microstructure of Mortars with Perlite and Thermal-Treated Materials
31. A study of thermal decomposition of phases in cementitious systems using HT-XRD and TG
32. Thermal properties of calcium sulfoaluminate cement-based mortars incorporated with expanded perlite cured at cold temperatures
33. Properties of concrete at elevated temperatures
34. Behaviour of cement concrete at high temperature
35. Mechanical properties of concrete at high temperature-A review
36. Importance of quantitative thermogravimetry on initial cement mass basis to evaluate the hydration of cement pastes and mortars10.1007/s10973-013-3112-5 ↗
37. Thermogravimetry on calcined mass basis — hydrated cement phases and pozzolanic activity quantitative analysis10.1007/s10973-008-9761-0 ↗