journal article·2019-11-01

Corrosion in CO2 Systems with Impurities Creating Strong Acids

Bjørn H. Morland, Morten Tjelta, Arne Dugstad, Gaute Svenningsen

Corrosion· Volume 75· Issue 11
Publisher page

Abstract

There are several proposed specifications for CO2 transport regarding how much impurities that can be allowed in the CO2 stream. Many of these specifications are based on health, safety, and environment (HSE) considerations in case of accidental spill, and only limited focus has been on the pipeline integrity. Previous work has demonstrated that many of the impurities that are expected to be present in CO2 captured from flue gasses may react and form corrosive species. The present paper studied impurity reactions and corrosion under simulated transport conditions (25°C and 10 MPa of CO2). An experiment was performed in a transparent autoclave which allowed for in situ visual observation. Chemical reactions between the impurities were observed even at very low concentrations (<100 ppmv). These reactions contributed to the production of nitric and sulfuric acid together with formation of elemental sulfur. Corrosion was observed on coupons of carbon steel, but not on stainless steels. The corrosion rate of carbon steel was low, but the amount of acids and solids (corrosion products) produced cannot be accepted from a pipeline integrity perspective. Further experimental studies are needed to determine specific limits for impurity concentrations in captured CO2 for transport.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Offshore Engineering and Technologies · Risk and Safety Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

*Department of Chemistry, University of Oslo, Sem Sælands vei 26, NO-0371 Oslo, Norway.

**Corrosion Technology Department, Instituttveien 18, NO-2007 Kjeller, Norway.

References (27)

Show source-provided references
1. “Climate Change 2013: The Physical Science Basis”
2. Gassco, Gassnova, Ministry of Petroleum and Energy · 2016
3. Halseid · Energ. Proc. · 2014 · 63 · 255710.1016/j.egypro.2014.11.278 ↗
4. “Quality Guidelines for Energy System Studies—CO2 Impurity Design Parameters,”
5. Dugstad · Energ. Proc. · 2014 · 63 · 254710.1016/j.egypro.2014.11.277 ↗
6. “Corrosion Stability of Piping Steels in a Circulating Supercritical Impure CO2 Environment,”
7. “COORAL– CO2 Purity for Capture and Storage,”
8. “Dense Phase CO2 Transport–When is Corrosion a Threat,”
9. “Corrosion in Dense Phase CO2 with Small Amounts of SO2, NO2 and Water,”
10. Brown · Energ. Proc. · 2014 · 63 · 243210.1016/j.egypro.2014.11.265 ↗
11. “Effects of CO2 Phase Change, SO2 Content and Flow on the Corrosion of CO2 Transmission Pipeline Steel,”
12. “Effect of Water Content on the Corrosion Behavior of Carbon Steel in Supercritical CO2 Phase with Impurities,”
13. Xiang · J. Supercritical Fluids · 2011 · 58 · 28610.1016/j.supflu.2011.06.007 ↗
14. “Corrosion in Dense Phase CO2 Pipelines–State of the Art,”
15. “Transport of Dense Phase CO2 in C-Steel Pipelines—When is Corrosion an Issue?”
16. Hua · Corrosion · 2015 · 71 · 66710.5006/1504 ↗
17. Sun · Corros. Sci. · 2018 · 137 · 15110.1016/j.corsci.2018.03.041 ↗
18. Sun · Corros. Sci. · 2016 · 107 · 19310.1016/j.corsci.2016.02.032 ↗
19. Sun · J. Supercritical Fluids · 2016 · 116 · 7010.1016/j.supflu.2016.05.006 ↗
20. Sun · Corros. Sci. · 2016 · 107 · 3110.1016/j.corsci.2016.02.017 ↗
21. Choi · Environ. Sci. Technol. · 2010 · 44 · 923310.1021/es102578c ↗
22. Xiang · Sci. Technol. · 2017 · 52 · 485
23. Kranzmann · Int. J. Greenhouse Gas Control · 2011 · 5 · S16810.1016/j.ijggc.2011.05.029 ↗
24. Dugstad · Energ. Proc. · 2013 · 37 · 287710.1016/j.egypro.2013.06.173 ↗
25. Leygraf · , & , 1995
26. Panossian · Corros. Sci. · 2012 · 58 · 110.1016/j.corsci.2012.01.025 ↗
27. Damon · Ind. Eng. Chem. · 1941 · 33 · 6710.1021/ie50373a013 ↗