journal article·2017-08-01

Corrosion Behavior of Mild Steel in Sour Environments at Elevated Temperatures

Shujun Gao, Peng Jin, Bruce Brown, David Young, Srdjan Nesic, Marc Singer

Corrosion· Volume 73· Issue 8
Publisher page

Abstract

The objective of this work was to determine the corrosion rate of mild steel and characterize the corrosion products in sour environments at temperatures ranging from 80°C to 200°C. First, a H2S–H2O water chemistry model was developed based on available literature for a closed system at high temperature. Then, H2S corrosion tests were conducted at 80°C, 120°C, 160°C, and 200°C with an exposure time of 4 d. Linear polarization resistance (LPR) and weight loss (WL) methods were used to measure the corrosion rates. X-ray diffraction (XRD) and scanning electron microscopy with energy dispersive x-ray spectroscopy microanalysis (SEM/EDS) were used to characterize the corrosion products and surface morphology. The results show that the initial corrosion rates increased with temperature then decreased as they achieved steady state. The corrosion product was comprised of two distinct layers. The inner corrosion product was always an iron oxide layer (hypothesized to be Fe3O4), while mackinawite, troilite, pyrrhotite, and pyrite were identified as the main components of the outer layer at 80°C, 120°C, 160°C and 200°C, respectively. Pourbaix diagrams generated based on the analysis of water chemistry corroborated the experimental characterization of the corrosion products.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

*Institute for Corrosion and Multiphase Technology, Department of Chemical & Biomolecular Engineering, Ohio University, 342 West State Street, Athens, OH 45701.

References (25)

Show source-provided references
1. DeBruijin · Oilfield Rev. · 2008 · 20 · 46
2. “High Temperature Corrosion Inhibition Performance of Imidazoline and Amide,”
3. Prabha · Eur. Chem. Bull. · 2014 · 3 · 300
4. Ma · Corros. Sci. · 2000 · 42 · 166910.1016/S0010-938X(00)00003-2 ↗
5. “Kinetics of Iron Sulfide and Mixed Iron Sulfide/Carbonate Scale Precipitation in CO2/H2S Corrosion,”10.5006/C2006-06644 ↗
6. Tang · Corros. Sci. · 2010 · 52 · 205010.1016/j.corsci.2010.02.004 ↗
7. Zheng · Corrosion · 2013 · 70 · 35110.5006/0937 ↗
8. Ning · Corrosion · 2015 · 71 · 94510.5006/1566 ↗
9. “A Parametric Study of Sour Corrosion of Carbon Steel,”10.5006/C2010-10278 ↗
10. Ramanarayanam · Corrosion, · 1990 · 46 · 6610.5006/1.3585068 ↗
11. Shi · Corros. Sci. · 2016 · 102 · 10310.1016/j.corsci.2015.09.024 ↗
12. Backensto · Corrosion · 1956 · 12 · 2210.5006/0010-9312-12.1.22 ↗
13. Skalunov · Fibre Chem. · 1987 · 18 · 32110.1007/BF00556561 ↗
14. Qi · Int. J. Electrochem. Sci. · 2014 · 9 · 210110.1016/S1452-3981(23)07914-2 ↗
15. Zheng · Corrosion · 2016 · 72 · 67910.5006/1667 ↗
16. “Construction and Verification of Pourbaix Diagrams for CO2 Corrosion of Mild Steel Valid up to 250°C,”10.5006/C2012-01418 ↗
17. “Corrosion Fatigue Performance of Super 13 CR, Duplex 2205 and 2507 for Riser Applications,”
18. “Construction and Verification of Pourbaix Diagrams for Hydrogen Sulfide Corrosion of Mild Steel,”10.5006/C2015-05507 ↗
19. Jones · J. Res. Natl. Inst. Standards Technol. · 1992 · 97 · 33510.6028/jres.097.013 ↗
20. Suleimenov · Geochim. Cosmochim. Acta · 1994 · 58 · 243310.1016/0016-7037(94)90022-1 ↗
21. Suleimenov · Geochim. Cosmochim. Acta · 1997 · 61 · 518710.1016/S0016-7037(97)00291-3 ↗
22. Ning · Corrosion · 2014 · 70 · 37510.5006/0951 ↗
23. Singh · Corrosion · 2003 · 59 · 102910.5006/1.3277521 ↗
24. “The Role of Iron Sulfide Polymorphism in Localized H2S Corrosion of Mild Steel,”10.5006/C2016-07502 ↗
25. Benning · Chem. Geol. · 2000 · 167 · 2510.1016/S0009-2541(99)00198-9 ↗