Erosion-Corrosion Behavior of Some Cast Alloys in Seawater
Source abstract
Abstract
The corrosion behaviors of high-chromium duplex cast steel, high-silicon, nodular, and nickel-resist cast iron were studied in stagnant and flowing seawater (flow velocities of 2.5, 5.4, and 8.3 m/s). The experiments involved measurements of the mass loss and examination of the corrosion morphology. The duplex stainless steel did not experience corrosion and/or erosion damage. The high-silicon cast iron exhibited excellent erosion-corrosion resistance but was susceptible to pitting attack only under stagnant and relatively low-flow conditions. The attack occurred at the boundaries of graphite flakes and interdendritic carbides. Both the nodular and nickel-resist cast irons suffered from erosion-corrosion damage that was more severe in the former alloy. Under stagnant conditions, the corrosion rates were very low for both alloys, and thin scales were observed. However, under flow conditions, relatively thick scales were formed showing patterns of seawater flow. There was a sharp increase in the corrosion rates reaching peak values (velocity dependent) after 3 days of testing. This was followed by a gradual decrease until steady rates were reached after about 17 to 21 days. Removal of the scales revealed that corrosion was more intensive around graphite nodules and flakes, leading to loosening and removal of the graphite.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Erosion and Abrasive Machining · High-Temperature Coating Behaviors · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
*Technical Research Center of Finland, Metals Laboratory, P.O. Box 26 (Kemistintie 3), SP-02151 Espoo, Finland.
**National Research Center of Egypt, Corrosion Laboratory, Tahrir St., P.O. Box 12311, Dokki, Cairo, Egypt.
References (26)
Show source-provided references
1. Lotz · Werkst. Korros. · 1983 · 34 · 45410.1002/maco.19830340906 ↗
2. Heitz · J. Appl. Electrochem. · 1979 · 9 · 24310.1007/BF00616094 ↗
3. Franz · Werkst. Korros. · 1973 · 24 · 3810.1002/maco.19730240110 ↗
4. Gouda · Materials Performance · 1989 · 28 · 53
5. Molgaard · 1974 · 792
6. Gouda · Br. Corros. J. · 1991 · 26 · 10910.1179/000705991798269314 ↗
7. Okada · Ship Res. · 1981 · 25 · 27
8. Karimi · Int. Met. Reviews · 1986 · 31 · 110.1179/imr.1986.31.1.1 ↗
9. Evans · 1960
10. Butter · Br. Corros. J. · 1965 · 1 · 11010.1179/000705965798327967 ↗
11. Mahato · Corros. Sci. · 1968 · 8 · 73710.1016/S0010-938X(68)80131-3 ↗
12. Syrett · Corrosion · 1976 · 32 · 24210.5006/0010-9312-32.6.242 ↗
13. Lotz · Werkst. Korros. · 1985 · 36 · 16310.1002/maco.19850360405 ↗
14. Heitz · 1974 · 477
15. Effrid · Corrosion · 1977 · 33 · 477
16. Bond · 1984 · 26
17. Dundas · 1985 · 206
18. Truman · 1982 · 8201-006
19. Schumacher · 1979
20. Fontana · 1967
21. Shreir · 1977
22. Collins · Br. Cast Iron Res. Ass. J. · 1963 · 10 · 543
23. Bloom · Materials Performance · 1984 · 23 · 21
24. Palmer · Materials Perfomance · 1988 · 26 · 58
25. Okada · Wear · 1983 · 84 · 16710.1016/S0043-1648(83)80006-4 ↗
26. Temperly · Corros. Sci. · 1965 · 5 · 58110.1016/S0010-938X(65)80047-6 ↗